journal article·2024-02

Chemical characterization of archaeological marine wooden piles from the ancient harbor Theodosius in Istanbul

Oktay Gonultas, Mualla Balaban-Ucar

Publisher page

Abstract

The ultrastructure and chemical composition of marine wooden piles from Cupressussempervirens and Castaneasativa, buried for approximately 1000 years, were investigated along with recent woods (RW) using wet chemical analyses, FTIR spectroscopy, and TGA. The ash content in RW chestnut samples was 0.49%, compared to 3.30% in archeological wood (AW), and for cypress, it was 0.32% and 1.87%, respectively. Solubility in ethanol-cyclohexane decreased in the archaeological samples due to extractives leaching, while cypress AW showed increased solubility at 1% NaOH. Differences in polysaccharide degradation ratios during aging were observed, with cypress wood having lower & alpha;-cellulose content than chestnut wood. Glucuronoxylans in hardwood degraded easily, while galactoglucomannan in cypress exhibited more resistance. Lignin showed two types of alteration, with slight increase in hardwood and higher values in softwood due to reduced holocellulose. Micro and morphological changes were identified using light microscopy and SEM. Inorganic material accumulation was observed in AW, while resin residues were found only in cypress wood. Cell wall delamination, degradation in ray cells, and deposits from inorganic matter or fungal hyphae were observed. EDX analysis revealed lower potassium contents in AW samples compared to petrified wood. Iron was detected in archaeological chestnut wood, attributed to tannin content acting as a chelator. Chestnut AW exhibited high calcium content due to calcification. FTIR spectra showed minimal hemicellulose peaks in archaeological samples, consistent with wet analysis. The disappearance of the shoulder below 300 & DEG;C in the DTG curve indicated hemicellulose loss, especially in AW chestnut. Lignin index values correlated with wet analysis, with higher values in cypress AW. The intensity of lignin-associated peaks at 1510 cm-1 was higher in archaeological samples. The second peak in the DTG curve, related to lignin and phenolic compound degradation, was observed at lower temperatures, particularly in chestnut AW.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Cultural Heritage Materials Analysis · Wood Treatment and Properties · Lignin and Wood Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Akkemik Ü, Kocabaş U (2013) Woods of the old galleys of Yenikapi, İstanbul. Mediterranean Archaeol Archaeometry 13(2):31–41
2. Baar J, Paschová Z, Hofmann T, Kolář T, Koch G, Saake B, Rademacher P (2019) Natural durability of subfossil oak: wood chemical composition changes through the ages. Holzforschung 74(1):47–5910.1515/hf-2018-0309 ↗
3. Bader TK, de Borst K, Fackler K, Ters T, Braovac S (2013) A nano to macroscale study on structure-mechanics relationships of archaeological oak. J Cult Herit 14:377–388. https://doi.org/10.1016/j.culher.2012.09.00710.1016/j.culher.2012.09.007 ↗
4. Balaban-Ucar M, Gonultas O (2019) Volatile compounds of archaeological wood from the ancient harbor Theodosius in Istanbul. Eur J Wood Prod 77:475–481. https://doi.org/10.1007/s00107-019-01391-110.1007/s00107-019-01391-1 ↗
5. Björdal CG, Nilsson T (2008) Reburial of shipwrecks in marine sediments: a long-term study on wood degradation. J Archaeol Sci 35(4):862–872. https://doi.org/10.1016/j.jas.2007.06.00510.1016/j.jas.2007.06.005 ↗
6. Castano-Santamaria J, Bravo F (2012) Variation in carbon concentration and basic density along stems of sessile oak (Quercus petraea (Matt.) Liebl.) and Pyrenean oak (Quercus pyrenaica Willd.) in the Cantabrian Range (NW Spain). Ann for Sci 69:663–67210.1007/s13595-012-0183-6 ↗
7. Cavallaro G, Lazzara G, Milioto S, Parisi F, Ruisi F (2017) Nanocomposites based on esterified colophony and halloysite clay nanotubes as consolidants for waterlogged archaeological woods. Cellulose 24:3367–337610.1007/s10570-017-1369-8 ↗
8. Cavallaro G, Agliolo Gallitto A, Lisuzzo L, Lazzara G (2019) Comparative study of historical woods from XIX century by thermogravimetry coupled with FTIR spectroscopy. Cellulose 26:8853–8865. https://doi.org/10.1007/s10570-019-02688-310.1007/s10570-019-02688-3 ↗
