An investigation into collapse and shrinkage behaviour of Eucalyptus grandis and Eucalyptus grandis-urophylla wood
Source abstract
Abstract
In this study, the variation of collapse and shrinkage both radially and along the height of trees was investigated and their relationships with warp in the sawn boards as well as the basic physical properties of wood (density, moisture content, permeability, extractives contents and heartwood/sapwood ratio) were determined. Seventy trees of Eucalyptus grandis and Eucalyptus grandis-urophylla were selected based on age (young, medium and old) and genetics (improved and unimproved). Collapse and shrinkage were measured on both wedges and sawn boards. In terms of the causal factors in wedges, there were weak but significant correlations between collapse and extractives content, density, and permeability, while shrinkage showed stronger correlations with the same parameters. The results showed that on boards, collapse and shrinkage varied depending on group (age x genetics), log position and the radial position of the boards. The radial and tangential collapse measured on wedges did not correspond well with collapse observed in sawn board specimens. Future research should focus on understanding collapse in Eucalyptus grandis and Eucalyptus grandis-urophylla on an anatomical level including the clear directional nature as well as the influence that specimen geometry has on collapse.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Tree Root and Stability Studies · Bamboo properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Akbari A, Hill RJ, van de Ven TGM (2015) An elastocapillary model of wood-fibre collapse. Proc R Soc A 471:2015018410.1098/rspa.2015.0184 ↗
2. Ananías RA, Sepúlveda-Villarroel V, Pérez-Peña N, Leandro-Zuñiga L, Salvo-Sepúlveda L, Salinas-Lira C, Cloutier A, Elustondo DM (2014) Collapse of Eucalyptus nitens wood after drying depending on the radial location within the stem. Dry Technol 32(14):1699–170510.1080/07373937.2014.924132 ↗
3. Avramidis S (2007) Bound water migration in wood. In: Perré P (ed) Fundamentals of wood drying. A.R.BO.LOR, Nancy, pp 105–124
4. Bao FC, Jiang ZH, Jiang XM, Lu XX, Luo X, Zhang SY (2001) Differences in wood properties between juvenile wood and mature wood in 10 species grown in China. Wood Sci Technol 35:363–37510.1007/s002260100099 ↗
5. Bariska M (1992) Collapse phenomena in Eucalypts. Wood Sci Technol 26:165–17910.1007/BF00224290 ↗
6. Barkas WW (1941) Wood water relationships, VI. The influence of ray cells on the shrinkage of wood. Trans Faraday Soc 37:535–54710.1039/tf9413700535 ↗
7. Bateson RG (1946) Timber drying and the behaviour of seasoned timber in use, 2nd edn. Lockwood, London
8. Bhat KM, Bhat KV, Dhamodaran TK (1990) Wood density and fiber length of Eucalyptus grandis grown in Kerala. India Wood Fiber Sci 22(1):54–61
9. Blakemore Ph, Langrish TAG (2007) Effect of mean moisture content on the steam reconditioning of collapsed Eucalyptus regnans. Wood Sci Technol 41:87–9810.1007/s00226-006-0093-6 ↗
10. Bossu J, Beauchene J, Estevez JY, Duplais C, Clair B (2016) New insights on wood dimensional stability influenced by secondary metabolites: the case of fast-growing tropical species Bagassa guinanensis Aubli. PloS one 11(3): e0150777. https://doi.org/10.1371/journal.pone.015077710.1371/journal.pone.0150777 ↗
11. Calil C Jr, Rocco Lahr FA, Dias AA (2003) Dimensionamento de elementos estruturais de madeira [Design of wooden structural elements]. Manole Ltda, Rio de Janeiro
12. Chafe SC (1985) The distribution and interrelationship of collapse, volumetric shrinkage, moisture content and density in trees of Eucalyptus regnans F. Muell. Wood Sci Technol 19:329–34510.1007/BF00350810 ↗
13. Chamberlain D, Essop H, Hougaard C, Malherbe S, Walker R (2005) Part I: The contribution, costs and development opportunities of the forestry, timber, pulp and paper industries in South Africa. Final report–29 June. Genesis Analytics (Pty) Ltd, Johannesburg
14. Cherelli SG, Sartori MMP, Prospero AG, Ballarin AW (2018) Heartwood and sapwood in Eucalyptus trees: non-conventional approach to wood quality. An Acad Bras Ciênc 90(1):425–43810.1590/0001-3765201820160195 ↗
