Modification of beech veneers with lignin phenol formaldehyde resins in the production of laminated veneer lumber (LVL)
Source abstract
Abstract
Rotary cut beech (Fagus sylvatica L.) veneers were treated with four different lignin phenol formaldehyde (LPF) solutions using dimethyl sulfoxide (DMSO) as a solvent. Four of these veneers were bonded with PF adhesive to produce four-layer laminated veneer lumber (LVL). To synthesize the LPF solutions, a commercial phenol formaldehyde resin (PF resin) was individually mixed with three different technical lignins (Indulin AT, BioChoice lignin, organosolv lignin) and lignin cleavage products (LCP) at a ratio of 3:2 (60%:40%). Differential scanning calorimetry showed an increased curing temperature for the LPF resins in comparison to the PF resin. The mechanical and water-related properties of the LPF-modified LVL were shown to be similar or slightly improved compared to PF-modified LVL. Fungal degradation experiments with white-rot fungus (Trametes versicolor) and brown-rot fungus (Coniophora puteana) exhibited no significant differences in the mass loss of the LPF-modified and PF-modified samples except in one case: LVL made from veneers treated with Indulin AT exposed to the white-rot fungus. The resistance to weathering of LVL samples made from veneers treated with technical lignins was low; however, specimens treated with LCP and the reference PF resin displayed a higher resistance to weathering. It is concluded that technical lignins or LCP can, to a certain extent, be used as a substitute for crude-oil based PF resin.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Lignin and Wood Chemistry · Fermentation and Sensory Analysis · Biochemical and biochemical processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Alonso MV, Oliet M, Perz JM (2004) Determination of curing kinetic parameters of lignin-phenol-formaldehyde resol resins by several dynamic differential scanning calorimetry methods. Thermochem Acta 419(1–2):161–16710.1016/j.tca.2004.02.004 ↗
2. Alonso MV, Oliet M, Rodríguez F, García J, Gilarranz MA, Rodríguez JJ (2005) Modification of ammonium lignosulfonate by phenolation for use in phenolic resins. Bioresour Technol 96(9):1013–101810.1016/j.biortech.2004.09.009 ↗
3. Christiansen AW, Gollob L (1985) Differential scanning calorimetry of phenol-formaldehyde resols. J Appl Polym Sci 30:2279–228910.1002/app.1985.070300601 ↗
4. Danielson B, Simonson R (1998) Kraft lignin in PF resin. Part 1. Partial replacement of phenol by kraft lignin in PF adhesives for plywood. J Adhes Sci Technol 12:923–93910.1163/156856198X00542 ↗
5. Dieste A, Krause A, Bollmus S, Militz H (2009) Gluing ability of plywood produced with DMDHEU-modified veneers of Fagus sp., Betula sp. and Picea sp.. Int J Adhes Adhes 29(2):206–20910.1016/j.ijadhadh.2008.05.001 ↗
6. DIN CEN/TS 15083–1 (2005) Durability of wood and wood-based products—determination of the natural durability of solid wood against wood-destroying fungi, test methods—Part 1: basidiomycetes; German version CEN/TS 15083-1:2005. Deutsches Institut für Normung
7. El Mansouri N-E, Salvadó J (2006) Structural characterization of technical lignins for the production of adhesives: application to lignosulfonate, kraft, soda-anthraquinone, organosolv and ethanol process lignins. Ind Crops Prod 24(1):8–1610.1016/j.indcrop.2005.10.002 ↗
8. EN 310 (1993) Wood-based panels. Determination of modulus of elasticity in bending and of bending strength. European Committee of Standardisation (CEN), Brussels
9. EN 84 (1997) Wood preservatives. Accelerated ageing of treated wood prior to biological testing. Leaching procedure. European Committee of Standardisation (CEN), Brussels
10. EN 927–6 (2008) Paints and varnishes—coating materials and coating systems for exterior wood—Part 6: exposure of wood coatings to artificial weathering using fluorescent UV lamps and water. European Committee of Standardisation (CEN), Brussels
11. Evans PD, Kraushaar Gibson S, Cullis I, Liu C, Sèbe G (2013) Photostabilization of wood using low molecular weight phenol formaldehyde resin and hindered amine light stabilizer. Polym Degrad Stabil 98:158–16810.1016/j.polymdegradstab.2012.10.015 ↗
12. Fengel D, Wegener G (1984) Wood: chemistry, ultrastructure, reactions. Walter de Gruyter, Berlin
13. Furuno T, Imamura Y, Kajita H (2004) The modification of wood by treatment with low molecular weight phenol-formaldehyde resin: a properties enhancement with neutralized phenolic-resin and resin penetration into wood cell walls. Wood Sci Technol 37:349–36110.1007/s00226-003-0176-6 ↗
14. Gosselink RJA, deJoug E, Guran B, Abächerlie A (2004) Co-ordination network for lignin-standardization, production and application adapted to market requirements (EUROLIGNIN). Ind Crops Prod 20(2):121–12910.1016/j.indcrop.2004.04.015 ↗