9. Christiernin M, Notley SM, Zhang L, Nilsson T, Henriksson G (2009) Comparison between 10,000-year old and contemporary spruce lignin. Wood Sci Technol 43:23–41. https://doi.org/10.1007/s00226-008-0222-510.1007/s00226-008-0222-5 ↗
10. Colom X, Carrillo F, Nogués F, Garriga P (2003) Structural analysis of photodegraded wood by means of FTIR spectroscopy. Polym Degrad Stab 80(3):543–54910.1016/S0141-3910(03)00051-X ↗
11. Colombini G, Orlandi M, Modugno F, Tolppa E-L, Sardelli M, Zoia L, Crestini C (2007) Archaeological wood characterisation by PY/GC/MS, GC/MS, NMR and GPC Techniques. Microchem J 85(1):164–173. https://doi.org/10.1016/j.microc.2006.05.00110.1016/j.microc.2006.05.001 ↗
12. Colombini MP, Lujecko JJ, Modugno F, Orlandi M, Tolppa E-L, Zoia L (2009) A multi-analytical study of degradation of lignin in archaeological waterlogged wood. Talanta 80(1):61–70. https://doi.org/10.1016/j.talanta.2009.06.02410.1016/j.talanta.2009.06.024 ↗
13. Emandi ANA, Ileana Vasiliu C, Budrugeac P, Stamatin I (2011) Quantitative investigation of wood composition by integrated FT-IR and thermogravimetric methods. Cellul Chem Technol 45(9):579
14. Gelbrich J, Mai C, Militz H (2008) Chemical changes in wood degraded by bacteria. Int Biodeterior Biodegrad 61(1):24–32. https://doi.org/10.1016/j.ibiod.2007.06.00710.1016/j.ibiod.2007.06.007 ↗
15. Ghavidel A, Hosseinpourpia R, Militz H, Vasilache V, Sandu I (2020a) Characterization of archaeological European white elm (Ulmus laevis P.) and black poplar (Populus nigra L.). Forests 11(1329):1–13. https://doi.org/10.3390/f1402039310.3390/f14020393 ↗
16. Ghavidel A, Hofmann T, Bak M, Sandu I, Vasilache V (2020b) Comparative archaeometric characterization of recent and historical oak (Quercus spp.) wood. Wood Sci Technol 54:1121–1137. https://doi.org/10.1007/s00226-020-01202-410.1007/s00226-020-01202-4 ↗
17. Glastrup J (1996) Degradation of polyethylene glycol. A study of the reaction mechanism in a model molecule: tetraethylene glycol. Polym Degrad Stab 52(3):217–22210.1016/0141-3910(95)00225-1 ↗
18. Guo J, Xiao L, Han L, Wu H, Yang T, Wu S, Yin Y (2019) Deterioration of the cell wall in waterlogged wooden archeological artifacts, 2400 years old. IAWA J 40(4):820–844. https://doi.org/10.1163/22941932-4019024110.1163/22941932-40190241 ↗
19. Gupta BS, Jelle BP, Gao T (2015) Wood facade materials ageing analysis by FTIR spectroscopy. Proc Inst Civil Eng Constr Mater 168(5):219–23110.1680/coma.13.00021 ↗
20. High KE, Penkman KE (2020) A review of analytical methods for assessing preservation in waterlogged archaeological wood and their application in practice. Herit Sci 8(1):83. https://doi.org/10.1186/s40494-020-00422-y10.1186/s40494-020-00422-y ↗
21. Huang C, Su Y, Shi J, Yuan C, Zhai S, Yong Q (2019) Revealing the effects of centuries of ageing on the chemical structural features of lignin in archaeological fir woods. N J Chem 43:3520–3528. https://doi.org/10.1039/C9NJ00026G10.1039/C9NJ00026G ↗
22. Humar M, Balzano A, Kržišnik D, Lesar B (2021) Assessment of wooden foundation piles after 125 years of service. Forests 12(2):143. https://doi.org/10.3390/f1202014310.3390/f12020143 ↗
23. Kacik F, Smira P, Kačíková D, Reinprecht L, Nasswettrova A (2014) Chemical changes in fir wood from old buildings due to ageing. Cell Chem Technol 48(1–2):79–88
24. Kızıltan Z (2008) Excavations at Yenikapı, Sirkeci and Üsküdar within marmaray and metro projects. In: Proceedings of the 1st symposium on marmaray-metro salvage excavations, 5th–6th May, pp 1–17
25. Kocabas U (2011) The first five years and future perspectives of Yenikapi Shipwrecks project. Shipwrecks 2011, 18–21 October, Stockholm, Sweden
26. Kranitz K (2014) Effect of natural aging on wood (Doctoral dissertation, ETH Zurich)
27. Krutul D, Kozakiewicz P (2003) Impact of chemical factors on concentration changes of selected elements in native wood and excavated wood. Annals of Warsaw Agricultural University. Forestry and Wood Technology, 53
28. Krutul D, Radomski A, Zawadzki J, Zielenkiewicz T, Antczak A (2010) Comparison of the chemical composition of the fossil and recent oak wood. Wood Res 55:113–120
