Physical and mechanical properties of Paulownia clone in vitro 112
Source abstract
Abstract
Abstract For the Paulownia Clone in vitro 112 hybrid to be used in the wood industry, it is necessary to know its basic properties. Its air dry density of 231 kg/m3 is nearly 20% lower than that of Paulownia tomentosa. Its average compressive strength is 19.9 MPa, its shear strength is 4.1 MPa, the static modulus of rupture (MOR) is 32.3 MPa, and the modulus of elasticity (MOE) is 3800 MPa. Its volumetric shrinkage is 8.47%, with longitudinal 0.6%, radial 3.2% and tangential 5.0%. The ratio of tangential to radial shrinkage is very favorable, just 1.6.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. DIN 52184 (1979) Testing of wood—determination of swelling and shrinkage. Beuth Verlag GmbH, Berlin
2. DIN 52185 (1976) Testing of wood—compression test parallel to grain. Beuth Verlag GmbH, Berlin
3. DIN 52186 (1978) Testing of wood—bending test. Beuth Verlag GmbH, Berlin
4. DIN 52187 (1979) Testing of wood—determination of ultimate shearing stress parallel to grain. Beuth Verlag GmbH, Berlin
5. DIN 68364 (2003) Characteristics of wood species—bulk density, modulus of elasticity and strengths. Beuth Verlag GmbH, Berlin
6. Koman Sz, Feher S (2017) Physical and mechanical properties of paulownia tomentosa wood planted in hungaria. Wood Res 62(2):335–340