journal article·2013-07

Effects of chemical modification on the mechanical properties of wood

Yanjun Xie, Qiliang Fu, Qingwen Wang, Zefang Xiao, Holger Militz

Publisher page

Abstract

Chemical modification has been recognized as an efficient strategy for dimensionally stabilizing wood and protecting it from environmental damage, such as deterioration due to weathering and fungal decay during the service period. Studies reported in the literature mainly concern the establishment of workable modification techniques, testing methodologies, and assessment of the durability of modified wood. The development of wood modification techniques has recently been reviewed; limited information is however given on the effects of chemical modification on the mechanical properties of wood that are of importance to it as an engineering material. This paper reviews the effects of wood modification, typically by heat treatments and impregnation with low molecular weight resins, reactive monomers, or hot melting paraffins on the mechanical properties of wood. The modifying variables associated with mechanical properties of wood such as wood species, treating temperature and time, catalyst, type of solvent, weight percent gain, and molecular structures of the modifying agent were analysed and the results interpreted. The reasons for changes in the mechanical properties of wood are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Bamboo properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Alén R, Oesch P, Kuoppala E (1995) Py-GC/AED studies on thermochemical behavior of softwood. J Anal Appl Pyrol 35:259–26510.1016/0165-2370(95)00915-6 ↗
2. Alma MH, Hafizolu H, Maldas D (1996) Dimensional stability of several wood species treated with vinyl monomers and polyethylene glycol-1000. Int J Polym Mater 32:93–9910.1080/00914039608029385 ↗
3. Arnold M (2010) Effect of moisture on the bending properties of thermally modified beech and spruce. J Mater Sci 45:669–68010.1007/s10853-009-3984-8 ↗
4. Barsberg S, Thygesen LG (2009) Poly(furfuryl alcohol) formation in neat furfuryl alcohol and in cymene studied by ATR-IR spectroscopy and density functional theory (B3LYP) prediction of vibrational bands. Vib Spectrosc 49:52–6310.1016/j.vibspec.2008.04.013 ↗
5. Baysal E, Yalinkilic MK, Altinok M, Sonmez A, Peker H, Colak M (2007) Some physical, biological, mechanical, and fire properties of wood polymer composite (WPC) pretreated with boric acid and borax mixture. Constr Build Mater 21:1879–188510.1016/j.conbuildmat.2006.05.026 ↗
6. Bergman R, lbach RE, LaPasha C, Denig J (2009) Evaluating physical property changes for small-diameter, plantation-grown southern pine after in situ polymerization of an acrylic monomer. Forest Prod J 59:64–7110.13073/0015-7473-59.10.64 ↗
7. Bhat I, Abdul Khalil HPS, Awang KB, Bakare IO, Issam AM (2010) Effect of weathering on physical, mechanical and morphological properties of chemically modified wood materials. Mater Design 31:4363–436810.1016/j.matdes.2010.03.045 ↗
8. Bollmus S, Rademacher P, Krause A, Militz H (2010) Material evaluation and product performance of beech wood modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU). In: The Fifth European Conference on Wood Modification. Riga, Latvia
9. Bongers HPM, Beckers EPJ (2003) Mechanical properties of acetylated solid wood treated on pilot plant scale. In: Van Acker J, Hill CAS (eds) The first European conference on wood modification. Ghent, Belgium, pp 341–350
10. Boonstra M (2008) A two-stage thermal modification of wood. PhD thesis, Soil and Forest Management: Henry Poincare University-Nancy, France
11. Cai X, Riedl B, Zhang SY, Wan H (2007) Effects of nanofillers on water resistance and dimensional stability of solid wood modified by melamine-urea-formaldehyde resin. Wood Fiber Sci 39:307–318
12. Christmas J, Sargent R, Tetri T (2005) Thermal modification of New Zealand Radiata pine. In: Militz H, Hill CAS (eds) The second European conference on wood modification. Göttingen, Germany, pp 83–86
