Abstract
Abstract Wood modification with thermosetting resins results in improved dimensional stability and durability. However, the treatment does not enhance fire resistance. To address this, Scots pine sapwood (Pinus sylvestris L.) was impregnated with thermosetting resins such as 1,3-dimethylol-4,5-dihydroxyethyleneurea, phenol-formaldehyde resin and melamine-formaldehyde resin, along with a phosphorus polyol as the flame retardant. Both weight percent gain and cell wall bulking were measured to investigate the deposition of resin and phosphorus polyol. Fire resistance was assessed through thermogravimetric analysis, Bunsen burner test and mass loss calorimeter. The inclusion of a phosphate polyol improved thermal stability, reduced flammability and heat release. Melamine-formaldehyde resin combined with phosphorus polyol demonstrated self-extinguishing capability with the heat release rate comparable to non-combustible materials inside 400 s. Moreover, the total heat release within 600 s shows an 84% reduction compared to untreated wood.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Flame retardant materials and properties · Fire dynamics and safety research · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Alongi J, Han Z, Bourbigot S (2015) Intumescence: tradition versus novelty. A comprehensive review. Prog Polym Sci 51:28–73. https://doi.org/10.1016/j.progpolymsci.2015.04.01010.1016/j.progpolymsci.2015.04.010 ↗
2. Chung Y-J (2010) Comparison of combustion properties of native wood species used for Fire pots in Korea. J Ind Eng Chem 16:15–1910.1016/j.jiec.2010.01.031 ↗
3. Dorieh A, Pour MF, Movahed SG, Pizzi A, Selakjani PP, Kiamahalleh MV, Hatefnia H, Shahavi MH, Aghaei R (2022) A review of recent progress in melamine-formaldehyde resin based nanocomposites as coating materials. Prog Org Coat 165:10676810.1016/j.porgcoat.2022.106768 ↗
4. Emmerich L, Bollmus S, Militz H (2019) Wood modification with DMDHEU (1.3-dimethylol-4.5-dihydroxyethyleneurea) – state of the art, recent research activities and future perspectives. Wood Mater Sci Eng 14:3–18. https://doi.org/10.1080/17480272.2017.141790710.1080/17480272.2017.1417907 ↗
5. Gao J, Liu Y, Yang L (1999) Thermal stability of boron-containing phenol formaldehyde resin. Polym Degrad Stab 63:19–22. https://doi.org/10.1016/S0141-3910(98)00056-110.1016/S0141-3910(98)00056-1 ↗
6. Girods P, Dufour A, Rogaume Y, Rogaume C, Zoulalian A (2008) Thermal removal of nitrogen species from wood waste containing urea formaldehyde and melamine formaldehyde resins. J Hazard Mater 159:210–221. https://doi.org/10.1016/j.jhazmat.2008.02.00310.1016/j.jhazmat.2008.02.003 ↗
7. Green J (1992) A review of phosphorus-containing flame retardants. J Fire Sci 10:470–48710.1177/073490419201000602 ↗
8. Guillaume E, Dréan V, Girardin B, Benameur F, Fateh T (2020) Reconstruction of Grenfell Tower Fire. Part 1: lessons from observations and determination of work hypotheses. Fire Mater 44:3–14. https://doi.org/10.1002/fam.276610.1002/fam.2766 ↗
9. Hakkarainen T, Kokkala MA (2001) Application of a one-dimensional thermal flame spread model on predicting the rate of heat release in the SBI test. Fire Mater 25:61–70. https://doi.org/10.1002/fam.76010.1002/fam.760 ↗
10. Hasburgh LE, White RH, Dietenberger MA, Boardman CR, Forest US, Forest S, Pinchot OG (2015) Comparison of the heat release rate from the mass loss calorimeter to the cone calorimeter for wood-based materials. Proceedings of the Fire and Materials
