The rates of stabilization or fixation of copper in ACQ-treated wood were compared for different post treatment conditioning temperatures (22°C and 50°C), solution concentrations (0.4–2.3%) and wood species. In some species, sapwood/heartwood differences were evaluated. The rate and extent of copper stabilization were estimated from changes in concentration of expressed solution at different times after treatment. The quality of the stabilization reaction was evaluated based on leaching performance of the wood after conditioning. Copper stabilized much faster at lower ACQ retentions and when conditioned at 50°C compared to high retentions and stabilization at 22°C. High retention treatments held without drying at 22°C could require five weeks or more for the copper to stabilize in the wood. Generally species effects were minor for the species evaluated, except for Douglas-fir in which copper reacted more quickly than in other species.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Cultural Heritage Materials Analysis · Lignin and Wood Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. AWPA (1999) Book of standards. American Wood Preservers’ Association, Woodstock, MD 21163-0286, USA
2. Cooper PA (1998) Diffusion of copper wood preservatives in wood cell walls following treatment. Wood Fiber Sci 30(4):382–395
3. Jiang X, Ruddick JNR (1999) A spectroscopic investigation of copper ethylenediamine fixation in wood. International Research Group on Wood Preservation Document No IRG/WP 99-20160
4. Jiang X, Ruddick JNR (2000) A comparison of the leaching resistance of copper 2-ethanolamine and copper ethylenediamine treated scots pine. International Research Group on Wood Preservation Document No IRG/WP 00-30233
5. Kamdem DP, Zhang J (2000) Contribution of wood components on the absorption of copper amine. International Research Group on Wood Preservation Document No IRG/WP 00-30216
6. Lucas N, Ruddick JNR (2002) Determination of the amine to copper ratio remaining in wood after water leaching. International Research Group on Wood Preservation Document No IRG/WP 02-30285
7. Pasek EA (2003) Minimizing preservative losses: fixation a report of the P4 migration/fixation/depletion task force. In: Proceedings, American Wood Preserver’s Association 2003:100–124
8. Ruddick JNR (1996) The fixation of ammoniacal copper preservatives. Branch Lines. UBC Fac Forestry Newslett 7(2):2
9. Ruddick JNR (2003) Basic copper wood preservatives, preservative depletion: factors which influence loss. Proc Can Wood Preserv Assoc 24:26–59
10. Stevanovic-Janezic T, Cooper P, Ung T (2001) Chromated copper arsenate preservative treatment of North American hardwoods. Part 2: leaching performance. Holzforschung 55:7–1210.1515/HFSG.2001.7 ↗
11. Zhang J, Kamdem DP (2000a) FTIR characterization of copper ethanolamine—wood interaction for wood preservation. Holzforschung 54:119–12210.1515/HF.2000.020 ↗
12. Zhang J, Kamdem DP (2000b) Interaction of copper amine with southern pine: retention and migration. Wood Fiber Sci 32(3):332–339