13. Deka M, Saikia CN (2000) Chemical modification of wood with thermosetting resin: effect on dimensional stability and strength property. Bioresource Technol 73:179–18110.1016/S0960-8524(99)00167-4 ↗
14. Deka M, Saikia CN, Baruah KK (2002) Studies on thermal degradation and termite resistant properties of chemically modified wood. Bioresource Technol 83:151–15710.1016/S0960-8524(02)00016-0 ↗
15. Devi RR, Ali I, Maji TK (2003) Chemical modification of rubber wood with styrene in combination with a crosslinker: effect on dimensional stability and strength proeprty. Bioresource Technol 88:185–18810.1016/S0960-8524(03)00003-8 ↗
16. Dreher WA, Goldstein IS, Cramer GR (1964) Mechanical properties of acetylated wood. Forest Prod J 14:66–68
17. Epmeier H, Kliger R (2005) Experimental study of material properties of modified Scots pine. Eur J Wood Wood Prod 63:430–43610.1007/s00107-005-0019-2 ↗
18. Epmeier H, Westin M, Rapp AO, Nilsson T (2003) Comparison of properties of wood modified by 8 different methods—durability, mechanical and physical properties. In: Van Acker J, Hill CAS (eds) The first European conference on wood modification. Ghent, Belgium, pp 121–142
19. Epmeier H, Westin M, Rapp AO (2004) Differently modified wood: comparison of some selected properties. Scand J Forest Res 19(suppl 5):31–3710.1080/02827580410017825 ↗
20. Epmeier H, Johansson M, Kliger R, Westin M (2007) Bending creep performance of modified timber. Eur J Wood Wood Prod 65:343–35110.1007/s00107-007-0189-1 ↗
21. Esteves BM, Pereira HM (2009) Wood modification by heat treatment: a review. BioResources 4:370–40410.15376/biores.4.1.Esteves ↗
22. Esteves B, Marques AV, Domingos I, Pereira H (2007) Influence of steam heating on the properties of pine (Pinus pinaster) and eucalypt (Eucalyptus globulus) wood. Wood Sci Technol 41:193–20710.1007/s00226-006-0099-0 ↗
23. Esteves B, Nunes L, Pereira H (2011) Properties of furfurylated wood (Pinus pinaster). Eur J Wood Wood Prod 69:521–52510.1007/s00107-010-0480-4 ↗
24. Evans PD, Wallis AF, Owen NL (2000) Weathering of chemically modified wood surfaces: natural weathering of Scots pine acetylated to different weight gains. Wood Sci Technol 34:151–16510.1007/s002260000039 ↗
25. Furono T, Imamura Y, Kajita H (2004) The modification of wood by treatment with low molecular weight phenol-formaldehyde resin: a properties enhancement with neutralized phenolic resin and resin penetration into wood cell walls. Wood Sci Technol 37:349–36110.1007/s00226-003-0176-6 ↗
26. Gabrielli CP, Kamke FA (2010) Phenol-formaldehyde impregnation of densified wood for improved dimensional stability. Wood Sci Technol 44:95–10410.1007/s00226-009-0253-6 ↗
27. Gerhards CC (1982) Effect of moisture content and temperature on the mechanical properties of wood. Wood Fiber 14:4–36
28. Gindl W, Gupta HS (2002) Cell-wall hardness and Young’s modulus of melamine-modified spruce wood by nano-indentation. Compos Part A-Appl S 33:1141–114510.1016/S1359-835X(02)00080-5 ↗
29. Gindl W, Dessipri E, Wimmer R (2002) Using UV-microscopy to study diffusion of melamine-urea-formaldehyde resin in cell walls of spruce wood. Holzforschung 56:103–10710.1515/HF.2002.017 ↗
30. Gindl W, Müller U, Teischinger A (2003) Transverse compression strength and fracture of spruce wood modified by melamine-formaldehyde impregnation of cell walls. Wood Fiber Sci 35:239–246
31. Gindl W, Hansmann C, Gierlinger N, Schwanninger M, Hinterstoisser B, Jeronimidis G (2004) Using a water-soluble melamine-formaldehyde resin to improve the hardness of Norway spruce wood. J Appl Polym Sci 93:1900–190710.1002/app.20653 ↗
32. Goldstein IS (1955) The impregnation of wood to impart resistance to alkali and acid. Forest Prod J 5:265–267
33. Goldstein IS, Dreher WA (1960) Stable furfuryl alcohol impregnating solutions. Ind Eng Chem 52:57–5810.1021/ie50601a039 ↗
34. Goldstein IS, Jeroski EB, Nielson JF, Weaver JW (1961) Acetylation of wood in lumber thickness. Forest Prod J 11:363–370
35. González R, Martínez R, Ortiz P (1992a) Polymerization of furfuryl alcohol with trifluoroacetic acid: the influence of experimental conditions. Die Makromol Chem 193:1–910.1002/macp.1992.021930101 ↗
36. González R, Martínez R, Ortiz P (1992b) Polymerization of furfuryl alcohol with trifluoroacetic acid: the formation of difurfuryl ether. Die Makromol Chem 13:517–52310.1002/marc.1992.030131107 ↗
37. Hansmann C, Deka M, Wimmer R, Gindl W (2006) Artificial weathering of wood surfaces modified by melamine formaldehyde resins. Eur J Wood Wood Prod 64:198–20310.1007/s00107-005-0047-y ↗
38. Hill CAS (2006) Wood modification: chemical, thermal and other processes. Wiley, Chichester10.1002/0470021748 ↗
39. Hill CAS (2011) Wood modification: an update. BioResources 6:918–91910.15376/biores.6.2.918-919 ↗
40. Hill CAS, Abdul Khalil HPS, Hale MD (1988) A study of the potential of acetylation to improve the properties of plant fibres. Ind Crop Prod 8:53–6310.1016/S0926-6690(97)10012-7 ↗
41. Hill CAS, Jones D, Strickland G, Cetin NS (1998) Kinetic and mechanistic aspects of the acetylation of wood with acetic anhydride. Holzforschung 52:623–62910.1515/hfsg.1998.52.6.623 ↗
42. Hillis WE (1984) High-temperature and chemical effects on wood stability. Wood Sci Technol 18:281–29310.1007/BF00353364 ↗
43. Homan WJ, Jorissen AJM (2004) Wood modification developments. Heron 49:361–386
44. Hon DNS (1995) Stabilization of wood color: is acetylation blocking effective? Wood Fiber Sci 27:360–367
45. Hoydonckx HE, Van Rhijn WM, Van Rhijn W, Hueting D, Tjeerdsma B, van der Zee M, Van Acker J (2007) Renewable furfuryl resin technology for wood modification. In: Hill CAS, Jones D, Militz H (eds) The third European conference on wood modification. Cardiff, UK, pp 81–86
46. Jamsa S, Viitaniemi P (2001) Heat treatment of wood better durability without chemicals. In: Rapp AO (ed) Seminar of Cost Action E22, Antibes, France
47. Jorissen A, Bongers F, Kattenbroek B, Homan W (2005) The influence of acetylation of Radiata pine in structural sizes on its strength properties. In: Militz H, Hill CAS (eds) The Second European Conference on Wood Modification. Göttingen, Germany
48. Kamdem DP, Pizzi A, Jermannaud A (2002) Durability of heat-treated wood. Eur J Wood Wood Prod 60:1–610.1007/s00107-001-0261-1 ↗
49. Kocaefe D, Poncsák S, Tang J, Bouazara M (2010) Effect of heat treatment on the mechanical properties of North American jack pine: thermogravimetric study. J Mater Sci 45:681–68710.1007/s10853-009-3985-7 ↗
50. Kollmann FFP, Côté WA Jr (1968) Principles of wood science and technology. Volume I: Solid wood. Springer, Berlin10.1007/978-3-642-87928-9 ↗
51. Korkut S, Akgül M, Dündar T (2008) The effects of heat treatment on some technological properties of Scots pine (Pinus szlvestris L.) wood. Bioresource Technol 99:1861–186810.1016/j.biortech.2007.03.038 ↗
52. Krause A, Jones D, Van der Zee M, Militz H (2003) Interlace treatment—wood modification with N-methylol compounds. In: Van Acker J, Hill CAS (eds) The First European Conference on Wood Modificaiton. Ghent, Belgium, pp 317–327
53. Krause A, Wepner F, Xie Y, Militz H (2008) Wood protection with dimethylodihydroxy-ethyleneurea and its derivatives. In: Schultz TP, Militz H, Freeman MH, Goodell B, Nicholas DD (eds) Development of commercial wood preservatives: efficacy, environmental, and health issues. ACS Symposium Series; American Chemical Society, Washington, DC, pp 356–371
54. Kretschmann DE (2010) Mechanical properties of wood. Madison, U.S. Department of Agriculture, Forest Service, Forest Products Laboratory: General technical report FPL-GTR-190
55. Kubojima Y, Okano T, Ohta M (2000) Bending strength and toughness of heat-treated wood. J Wood Sci 46:8–1510.1007/BF00779547 ↗
56. Lande S, Westin M, Schneider MH (2004) Properties of furfurylated wood. Scand J Forest Res 19(Sup5):22–3010.1080/0282758041001915 ↗
57. Lande S, Eikenes M, Westin M, Schneider MH (2008) Furfurylation of wood: chemistry, properties, and commercialization. In: Schultz TP, Militz H, Freeman MH, Goodell B, Nicholas DD (eds) Development of commercial wood preservatives: efficacy, environmental, and health issues. ACS Symposium Series; American Chemical Society, Washington, DC, pp 337–35510.1021/bk-2008-0982.ch020 ↗