15. Choong ET (1969) Effect of extractives on shrinkage and other hygroscopic properties of ten Southern pine woods. Wood Fiber Sci 1(2):124–133
16. Crafford PL, Wessels CB (2016) The potential of young, green finger-jointed Eucalyptus grandis lumber for roof truss manufacturing. South for J 78(1):60–71
17. Crickmay and Associates (2005) Study of supply and demand of industrial roundwood in South Africa. Crickmay and Associates (Pty) Ltd, Hilton
18. da Silva MR, de Oliveira MG, Deiner J, Calil Junior C (2010) Permeability measuremens of Brazilian Eucalyptus. Mater Res 13(3):281–28610.1590/S1516-14392010000300002 ↗
19. Derome D, Griffa M, Koebel M (2011) Hysteretic swelling of wood at cellular scale probed by phase-contrast X-ray tomography. J Struct Biol 173:180–19010.1016/j.jsb.2010.08.011 ↗
20. Emaminasab M, Tarmian A, Pourtahmasi K (2015) Permeability of poplar normal wood and tension wood bio-incised by Physisporinus vitreus and Xylaria longipes. Int Biodeterior Biodegrad 105:178–18410.1016/j.ibiod.2015.09.003 ↗
21. Engelund ET, Thygesen LG, Svensson S, Hill CAS (2013) A critical discussion of the physics of wood-water interactions. Wood Sci Technol 47:141–16110.1007/s00226-012-0514-7 ↗
22. Githiomi JK, Dougal E (2012) Analysis of heartwood-sapwood dermacation methods and variation of sapwood and heartwood within and between 15-year-old plantation grown Eucalyptus regnans. Int J Appl Sci Technol 2(8):63–70
23. Githiomi JK, Kariuki JG (2010) Wood basic density of Eucalyptus grandis from plantations in central Rift valley, Kenya: variation with age, height level and between sapwood and heartwood. J Trop for Sci 22(3):281–286
24. Greenhill WL (1936) Shrinkage of Australian timbers. Part 1. A new method for determining shrinkages and shrinkage figures of a number of Australian species. CSIR, Australia, Division of Forest Products, Technological Paper No. 33.
25. Hein PRG, Siva JRM, Brancheriau L (2013) Correlations among microfibril angle, density, modulus of elasticity, modulus of rapture and shrinkage in 6-year-old Eucalyptus urophylla x E. grandis. Maderas Cierc Y Technol 15(1):171–182
26. Ilic J (1999) Shrinkage-related degrade and its association with some physical properties in Eucalyptus regnans F. Muell. Wood Sci Technol 33:425–43710.1007/s002260050127 ↗
27. Innes TC (1995) Collapse free pre-drying of Eucalyptus regnans F. Muell. Holz Roh- Werkst 53:403–40610.1007/s001070050119 ↗
28. Innes TC (1996) Improving seasoned hardwood timber quality. PhD thesis, University of Tasmania, Hobart.
29. Jacobs MR (1955) Growth habits of the Eucalypts. Commonwealth Forestry and Timber Bureau, Canberra
30. Kauman WG (1960) Contributions to the theory of cell collapse in wood: Investigations with Eucalyptus regnans. Austral J Appl Sci 11(1):122–145
31. Kauman WG (2002) Contribution to the theory of cell collapse in wood: investigations with eucalyptus regnans. Maderas Cienc y Tecnol 4:77–99
32. Kauman WG (1964) Cell collapse in wood. CSIRO Aust. Div. Forest Prod. Reprint No. 566. CSIRO Transl. Holz Roh-Werkst 22: 183–196, 465–47210.1007/BF02605572 ↗
33. Kord B, Kialashaki A, Kord B (2010) The within-tree variation in wood density and shrinkage, and their relationship in Populus euramericana. Turk J Agric for 34:121–126
34. Kumar A, Dhillon GPS (2014) Variation of sapwood and heartwood content in half-sib properties of Eucalyptus tereticornis Sm. Indian J Nat Prod Resour 5(4):338–344
35. Lloyd JA (1978) Distribution of extractives in Pinus radiata earlywood and latewood. NZ J for Sci 8:288
36. Lukasek J, Zeidler A, Barcik S (2012) Shrinkage of grand fir wood and its variability within the stem. Drevna Ind 63(2):121–12810.5552/drind.2012.1140 ↗
37. Machado GO, Calil C Jr, Polito W, Pawlicka A (2006) Preservante natural de madeira para uso na construção civil : óleo de Neem [Natural wood preservative for use in construction: neem oil]. Minerva 3(1):1–8
38. Malan FS (1984) Studies on the phenotypic variation in growth stress intensity and its association with tree and wood properties of South African grown Eucalyptus grandis (Hill ex Maiden). Ph.D. thesis, University of Stellenbosch.
