Influence of curing temperature on the bonding strength of heat-treated plywood made with melamine-urea-formaldehyde and phenol–formaldehyde resins
Source abstract
Abstract
Melamine-urea-formaldehyde resin (MUF) and phenol–formaldehyde resin (PF) were prepared in the laboratory. Their curing behavior was analyzed by differential scanning calorimetry (DSC). MUF resin was then cured at 110, 120, and 130 °C, while PF resin was cured at 135, 150, and 165 °C. The dry and wet bonding strength of plywood made by hot-pressing at different temperatures and heat-treatment at 200 and 250 °C were measured. DSC results show that the PF resin had a more obvious exothermic peak than the MUF resin during heat scanning. Fourier transform infrared spectroscopy analysis shows that MUF and PF resins cured at higher temperature undergo more condensation reactions. Solvent dissolution test shows that PF resin cured at 135 °C has a weight retention similar to that of resins cured at 150 and 165 °C. However, using a temperature of 120 °C was better than 110 and 130 °C for MUF resin. Thermogravimetric analysis results show that PF resin had better heat resistance than MUF resin. The curing temperature did not influence the thermal degradation behavior of cured resins. However, increasing the curing temperature resulted in higher thermal stability. Heat treatment decreased the bonding strength of plywood. However, the bonding strength still met the requirement of the CNS 1349 standard when heat-treated at 200 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Lignin and Wood Chemistry · Dyeing and Modifying Textile Fibers · Phytochemicals and Antioxidant Activities
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Alén R, Kuoppala E, Oesch P (1996) Formation of the main degradation compound groups from wood and its components during pyrolysis. J Anal Appl Pyrol 36:137–14810.1016/0165-2370(96)00932-1 ↗
2. Ayadi N, Lejeune F, Charrier F, Charrier B, Merlin A (2003) Color stability of heat-treated wood during artificial weathering. Holz Roh Werkst 61:221–22610.1007/s00107-003-0389-2 ↗
3. Bekhta P, Niemz P (2003) Effect of high temperature on the change in color, dimensional stability and mechanical properties of spruce wood. Holzforschung 57:539–54610.1515/HF.2003.080 ↗
4. Boonstra MJ, Pizzi A, Zomers F, Ohlmeyer M, Paul W (2006) The effects of a two stage heat treatment process on the properties of particleboard. Holz Roh Werkst 64:157–16410.1007/s00107-005-0055-y ↗
5. Borrega M, Kärenlampi PP (2008) Mechanical behavior of heat-treated spruce (Picea abies) wood at constant moisture content and ambient humidity. Holz Roh Werkst 66:63–6910.1007/s00107-007-0207-3 ↗
6. Borrega M, Kärenlampi PP (2010) Hygroscopicity of heat-treated Norway spruce (Picea abies) wood. Eur J Wood Prod (2010) 68:233–23510.1007/s00107-009-0371-8 ↗
7. Candelier K, Thevenon MF, Petrissans A, Dumarcay S, Gerardin P, Petrissans M (2016) Control of wood thermal treatment and its effects on decay resistance: a review. Ann Forest Sci 73:571–58310.1007/s13595-016-0541-x ↗
8. Chauvet J, Asua JM, Leiza JR (2005) Independent control of sol molar mass and gel content in acrylate polymer/latexes. Polymer 46:9555–956110.1016/j.polymer.2005.08.061 ↗
9. Costa L, di Montelera LR, Camino G, Weil ED, Pearce EM (2007) Structure-charring relationship in phenol-formaldehyde type resins. Polym Degrad Stabil 56:23–3510.1016/S0141-3910(96)00171-1 ↗
10. Dubey MK, Pang S, Walker J (2011) Effect of oil heating age on colour and dimensional stability of heat treated Pinus radiate. Eur J Wood Prod 69:255–26210.1007/s00107-010-0431-0 ↗
11. Esteves BM, Pereira HM (2009) Wood modification by heat treatment: a review. BioResources 4:370–40410.15376/biores.4.1.Esteves ↗
12. Esteves BM, Domingos IJ, Pereira HM (2008) Pine wood modification by heat treatment in air. BioResources 3:142–15410.15376/biores.3.1.142-154 ↗
13. Hill CAS (2006) Wood modification: chemical, thermal and other processes. Wiley, Chichester10.1002/0470021748 ↗