58. Larsson P, Simonson R (1994) A study of strength, hardness and deformation of acetylated Scandinavian softwoods. Eur J Wood Wood Prod 52:83–8610.1007/BF02615470 ↗
59. Lesar B, Humar M (2011) Use of wax emulsions for improvement of wood durability and sorption properties. Eur J Wood Wood Prod 69:231–23810.1007/s00107-010-0425-y ↗
60. Lesar B, Pavlič M, Petrič M, Škapin AS, Humar M (2011) Wax treatment of wood slows photodegradation. Polym Degrad Stabil 96:1271–127810.1016/j.polymdegradstab.2011.04.006 ↗
61. Li JZ, Furuno T, Zhou WR, Ren Q, Han XZ, Zhao JP (2009) Properties of acetylated wood prepared at low temperature in the presence of catalysts. J Wood Chem Technol 29:241–25010.1080/02773810903009499 ↗
62. Li Y, Wang B, Fu Q, Liu Y, Dong X (2010) Performance of wood-polymer composite prepared by in situ synthesis of terpolymer within wood. Appl Mech Mater 34–35:1165–116910.4028/www.scientific.net/AMM.34-35.1165 ↗
63. Li Y, Liu YX, Wang XM, Wu QL, Yu HP, Li J (2011) Wood-polymer composites prepared by the in situ polymerization of monomers within wood. J Appl Polym Sci 119:3207–321610.1002/app.32837 ↗
64. Lukowsky D (2002) Influence of the formaldehyde content of waterbased melamine formaldehyde resins on physical properties of Scots pine impregnated therewith. Eur J Wood Wood Prod 60:349–35510.1007/s00107-002-0324-y ↗
65. Mayes D, Oksanen O (2002) ThermoWood handbook. By: Thermowood, Finnforest, Stora
66. Militz H (1991) Die Verbesserung des Schwind- und Quellverhaltens und der Dauerhaftigkeit von Holz mittels Behandlung mit unkatalysiertem Essigsäureanhydrid. Eur J Wood Wood Prod 49:147–15210.1007/BF02607895 ↗
67. Militz H (1993) Treatment of timber with water soluble dimethylol resins to improve their dimensional stability and durability. Wood Sci Technol 27:347–35510.1007/BF00192221 ↗
68. Militz H (2002) Thermal treatment of wood: European processes and their background. In: The International Research Group on Wood Protection. IRG/WP 02-40241, Cardiff, Wales, UK
69. Militz H, Peters BC, Fitzgerald CJ (2009) Termite resistance of some modified wood species. In: The International Research Group on Wood Protection, IRG/WP 09-40449. Beijing, China
70. Minato K, Takazawa R, Ogura K (2003) Dependence of reaction kinetics and physical and mechanical properties on the reaction systems of acetylation. II: physical and mechanical properties. J Wood Sci 49:519–52410.1007/s10086-002-0514-6 ↗
71. Miroy F, Eymard P, Pizzi A (1995) Wood hardening by methoxymethyl melamine. Eur J Wood Wood Prod 53:27610.1007/s001070050089 ↗
72. Mitchell PH (1988) Irreversible property changes of small loblolly pine specimens heated in air, nitrogen, or oxygen. Wood Fiber Sci 20:320–355
73. Mundigler N, Rettenbacher M (2005) Natwood technology—a material thermal wood modification. In: Hill CAS, Militz H (eds) The Second European Conference on Wood Modification. Göttingen, Germany, pp 270–275
74. Nicholas DD, Williams AD (1987) Dimensional stabilization of wood with dimethylol compounds. In: International Research Group on Wood Protection, IRG/WP87-3412. Stockholm, Sweden
75. Nordstierna L, Lande S, Westin M, Furó I, Brynildsen P (2007) 1H NMR demonstration of chemical bonds between lignin-like model molecules and poly(furfuryl alcohol): relevance to wood furfurylation. In: The Third European Conference of Wood Modification. Cardiff, UK, pp 15–16
76. Nunes L, Nobre T, Rapp AO (2004) Thermally modified wood in choice tests with subterranean termites. In: Seminar of COST E37, Reinbeck
77. Nurmi A, Kokko HRDP, Murphy RJ, Stevens M, Hill CAS (1999) Natural resins as a potential wood processing agent. European project report, Agriculture and Agro-Industry including Fisheries Program of Research and Technological Development (FAIR), Program: Forestry-Wood Chain
78. Papadopoulos AN, Pougioula G (2010) Mechanical behaviour of pine wood chemically modified with a homologous series of linear chain carboxylic acid anhydrides. Bioresource Technol 101:6147–615010.1016/j.biortech.2010.02.079 ↗