29. Li R, Guo J, Macchioni N, Pizzo B, Xi G, Tian X, Yin Y (2022) Characterization of waterlogged archaeological wood from Nanhai No. 1 shipwreck by multidisciplinary diagnostic methods. J Cult Herit 56:25–35. https://doi.org/10.1016/j.culher.2022.05.00410.1016/j.culher.2022.05.004 ↗
30. Lisuzzo L, Hueckel T, Cavallaro G, Sacanna S, Lazzara G (2021) Pickering emulsions based on wax and halloysite nanotubes: an ecofriendly protocol for the treatment of archeological woods. ACS Appl Mater Interfaces 13(1):1651–166110.1021/acsami.0c20443 ↗
31. Lucejko JJ, Zborowska M, Modugno F, Colombini MP, Pradzynski W (2012) Analytical pyrolysis vs. classical wet chemical analysis to assess the decay of archaeological waterlogged wood. Anal Chim Acta 745:70–77. https://doi.org/10.1016/j.aca.2012.07.04610.1016/j.aca.2012.07.046 ↗
32. Moosavinejad SM, Madhoushi M, Vakili M, Rasouli D (2019) Evaluation of degradation in chemical compounds of wood in historical buildings using FT-IR and FT-Raman vibrational spectroscopy. Maderas Ciencia y Tecnología 21(3):381–392. https://doi.org/10.4067/S0718-221X201900500031010.4067/S0718-221X2019005000310 ↗
33. Muyzer G, Stams AJ (2008) The ecology and biotechnology of sulphate-reducing bacteria. Nat Rev Microbiol 6(6):441–45410.1038/nrmicro1892 ↗
34. Passialis CN (1997) Physico-chemical characteristics of waterlogged archaeological wood. Holzforschung 51:111–11310.1515/hfsg.1997.51.2.111 ↗
35. Pearson CL, Griggs CB, Kuniholm PI, Brewer PW, Wazny T, Canady L (2012) Dendroarchaeology of the mid-first millennium AD in constantinople. J Archaeol Sci 39:3402–341410.1016/j.jas.2012.05.024 ↗
36. Pedersen NB, Gierlinger N, Thygesen LG (2015) Bacterial and abiotic decay in waterlogged archaeological Picea abies (L.) Karst studied by confocal Raman imaging and ATR-FTIR spectroscopy. Holzforschung 69:103–112. https://doi.org/10.1515/hf-2014-002410.1515/hf-2014-0024 ↗
37. Pedersen NB, Łucejko JJ, Modugno F, Björdal C (2021) Correlation between bacterial decay and chemical changes in waterlogged archaeological wood analysed by light microscopy and Py-GC/MS. Holzforschung 75(7):635–645. https://doi.org/10.1515/hf-2020-015310.1515/hf-2020-0153 ↗
38. Pozhidaev VM, Sergeeva YE, Malakhov SN, Yatsishina EB (2021) Identification of archaeological wood species by IR spectroscopy. J Anal Chem 76(5):573–577. https://doi.org/10.1134/S106193482105014210.1134/S1061934821050142 ↗
39. Romagnoli M, Galotta G, Antonelli F, Sidoti G, Humar M, Kržišnik D, Petriaggi BD (2018) Micro-morphological, physical and thermogravimetric analyses of waterlogged archaeological wood from the prehistoric village of Gran Carro (Lake Bolsena-Italy). J Cult Herit 33:30–38. https://doi.org/10.1016/j.culher.2018.03.01210.1016/j.culher.2018.03.012 ↗
40. Rosu D, Teaca CA, Bodirlau R, Rosu L (2010) FTIR and color change of the modified wood as a result of artificial light irradiation. J Photochem Photobiol, B 99(3):144–14910.1016/j.jphotobiol.2010.03.010 ↗
41. Runkel ROH, Wilke KD (1951) Zur Kenntnis des thermo-plastischen Verhaltens von Holz. (On the knowledge of the thermoplastic behavior of wood). Holz Roh Werkst 9(2):41–5310.1007/BF02617537 ↗
42. Solar R, Reinprecht L, Kačík F, Melcer I, Horský D (1987) Comparison of some physico-chemical and chemical properties of polysacharidic and lignin part of contemporary and subfossil oak wood. Cell Chem Technol 2:513–524
43. Tintner J, Smidt E, Tieben J, Reschreiter H, Kowarik K, Grabner M (2016) Aging of wood under long-term storage in a salt environment. Wood Sci Technol 50:953–961. https://doi.org/10.1007/s00226-016-0830-410.1007/s00226-016-0830-4 ↗
44. Tomassetti M, Campanella L, Tomellini R (1990) Thermogravimetric analysis of ancient and fresh woods. Thermochim Acta 170:51–65. https://doi.org/10.1016/0040-6031(90)80524-310.1016/0040-6031(90)80524-3 ↗
45. Traore M, Kaal J, Cortizas AM (2016) Application of FTIR spectroscopy to the characterization of archeological wood. Spectrochim Acta Part A Mol Biomol Spectrosc 153:63–70. https://doi.org/10.1016/j.saa.2015.07.10810.1016/j.saa.2015.07.108 ↗
46. Ucar G, Staccioli G, Stoll M (1996) