Effect of grain orientation and surface wetting on vertical density profiles of thermally compressed fir and spruce
Source abstract
Abstract
The effects of grain orientation and surface wetting on wood densification by compression in a hot press were evaluated for two commercial Canadian wood species, balsam fir (Abies balsamea) and black spruce Picea mariana. The vertical density profiles (VDP) of wood densified at 180 °C could be engineered to achieve different properties depending on press closing rate, wood permeability and annual ring orientation. The lower permeability of spruce caused it to split frequently during hot pressing. For balsam fir, at a press closing time of 2 min, the compressed wood with an original grain angle of 0° (radial compression) shows widened high density bands due to collapse of low density earlywood adjacent to the dense latewood. All grain orientations show higher density areas close to the wood surfaces similar to those of wood-based composites. However, when wood was preheated without pressure for 5 min followed by a press closing time of 2 min, water migrated to and plasticized the board centre causing it to be densified while the surface density remained low. Wood surface plasticizing with water or urea solution causes some localized surface densification, but the effect was not great.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Natural Fiber Reinforced Composites · Textile materials and evaluations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Bodig J (1963) The peculiarity of compression of conifers in radial direction. Forest Prod J 13:438
2. Bodig J (1965a) The effect of anatomy on the initial stress-strain relationship in transverse compression. Forest Prod J 15(5):197–202
3. Bodig J (1965b) Effect of growth characteristics on the mechanical properties of Douglas-fir in radial compression. Holzforschung 19(3):83–8810.1515/hfsg.1965.19.3.83 ↗
4. Bodig J (1966) Stress-strain relationship for wood in transverse compression. J Mater 1(3):645–666
5. Bodig J, Jayne BA (1982) Mechanics of Wood and Wood Composites. Van Nostrand Reinhold Company, New York, America
6. Currier RA (1963) Compressibility and bond quality of western softwood veneers. Forest Prod J 13:71–80
7. Dai C, Steiner PR (1993) Compression behavior of randomly formed wood flake mats. Wood Fiber Sci 25(4):349–358
8. Dwianto W, Morooka T, Norimoto M (1998) The compressive stress relaxation of Albizia (Paraserienthes falcata Becker) wood during heat treatment (in Japanese with English abstract). Mokuzai Gakkaishi 44(6):403–409
9. Dwianto W, Morooka T, Norimoto M, Kitajima T (1999) Stress relaxation of sugi (Cryptomeria japonica D. Don) wood in radial compression under high temperature steam. Holzforschung 53:541–54610.1515/HF.1999.089 ↗
10. Dwianto W (1999) Mechanism of permanent fixation of radial compressive deformation of wood by heat or steam treatment [Dissertation]. Japan Wood Research Institute, Kyoto University, Kyoto
11. Inoue M, Norimoto M, Otsuka Y, Yamada T (1990) Surface compression of coniferous wood lumber.. A new technique to compress the surface layer. Mokuzai Gakkaishi 36(11):969–975
12. Inoue M, Norimoto M, Tanahashi M, Rowell RM (1993a) Steam or heat fixation of compressed wood. Wood Fiber Sci 25(3):224–235
13. Inoue M, Ogata S, Kawai S, Rowell RM, Norimoto M (1993b) Fixation of compressed wood using melamine-formaldehyde resin. Wood Fiber Sci 25(4):404–410
14. Inoue M (1993) Transverse compression deformation of wood and its permanent fixation [Dissertation]. Japan Wood Research Institute, Kyoto University, Kyoto
15. Inoue M, Minato K, Norimoto M (1994) Permanent fixation of compressive deformation of wood by crosslinking. Mokuzai Gakkaishi 40(9):931–936