79. Pittman CU Jr, Kim MG, Nicholas DD, Wang L, Ahmed Kabir FR, Schultz TP, Ingram LL Jr (1994) Wood enhancement treatments I. Impregnation of southern yellow pine with melamine-formaldehyde and melamine-ammeline-formaldehyde resins. J Wood Chem Technol 14:577–60310.1080/02773819408003114 ↗
80. Plackett DV, Dunningham EA, Singh AP (1992) Weathering of chemically modified wood: accelerated weathering of acetylated radiata pine. Eur J Wood Wood Prod 50:135–14010.1007/BF02663254 ↗
81. Poncsák S, Kocaefe D, Bouazara M, Pichette A (2006) Effect of high temperature treatment on the mechanical properties of birch (Betula papyrifera). Wood Sci Technol 40:647–66310.1007/s00226-006-0082-9 ↗
82. Ramsden MJ, Blake FSR, Fey NJ (1997) The effect of acetylation on the mechanical properties, hydrophobicity, and dimensional stability of Pinus sylvestris. Wood Sci Technol 31:97–10410.1007/BF00705699 ↗
83. Rapp AO, Sailer M (2000) Heat treatment of wood in Germany—state of the art. In: Proceedings of Seminar ‘Production and development of heat treated wood in Europe’. Helsinki, Stockholm, Oslo
84. Rapp AO, Bestgen H, Adam W, Peek RD (1999) Electron loss spectroscopy (EELS) for quantification of cell-wall penetration of a melamine resin. Holzforschung 53:111–11710.1515/HF.1999.018 ↗
85. Rowell RM (1982) Distribution of acetyl groups in southern pine reacted with acetic anhydride. Wood Sci 15:178–182
86. Rowell RM (2005) Chemical modification of wood. In: Handbook of wood chemistry and wood composites. CRC Press, Boca Raton, pp 381–42010.1201/9780203492437-17 ↗
87. Rowell RM (2006) Chemical modification of wood: a short review. Wood Mater Sci Eng 1:29–3310.1080/17480270600670923 ↗
88. Ryu JY, Imamura Y, Takahashi M (1992) Biological resistance of fufuryl alcohol-treated wood. In: The International Research Group on Wood Protection, IRG/WP 92-3703. Harrogate, UK
89. Schaffert S, Krause A, Militz H (2005) Upscaling and process development for wood modification with N-methylol compounds using superheated steam. In: Militz H, Hill CAS (eds) The Second European Conference on Wood Modification. Göttingen, Germany, pp 161–168
90. Scheiding W, Kruse K, Plaschkies K, Weiß B (2005) Thermally modified wood (TMW) for playground toys: investigations on 13 industrially manufactured products. In: Militz H, Hill CAS (eds) The Second European Conference on Wood Modification. Göttingen, Germany, pp 12–19
91. Schneider M (1994) Wood polymer composites. Wood Fiber Sci 26:142–151
92. Schneider MH (1995) New cell wall and cell lumen wood polymer composites. Wood Sci Technol 29:121–12710.1007/BF00229341 ↗
93. Schneider MH (2006) Furan polymer impregnated wood. Patent, U.S, No. 7008984
94. Schneider MH, Phillips JG (1991) Elasticity of wood and wood polymer composites in tension, compression and bending. Wood Sci Technol 25:361–36410.1007/BF00226175 ↗
95. Schneider MH, Phillips JG, Tingley DA, Brebner KI (1990) Mechanical properties of polymer-impregnated sugar maple. Forest Prod J 40:37–41
96. Scholz G, Krause A, Militz H (2009) Capillary water uptake and mechanical properties of wax soaked Scots pine. In: Englund F, Hill CAS, Militz H, Segerholm BK (eds) The Fourth European Conference on Wood Modification. Stockholm, Sweden
97. Scholz G, Krause A, Militz H (2010a) Exploratory study on the impregnation of Scots pine sapwood (Pinus sylvestris L.) and European beech (Fagus sylvatica L.) with different hot melting waxes. Wood Sci Technol 44:379–38810.1007/s00226-010-0353-3 ↗
98. Scholz G, Krause A, Militz H (2010b) Beeinflussung der Holzfestigkeit durch Wachstränkung. Holztechnologie 51:22–27
99. Scholz G, Nothnick E, Avramidis G, Krause A, Militz H, Viöl W, Wolkenhauer A (2010c) Verklebung von wachsimprägnierter Buche unter Variation der Klebesysteme und Durchführung einer Plasmabehandlung. Eur J Wood Wood Prod 68:315–32110.1007/s00107-010-0466-2 ↗
100. Scholz G, Krause A, Militz H (2012) Volltränkung modifizierten Holzes mit Wachs. Eur J Wood Wood Prod 70:91–9810.1007/s00107-010-0485-z ↗