11. He G, Riedl B (2004) Curing kinetics of phenol formaldehyde resin and wood-resin interactions in the presence of wood substrates. Wood Sci Technol 38:69–8110.1007/s00226-003-0221-5 ↗
12. Holme I, Patel SR (1982) 17—thermogravimetric analysis of n-methylolated resin finishes and diammonium hydrogen orthophosphate. J Text Inst 73:177–182. https://doi.org/10.1080/0040500820865893510.1080/00405008208658935 ↗
13. Jiang T, Feng X, Wang Q, Xiao Z, Wang F, Xie Y (2014) Fire performance of oak wood modified with N-methylol resin and methylolated guanylurea phosphate/boric acid-based Fire retardant. Constr Build Mater 72:1–6. https://doi.org/10.1016/j.conbuildmat.2014.09.00410.1016/j.conbuildmat.2014.09.004 ↗
14. Komatsu T (2001) The first synthesis and characterization of Cyameluric High polymers. Macromol Chem Phys 202:19–25. https://doi.org/10.1002/1521-3935(20010101)202:1<19::AID-MACP19>3.0.CO;2-G10.1002/1521-3935(20010101)202:1<19::AID-MACP19>3.0.CO;2-G ↗
15. Kraaijeveld A, Log T (2017) Vertical Flame Spread in Wooden Corners as a Function of Fuel Moisture Content. In Proceedings of the 15th International Conference Fire and Materials, San Francisco, CA, USA; pp. 307–318
16. Kurkowiak K, Wu M, Emmerich L, Militz H (2023) Fire-retardant properties of wood modified with sorbitol, citric acid and a phosphorous-based system. Holzforschung 77:38–44. https://doi.org/10.1515/hf-2022-011410.1515/hf-2022-0114 ↗
17. Li W, Chen L, Li Y, Li X (2020) Bamboo modification with 1, 3-dimethylol-4, 5-dihydroxyethyleneurea (DMDHEU) catalyzed by maleic anhydride. J Wood Chem Technol 40:126–13510.1080/02773813.2019.1697293 ↗
18. Lin C-F, Karlsson O, Mantanis GI, Sandberg D (2020) Fire performance and leach resistance of pine wood impregnated with guanyl-urea phosphate/boric acid and a melamine-formaldehyde resin. Eur J Wood Prod 78:107–111. https://doi.org/10.1007/s00107-019-01483-y10.1007/s00107-019-01483-y ↗
19. Lin C, Karlsson O, Martinka J, Rantuch P, Garskaite E, Mantanis GI, Jones D, Sandberg D (2021) Approaching highly leaching-resistant Fire-Retardant Wood by in situ polymerization with Melamine Formaldehyde Resin. ACS Omega 6:12733–12745. https://doi.org/10.1021/acsomega.1c0104410.1021/acsomega.1c01044 ↗
20. Östman B (2023) Acceptance criteria for products according to the cone calorimeter. Fire Mater 47:848–850. https://doi.org/10.1002/fam.311910.1002/fam.3119 ↗
21. Praticò Y, Ochsendorf J, Holzer S, Flatt RJ (2020) Post-fire restoration of historic buildings and implications for Notre-Dame de Paris. Nat Mater 19:817–820. https://doi.org/10.1038/s41563-020-0748-y10.1038/s41563-020-0748-y ↗
22. Pries M, Mai C (2013) Fire resistance of wood treated with a cationic silica sol. Eur J Wood Prod 71:237–244. https://doi.org/10.1007/s00107-013-0674-710.1007/s00107-013-0674-7 ↗
23. Rowell RM (ed) (2012) - Thermal properties, Combustion, and Fire Retardancy of Wood. Handbook of Wood Chemistry and Wood composites. CRC Press, pp 144–167. https://doi.org/10.1201/b12487-1110.1201/b12487-11 ↗
24. Sathre R, González-García S (2014) Life cycle assessment (LCA) of wood-based building materials. Eco-efficient Construction and Building materials. Elsevier, pp 311–337. https://doi.org/10.1533/9780857097729.2.31110.1533/9780857097729.2.311 ↗
25. Sauerbier P, Mayer AK, Emmerich L, Militz H (2020) Fire Retardant Treatment of Wood – State of the art and future perspectives. In: Makovicka Osvaldova L, Markert F, Zelinka SL (eds) Wood & Fire Safety. Springer International Publishing, Cham, pp 97–102. https://doi.org/10.1007/978-3-030-41235-7_1410.1007/978-3-030-41235-7_14 ↗