16. Kamke FA, Casey LJ (1988) Fundamentals of flakeboard manufacture: internal-mat conditions. Forest Prod J 38(6):38–44
17. Kennedy RW (1968) Wood in transverse compression-Influence of some anatomical variables and density on behavior. Forest Prod J 18(3):36–40
18. King EG (1961) Time-dependent strain behavior of wood in tension parallel to the grain. Forest Prod J 11:156–165
19. Kunesh RH (1961) The inelastic behavior of wood: A new concept for improved panel forming processes. Forest Prod J 11:395–406
20. Lenth CA, Kamke FA (1996) Investigations of flakeboard mat consolidation / characterization the cellular structure. Wood Fiber Sci 28(2):159–167
21. Liu YX, Norimoto M, Morooka T (1993) The large compressive deformation of wood in the transverse direction 1: Relationships between stress-strain diagrams and specific gravities of wood. Mokuzai Gakkaishi 39(10):1140–1145
22. Norimoto M (1993) Large compressive deformation in wood (in Japanese). Mokuzai Gakkaishi 39(8):867–874
23. Norimoto M (1994) Heat treatment and steam treatment of wood (in Japanese). Wood Ind 49(12):588–592
24. Schniewind AP (1959) Transverse anisotropy of wood: A function of gross anatomic structure. Forest Prod J 9:350–359
25. Seborg RM, Millett MA, Stamm AJ (1945) Heat-stabilized compressed wood-(Staypak). Mech Eng 67:25–31
26. Shamaev VA, El’kov LV, Popova NI (1975) Stabilization of wood modified with urea (in Russian). Izv VUZ, Lesnoi Zh 18(5):97–101
27. Stamm AJ, Harris EE (1953) Chemical processing of wood. Chemical Publishing Co, Inc, New York, America, pp 205–261
28. Stamm AJ (1964) Wood and Cellulose Science. Ronald Press, New York, pp 317–358
29. Strickler MD (1959) Effect of press cycle and moisture content on properties of Douglas-fir flakeboard. Forest Prod J 9(7):203–215
30. Tabarsa T, Chui YH (1997) Effects of hot-pressing on properties of white spruce. Forest Prod J 47(5):71–76
31. Tabarsa T, Chui YH (2000) Stress-strain response of wood under radial compression. Test method and influence of cellular properties. Wood Fiber Sci 32(2):144–152
32. Tabarsa T, Chui YH (2001) Characterizing microscope behavior of wood under transverse compression. Effect of species and loading direction. Wood Fiber Sci 33(2):223–232
33. Wang JY, Zhao GJ (1999) The mechanism of formation, recovery and permanent fixation of wood set (in Chinese with English abstract). J Beijing For Univ 21(3):71–77
34. Wang JY, Zhao GJ, Iida I (2000) Effect of oxidation on heat fixation of compressed wood of China fir. For Stud China 2(1):73–79
35. Wang JY (2000) Fixation of compressed wood of Chinese fir by heat treatment and gamma irradiation [Dissertation]. Beijing Forestry University, China
36. Wang JY, Zhao GJ (2001) Fixation and creep of compressed wood of Chinese fir irradiated with gamma rays. For Stud China 3(1):58–65
37. Wang S, Winistorfer PM (2000) Fundamentals of vertical density profile formation in wood composites. Part 2. Methodology of vertical density formation under dynamic conditions. Wood Fiber Sci 32(2):220–238
38. Winistorfer PM, Young TM, Walker E (1996) Modeling and comparing vertical density profiles. Wood Fiber Sci 28(1):133–141
39. Winistorfer PM, Moschler WW, Wang S, Depaula E, Bledsoe BL (2000) Fundamentals of vertical density profile formation in wood composites. Part 1. In-situ density measurement of the consolidation process. Wood Fiber Sci 32(2):209–219
40. Wolcott MP, Kamke FA, Dillard DA (1990) Fundamentals of flakeboard manufacture: Viscoelastic behavior of the wood components. Wood Fiber Sci 22(4):345–361
41. Wong ED, Zhang M, Wang Q, Kawai S (1999) Formation of the density profile and its effects on the properties of particleboard. Wood Fiber Sci 33(2):327–34010.1007/s002260050119 ↗
42. Youngs RL (1957) Mechanical properties of red oak related to drying. Forest Prod J 7:315–324