39. Malan FS (1993) The wood properties and qualities of three South African-grown eucalypt hybrids. S Afr for J 167(1):35–44
40. Malan FS (1994) The wood properties and quality of Pinus pringlei Shaw and P. greggii engel compared with that of P. patula and P. elliottii grown in South Africa. South Afr for J 171(1):43–52
41. Malan FS (2001) The wood quality of Pinus chiapensis (Mart.) Andresen grown in the Mpumalanga forest region. South Afr for J 192(1):51–57
42. Malan FS (2003) The wood quality of the South African timber resource for high-value solid wood products and its role in sustainable forestry. S Afr for J 198:53–62
43. Miranda I, Gominho J, Pereira H (2009) Variation of heartwood and sapwood in 18-year-old Eucalyptus globulus trees grown with different spacings. Trees 23:367–37210.1007/s00468-008-0285-9 ↗
44. Miranda I, Sousa V, Pereira H (2011) Wood properties of teak (Tectona grandis) from a mature unmanaged stand in East Timor. J Wood Sci 57:171–17810.1007/s10086-010-1164-8 ↗
45. Morais MC, Pereira H (2007) Heartwood and sapwood variation in Eucalyptus globulus labill. Trees at the end of rotation for pulpwood production. Ann for Sci 64:665–67110.1051/forest:2007045 ↗
46. Morais MC, Pereira H (2012) Variation of extractives content in heartwood and sapwood of Eucalyptus globulus trees. Wood Sci Technol 46(4):709–71910.1007/s00226-011-0438-7 ↗
47. Mugabi P (2007) Moisture content and drying defects in kiln-dried Eucalyptus grandis poles. Ph.D. Forestry (Wood Science) thesis, Stellenbosch University, South Africa.
48. Nocetti M, Pröller M, Brunetti M, Dowse GP, Wessels CB (2017) Investigating the potential of strength grading green Eucalyptus grandis lumber using multi-sensor technology. BioResources 12(4):9273–928610.15376/biores.12.4.9273-9286 ↗
49. Oliveira JTS, Hellmeister JC, Tomazello Filho M (2005) Variation of the moisture content and specific gravity in the wood of seven Eucalypt species. Revista Árvore 29(1):115–12710.1590/S0100-67622005000100013 ↗
50. Pagel C, Lenner R, Wessels CB (2020) Investigation into material resistance factors and properties of young, engineered Eucalyptus grandis timber. Constr Build Mater 230:1–1010.1016/j.conbuildmat.2019.117059 ↗
51. Pankevicius ER (1961) Influence of position in tree on recoverable collapse in wood. For Prod J 11(3):131–132
52. Priadi IT (2001) A study of pre-treatment in the drying of regrowth Eucalyptus obliqua L’herit. MSc thesis. University of Tasmania.