14. Jebrane M, Sèbe G (2007) A novel simple route to wood acetylation by transesterification with vinyl acetate. Holzforschung 61:143–14710.1515/HF.2007.026 ↗
15. Jebrane M, Pichavant F, Sèbe G (2011) A comparative study on the acetylation of wood by reaction with vinyl acetate and acetic anhydride. Carbohyd Polym 83:339–34510.1016/j.carbpol.2010.07.035 ↗
16. Kandelbauer A, Despres A, Pizzi A, Taudes I (2007) Testing by fourier transform infrared species variation during melamine-urea-formaldehyde resin preparation. J Appl Polym Sci 106:2192–219710.1002/app.26757 ↗
17. Křístková M, Filipb P, Weissa Z, Peterc R (2004) Influence of metals on the phenol–formaldehyde resin degradation in friction composites. Polym Degrad Stabil 84:49–6010.1016/j.polymdegradstab.2003.09.012 ↗
18. Kudanga T, Prasetyo EN, Widsten P, Kandelbauer A, Jury S, Heathcote C, Sipilä J, Weber H, Nyanhongob GS, Guebitzb GM (2010) Laccase catalyzed covalent coupling of fluorophenols increases lignocellulose surface hydrophobicity. Bioresour Technol 101:2793–289910.1016/j.biortech.2009.12.002 ↗
19. Kudanga T, Nyanhongob GS, Guebitzb GM, Burtona S (2011) Potential applications of laccase-mediated coupling and grafting reactions: a review. Enzyme Microb Technol 48:195–20810.1016/j.enzmictec.2010.11.007 ↗
20. Mamiński MŁ, Król M, McDonald AG, McIlroy DN, Niraula IB, Czechowska J, Parzuchowski P (2013) Thermally initiated solvent-free radical modification of beech (Fagus sylvatica) wood. Wood Sci Technol 47:1019–103110.1007/s00226-013-0555-6 ↗
21. Nakano T, Miyazaki J (2003) Surface fractal dimensionality and hygroscopicity for heated wood. Holzforschung 57:289–29410.1515/HF.2003.043 ↗
22. Pétrissans M, Gérardin P, El bakali I, Serraj M (2003) Wettability of heat-treated wood. Holzforschung 57:301–30710.1515/HF.2003.045 ↗
23. Ramiah MV (1970) Thermogravimetric and differential thermal analysis of cellulose, hemicellulose, and lignin. J Appl Polym Sci 14:1323–133710.1002/app.1970.070140518 ↗
24. Rapp AO, Brischke C, Welzbacher CR (2006) Interrelationship between the severity of heat treatments and sieve fractions after impact ball milling: a mechanical test for quality control of thermally modified wood. Holzforschung 60:64–7010.1515/HF.2006.012 ↗
25. Rowell RM (1986) Vapor phase acetylation of southern pine, douglas-fir, and aspen wood flakes. J Wood Chem Technol 6:293–30910.1080/02773818608085228 ↗
26. Sandberg D, Kutnar, A (2016) Thermally modified timber: recent developments in Europe and north America. Wood Fiber Sci 48:28–39
27. Sernek M, Boonstra M, Pizzi A, Despres A (2008) Bonding performance of heat treated wood with structural adhesives. Holz Roh Werkst 66:173–18010.1007/s00107-007-0218-0 ↗
28. Shi JL, Kocaefe D, Zhang J (2007) Mechanical behaviour of Québecwood species heat-treated using ThermoWood process. Holz Roh Werkst 65:255–25910.1007/s00107-007-0173-9 ↗
29. Siimer K, Kaljuvee T, Christjanson P, Lasn I (2006) Curing of urea-formaldehyde resins on a wood substrate. J Therm Anal Calorim 84:71–7710.1007/s10973-005-7185-7 ↗
30. Trick KA, Saliba TE (1995) Mechanisms of the pyrolysis of phenolic resin in a carbon/phenolic composite. Carbon 33:1509–151510.1016/0008-6223(95)00092-R ↗
31. Trick KA, Saliba TE, Sandhu SS (1997) A kinetic model of the pyrolysis of phenolic resin in a carbon/phenolic composite. Carbon 35:393–40110.1016/S0008-6223(97)89610-8 ↗
32. Walker JF (1975) Formaldehyde. Huntinton, New York
33. Weiland JJ, Guyonnet R (2003) Study of chemical modifications and fungi degradation of thermally modified wood using DRIFT spectroscopy. Holz Roh Werkst 61:216–22010.1007/s00107-003-0364-y ↗
34. Widsten P, Heathcote C, Kandelbauer A, Guebitz G, Nyanhongo GS, Prasetyo EN, Kudanga T (2010) Enzymatic surface functionalisation of lignocellulosic materials with tannins for enhancing antibacterial properties. Process Biochem 45:1072–108110.1016/j.procbio.2010.03.022 ↗
35. Zigon J, Pizzi A, Zhang H, Sega B, Cop M, Sernek, M (2015) The influence of heat and chemical treatments of beech wood on the shear strength of welded and UF bonded specimens. Eur J Wood Prod 73:685–68710.1007/s00107-015-0930-0 ↗