journal article·2007-11-02

Effect of high-temperature drying on properties of Norway spruce and larch

Eva Frühwald

Holz als Roh- und Werkstoff· Volume 65· Issue 6
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Wood Treatment and Properties · Tree Root and Stability Studies · Bamboo properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Bekhta P, Niemz P (2003) Effect of High Temperature on Change in Color, Dimensional Stability and Mechanical Properties of Spruce. Holzforschung 57(5):539–54610.1515/HF.2003.080 ↗
2. DIN 52186-1978: Prüfung von Holz; Biegeversuch (conforming with ISO 3133-1975 ‘‘Wood – Determination of ultimate strength in static bending’’)
3. Frühwald E (2007) High-temperature drying of Norway Spruce with and without restraint: Effect on twist. Dry Technol 25(6)10.1080/07373930601184056 ↗
4. Gerhards CC (1979) Effect of high-temperature drying on tensile strength of douglas fir 2 by 4’s. For Prod J 29(3):39–46
5. Gerhards CC (1983) Effect of high-temperature drying on bending strength of yellow-poplar 2 by 4’s. For Prod J 33(2):61–67
6. ISO 3131-1975: Wood – Determination of density for physical and mechanical tests
7. Jämsä S, Viitaniemi P (2001) Heat treatment of wood – Better durability without chemicals. Proceedings of COST E22 Special Seminar, Antibes, France, 2001-02-09, edited by Rapp AO: 21–26
8. Koch P, Wellford WLJ (1977) Some mechanical properties of small specimens cut from 1.79-inch-thick southern pine dried for 6 hours at 300 ° F or for 5 days at 180 ° F – a comparison. Wood Fiber Sci 8(4):235–240
9. Kubojima Y, Okano T, Masamitsu O (2000) Bending strength and toughness of heat-treated wood. J Wood Sci 46(1):8–1510.1007/BF00779547 ↗
10. McNaught AM, Gough DK (1995) Drying 40-mm-thick slash pine in 2.5 hours at 200 °C. For Prod J 45(1):51–54
11. Schneider A (1973) Investigations on the convection drying of lumber at extremely high temperatures. Part 2: Drying degrade, changes in sorption, colour, and strength of pine sapwood and beechwood at drying temperatures from 110 °C to 180 °C (in German). Holz Roh- Werkst 31(5):198–20610.1007/BF02613842 ↗
12. Sehlstedt-Persson M (1995) High-temperature drying of Scots pine. A comparison between HT- and LT-drying. Holz Roh- Werkst 53:95–9910.1007/BF02716400 ↗
13. Syrjänen T (2001) Production and classification of heat treated wood in Finland. Proceedings of COST E22 Special Seminar, Antibes, France, 2001-02-09, edited by Rapp AO: 11–19
14. Terziev N, Daniel G (2002) Industrial kiln drying and its effect on microstructure, impregnation and properties of Scots pine timber impregnated for above ground use – Part 2. Effect of drying on microstructure and some mechanical properties of Scots pine wood. Holzforschung 56(4):434–43910.1515/HF.2002.067 ↗
15. Thiam M, Milota MR, Leichti RJ (2002) Effect of high-temperature drying on bending and shear strengths of western hemlock lumber. For Prod J 52(4):64–68
16. Time B (2002) Studies on hygroscopic moisture transport in Norway spruce (Picea abies). Part 1: Sorption measurements of spruce exposed to cyclic step changes in relative humidity. Holz Roh- Werkst 60(4):271–27610.1007/s00107-002-0303-3 ↗
17. Yao J (1979) Effect of High-Temperature Drying on the Strength of Southern Pine Dimension Lumber. For Prod J 29(8):49–51