53. SANS 17801–1 (2010) Sawn Eucalyptus timber: proof-graded structural timber. SABS Standard Division, Pretoria
54. SANS 1783–1 (2009) South African National Standard. Sawn softwood timber, part 1: general requirements. SABS Standard Division, Pretoria
55. SANS 1783–2 (2012) Sawn softwood timber: stress-graded structural timber and for frame wall construction. SABS standard division, Pretoria
56. SANS 1783–3 (2010) Sawn softwood timber: industrial timber. SABS Standard Division, Pretoria
57. Schulgasser K, Witztum A (2015) How the relationship between density and shrinkage of wood depends on its microstructure. Wood Sci Technol 49:389–40110.1007/s00226-015-0699-7 ↗
58. Siau JF (1995) Wood: Influence of moisture on physical properties. Polytechnic Institute and State University, Blacksburg, pp 39–58
59. TAPPI (1994) TAPPI T 207 om-93: water solubility of wood and pulp. TAPPI Standard Method, Atlanta
60. Tarmian A, Zahedi Tajrishi I, Oladi R, Efhamisisi D (2020) Treatability of wood for pressure treatment processes: a literature review. Eur J Wood Prod 78:635–66010.1007/s00107-020-01541-w ↗
61. Taylor FW (1973) Variation in anatomical properties of South African grown Eucalyptus grandis. Appita 27:171–178
62. Tiemann D (1929) How to restore collapsed timber. Lumber Work 5(57):3–44
63. Tsoumis G (1991) Science and technology of wood, 1st edn. Kessel, Remagen-Oberwinter
64. Vermaas HF, Bariska M (1994) Collapse during low temperature drying of Eucalyptus grandis W. Hill and Pinus silvestris L. In: Proceedings IUFRO Wood Drying Conference, Rotorua, New Zealand, pp 141– 150
65. Washusen R, Ades P, Evans R, Ilic J, Vinden P (2001) relationships between density, shrinkage, extractives content and microfibril angle in tension wood from three provenances of 10-year-old Eucalyptus globulus Labill. Holzforschung 55(2):176–18210.1515/HF.2001.029 ↗
66. Wessels CB, Crafford PL, Du Toit B et al (2016) Variation in physical and mechanical properties from three drought tolerant Eucalyptus species grown on the dry west coast of Southern Africa. Eur J Wood Prod 74:563–57510.1007/s00107-016-1016-3 ↗
67. Wessels CB, Nocetti M, Brunetti M, Crafford PL, Pröller M, Dugmore MK, Pagel C, Lenner R, Naghizadeh Z (2020) Green-glued engineered products from fast growing Eucalyptus trees: a review. Eur J Wood Prod 78:933–94010.1007/s00107-020-01553-6 ↗
68. Wilkins AP, Horne R (1991) Wood-density variation of young plantation-grown Eucalyptus grandis in response to silvicultural treatments. For Ecol Manag 40:39–5010.1016/0378-1127(91)90090-I ↗
69. Wu Y, Hayashi K, Liu Y, Cai Y, Sugimori M, Luo J (2005) Collapse-type shrinkage characteristics in plantation-grown Eucalyptus: I. Correlation of basic density and some structural indices with shrinkage and collapse properties. J for Res 16(2):83–8810.1007/BF02857895 ↗
70. Wu Y, Hayashi K, Liu Y, Cai Y, Sugimori M (2006) Relationships of anatomical characteristics versus shrinkage and collapse properties in plantation-grown eucalypt wood from China. J Wood Sci 52(3):187–19410.1007/s10086-005-0751-6 ↗
71. Yamashita K, Hirakawa Y, Nkatani H, Ikeda M (2009) Tangential and radial shrinkage variation within trees of sugi (Cryptomeria japonica) cultivars. J Wood Sci 55:161–16810.1007/s10086-008-1012-2 ↗
72. Yang L, Liu H (2018) A review of Eucalyptus wood collapse and its control during drying. BioResources 13(1):2171–218110.15376/biores.13.1.Yang ↗
73. Yang L, Liu H (2021) Study of the collapse and recovery of Eucalyptus urophydis during conventional kiln drying. Eur J Wood Prod 79(1):129–13710.1007/s00107-020-01614-w ↗
74. Yang JL, Ilic J, Evans R (2003) Interrelationships between shrinkage properties, microfibril angle, and cellulose crystallite width in 10-year-old Eucalyptus globulus. N Z J for Sci 33(1):47–61
75. Zanuncio AJV, Carvalho AG, da Silva LF, Lima JT, Trugilho PF, da Silva JRM (2015) Predicting moisture content from basic density and Eucalyptus and Corymbia logs. Maderas Cienc y Tecnol 17(2):335–344