Improvement of the heat treatment of Jack pine (Pinus banksiana) using ThermoWood technology
Source abstract
Abstract
Thermal treatment in inert atmosphere is used to preserve wood without utilisation of toxic chemical agents. In addition, this process increases the dimensional stability of the wood matrix and results in attractive dark colour. On the other hand, it can deteriorate the mechanical strength and the flexibility of wood. For this reason, heat treatment parameters (such as maximum temperature, heating rate, the duration of the first plateau at constant temperature (100–120°C) and the second plateau at the maximum treatment temperature, humidity, final cool down rate) must be optimised in order to benefit from advantages of thermal treatment without deteriorating significantly the mechanical properties of wood. Correlation between wood properties and thermal treatment parameters depends not only on the wood species but also the environment (climate, soil) where the given species grow. This paper presents a study on thermal treatment of Canadian Jack pine (Pinus banksiana) using a medium size prototype furnace. The aim of this study was to optimize the set of parameters used during industrial treatments. The possibility of shortening the process time without causing any deterioration in wood quality was also investigated. The results show that increasing the maximum heat-treatment temperature increased the dimensional stability of Jack pine and darkened its colour. This parameter did not affect the modulus of elasticity but it decreased the modulus of rupture of Jack pine. A slight reduction in gas humidity during the initial warming up period permitted to shorten the drying period and at the same time increased the mechanical strength. This improvement helps save energy and increase productivity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Wood and Agarwood Research · Tree Root and Stability Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Alén R, Kotilainen R, Zaman A (2002) Thermochemical behavior of Norway spruce (Picea abies) at 180–225°C. Wood Sci Technol 36:163–17110.1007/s00226-001-0133-1 ↗
2. ASTM Int (2004) Annual book of ASTM standards. Wood 4(10):26–36 & 158
3. Chanrion P, Schreiber J (2002) Different processes; high temperature heat-treated wood (Les différents procédés, Bois traité par haute température). Edition CTBA, Paris, p 115 (In French)
4. Dirol D, Guyonnet R (1993) The improvement of wood durability by retification process. Document No IRG/WP 98-40015. International Research Group on Wood Protection, Stockholm, Sweden
5. Fengel D, Wegener G (1989) Wood: chemistry, ultrastructure, reactions. de Gruyter, Berlin
6. Kamden DP, Pizzi A, Jermannaud A (2002) Durability of heat-treated wood. Holz Roh- Werkst 60:1–610.1007/s00107-001-0261-1 ↗
7. Kifetew G, Thuvander F, Berglund L, Lindberg H (1998) The effect of drying on wood fracture surfaces from specimens loaded in wet conditions. Wood Sci Technol 32:83–9410.1007/BF00702589 ↗
8. Kocaefe D, Chaudry B, Poncsak S, Bouazara M, Pichette A (2007) Thermogravimetric study of high temperature treatment of aspen: effect of treatment parameters on weight loss and mechanical properties. J Mater Sci 42(3):854–86610.1007/s10853-006-0054-3 ↗
9. Pavlo B, Niemz P (2003) Effect of temperature on color and strength of spruce wood. Holzforschung 57:539–54610.1515/HF.2003.080 ↗
10. Poncsak S, Kocaefe D, Bouazara M, Pichette A (2006) Effect of high temperature treatment on the mechanical properties of birch. Wood Sci Technol 40:647–66810.1007/s00226-006-0082-9 ↗
11. Rusche H (1973) Thermal degradation of wood at temperatures up to 200°C, part I: strength properties of dried wood after heat treatment. Holz Roh- Werkst 29:275–278
12. Sanderman W, Augustin H (1963) Chemical investigations on the thermal decomposition of wood, part I: stand of research. Holz Roh- Werkst 21:256–26510.1007/BF02616316 ↗
13. Santos JA (2000) Mechanical behaviour of eucalyptus wood modified by heat. Wood Sci Technol 34:39–4310.1007/s002260050006 ↗
14. Schneider A (1973) Investigations on the convection drying of lumber at extremely high temperatures, part II: drying degrade, changes in sorption, colour and strength of pine sapwood and beech wood at drying temperatures from 110 to 180°C. Holz Roh- Werkst 31:198–20610.1007/BF02613842 ↗
15. Stamm AJ (1956) Thermal degradation of cellulose. Ind Eng Chem 48(3):413–41710.1021/ie51398a022 ↗
16. Sundqvist B, Karlsson O, Westermark U (2006) Determination of formic-acid and acetic acid concentrations formed during hydrothermal treatment of birch wood and its relation to colour, strength and hardness. Wood Sci Technol 40(7):549–56110.1007/s00226-006-0071-z ↗
17. Tjeerdsma BF, Militz H (2005) Chemical changes in hydrothermal treated wood: FTIR analysis of combined hydrothermal and dry heat treated wood. Holz Roh- Werkst 63:102–11110.1007/s00107-004-0532-8 ↗
18. UDSA (1999) Wood handbook, wood as an engineering material. United States Department of Agriculture, Forest Service, Forest Products Laboratory, Madison Wisconsin, General technical report FPL-GTR-113
19. Viitaniemi P (1997) ThermoWood modified wood for improved performance. Wood: the ecological material. In: 4th Eurowood symposium, Stockholm, Sweden, 22–23 September 1997. Swedish Institute for Wood Technology Research, Tratek, pp 67–70