26. Schartel B (2010) Phosphorus-based Flame Retardancy mechanisms—old hat or a starting point for Future Development? Materials 3:4710–4745. https://doi.org/10.3390/ma310471010.3390/ma3104710 ↗
27. Shams MI, Yano H (2011) Compressive deformation of phenol formaldehyde (PF) resin-impregnated wood related to the molecular weight of resin. Wood Sci Technol 45:73–81. https://doi.org/10.1007/s00226-010-0310-110.1007/s00226-010-0310-1 ↗
28. Steen-Hansen A, Kristoffersen B (2007) Prediction of Fire classification for wood based products. A multivariate statistical approach based on the cone calorimeter. Fire Mater 31:207–223. https://doi.org/10.1002/fam.93410.1002/fam.934 ↗
29. Ullah S, Bustam MA, Nadeem M, Naz MY, Tan WL, Shariff AM (2014) Synthesis and thermal degradation studies of Melamine Formaldehyde resins. Sci World J 2014:1–6. https://doi.org/10.1155/2014/94050210.1155/2014/940502 ↗
30. Wang J, Jiang H, Jiang N (2009) Study on the pyrolysis of phenol-formaldehyde (PF) resin and modified PF resin. Thermochimica Acta 496:136–142. https://doi.org/10.1016/j.tca.2009.07.01210.1016/j.tca.2009.07.012 ↗
31. Wu M, Emmerich L, Kurkowiak K, Militz H (2023) Fire resistance of pine wood treated with phenol-formaldehyde resin and phosphate-based flame retardant. Wood Mater Sci Eng 1–7. https://doi.org/10.1080/17480272.2023.220537910.1080/17480272.2023.2205379 ↗
32. Xie Y, Liu N, Wang Q, Xiao Z, Wang F, Zhang Y, Militz H (2014) Combustion behavior of oak wood (Quercus mongolica L.) modified by 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU). Holzforschung 68:881–887. https://doi.org/10.1515/hf-2013-022410.1515/hf-2013-0224 ↗
33. Xie Y, Xu J, Militz H, Wang F, Wang Q, Mai C, Xiao Z (2016) Thermo-oxidative decomposition and combustion behavior of scots pine (Pinus sylvestris L.) sapwood modified with phenol- and melamine-formaldehyde resins. Wood Sci Technol 50:1125–1143. https://doi.org/10.1007/s00226-016-0857-610.1007/s00226-016-0857-6 ↗
34. Xu Q, Chen L, Harries KA, Zhang F, Liu Q, Feng J (2015) Combustion and charring properties of five common constructional wood species from cone calorimeter tests. Constr Build Mater 96:416–427. https://doi.org/10.1016/j.conbuildmat.2015.08.06210.1016/j.conbuildmat.2015.08.062 ↗
35. Yalinkilic MK, Imamura Y, Takahashi M, Yalinkilic AC (1999) In situ polymerization of vinyl monomers during compressive deformation of wood treated with boric acid to delay boron leaching. For Prod J 49:43
36. Yue K, Chen Z, Lu W, Liu W, Li M, Shao Y, Tang L, Wan L (2017) Evaluating the mechanical and fire-resistance properties of modified fast-growing Chinese fir timber with boric-phenol-formaldehyde resin. Constr Build Mater 154:956–962. https://doi.org/10.1016/j.conbuildmat.2017.08.03510.1016/j.conbuildmat.2017.08.035 ↗
37. Yue K, Wu J, Xu L, Tang Z, Chen Z, Liu W, Wang L (2020) Use impregnation and densification to improve mechanical properties and combustion performance of Chinese fir. Constr Build Mater 241:118101. https://doi.org/10.1016/j.conbuildmat.2020.11810110.1016/j.conbuildmat.2020.118101 ↗
38. Zelinka SL, Altgen M, Emmerich L, Guigo N, Keplinger T, Kymäläinen M, Thybring EE, Thygesen LG (2022) Rev Wood Modif Wood Functionalization Technol Forests 13:1004. https://doi.org/10.3390/f1307100410.3390/f13071004 ↗
39. Zhu H, Xu S (2020) Preparation of flame-retardant rigid polyurethane foams by combining modified melamine–formaldehyde resin and phosphorus flame retardants. ACS Omega 5:9658–966710.1021/acsomega.9b03659 ↗