15. Hill CAS (2006) Wood modification: chemical, thermal and other processes. Wiley, Weinheim10.1002/0470021748 ↗
16. Hon DN-S, Chang S-T (1984) Surface degradation of wood by ultraviolet light. J Polym Sci 22:2227–2241
17. Hu Z, Du X, Liu J, Chang H, Jameel H (2016) Structural characterization of pine Kraft lignin: biochoice lignin vs indulin AT. J Wood Chem Technol 36:432–44610.1080/02773813.2016.1214732 ↗
18. Hultzsch K (1950) Chemie der Phenolharze (Chemistry of phenolic resins) (in German), vol 3. Springer, Berlin
19. Kartal NS, Ayrilmis N, Imamura Y (2007) Decay and termite resistance of plywood treated with various fire retardants. Build Environ 42:1207–121110.1016/j.buildenv.2005.11.018 ↗
20. Khan MA, Ashraf SM, Malhotra VP (2004) Eucalyptus bark lignin substituted phenol formaldehyde adhesives: a study on optimization of reaction parameters and characterization. J Appl Polym Sci 92:3514–352310.1002/app.20374 ↗
21. Kielmann BC, Mai C (2016) Application and artificial weathering performance of translucent coatings on resin-treated and dye-stained beech-wood. Prog Org Coat 95:54–6310.1016/j.porgcoat.2016.02.019 ↗
22. Klašnja B, Kopitović S (1992) Lignin-phenol-formaldehyde resins as adhesives in the production of plywood. Holz Roh Werkst 50:282–28510.1007/BF02615352 ↗
23. Kleinert M, Barth T (2008) Phenols from lignin. Chem Eng Technol 31(5):736–74510.1002/ceat.200800073 ↗
24. Laks PE, Richter DL, Larkin GM (2002) Fungal susceptibility of interior commercial building panels. Forest Prod J 52(5):41–44
25. Lora JH, Glasser WG (2002) Recent application of lignin: a suitable alternative to nonrenewable materials. J Polym Environ 10:1:39–4810.1023/A:1021070006895 ↗
26. Madsen B (1975) Moisture content–strength relationship for lumber subjected to bending. Can J Civil Eng 2(4):466–47310.1139/l75-043 ↗
27. Mittal M, Sharma CB (1992) Studies on lignin-based adhesives for plywood panels. Polym Int 29:7–810.1002/pi.4990290103 ↗
28. Panday MP, Kim CS (2011) Lignin depolymerization and conversion: a review of thermochemical methods. Chem Eng Technol 34:29–4110.1002/ceat.201000270 ↗
29. Pilato LA (2010) Phenolic resins: a century of progress. Springer, Berlin10.1007/978-3-642-04714-5 ↗
30. Pizzi A (1994) Advanced wood adhesives technology. Marcel Dekker, New York10.1201/9781482293548 ↗
31. Pradhan SK, Chakraborty I, Kar BB (2015) Chemically modified lignin—a potential resource material for composites with better stability. Int J Sci Environ Technol 4(1):183–189
32. Puls J (2009) Lignin—Verfügbarkeit, Markt und Verwendung: Perspektiven für schwefelfreie Lignine (Lignin—Availability, market and application: perspectives for sulfur-free lignins). In: Gülzower Fachgespräche, vol 31—Stoffliche Nutzung von Lignin. Fachagentur Nachwachsende Rohstoffe, Gülzow (In German)
33. Rowell RM, Banks WB (1985) Water repellency and dimensional stability of wood. USDA. For Serv F.P.L., Gen Techn Rep. FPL-50
34. Ryu JY, Imamura Y, Takahashi M, Kajita H (1993) Effects of molecular weight and some other properties of resins on the biological resistance of phenolic resin treated wood. Mokuzai Gakkaishi 39(4):486–492
35. Schultz TP, Hubbard TF Jr, Jin L, Fisher TH, Nicholas DD (1990) Role of stilbenes in the natural durability of wood: fungicidal structure–activity relationships. Phytochemistry 29(5):1501–150710.1016/0031-9422(90)80109-T ↗
36. Stamm AJ, Seborg RM (1936) Resin treated plywood. Ind Eng Chem 31:897–90210.1021/ie50355a023 ↗
37. Suparno O, Anthony D, Covington AD, Christine S, Evans CS (2005) Kraft lignin degradation products for tanning and dyeing of leather. J Chem Technol Biotechnol 80:44–4910.1002/jctb.1150 ↗
38. Tejado A, Peña C, Labidi J, Echeverria JM, Mondragon I (2007) Physico-chemical characterization of lignins from different sources for use in phenol-formaldehyde resin synthesis. Bioresour Technol 98:1655–166310.1016/j.biortech.2006.05.042 ↗
39. Trinh HM, Militz H, Mai C (2012) Modification of beech veneers with N-methylol-melamine compounds for the production of plywood. Eur J Wood Prod 70:421–43210.1007/s00107-011-0569-4 ↗
40. Vick CB, Rowell RM (1990) Adhesive bonding of acetylated wood. Int J Adhes Adhes 10:4:263–27210.1016/0143-7496(90)90044-X ↗
41. Vishtal A, Kraslawski A (2011) Challenges in industrial applications of technical lignins. Bioresources 6(3):3547–356810.15376/biores.6.3.3547-3568 ↗
42. Wang M, Leitch M, Xu C (2009) Synthesis of phenol-formaldehyde resol resins using organosolv pine lignins. Eur Polym J 45:3380–338810.1016/j.eurpolymj.2009.10.003 ↗
43. Wang H, Tucker M, Ji Y (2013) Recent development in chemical depolymerization of lignin: a review. J Appl Chem 2013:838645. https://doi.org/10.1155/2013/83864510.1155/2013/838645 ↗
44. Yang S, Zhang Y, Yuan T-Q, Su R-C (2015) Lignin-phenol-formaldehyde resin adhesives prepared with biorefinery technical lignins. J Appl Sci 132:42493. https://doi.org/10.1002/app.4249310.1002/app.42493 ↗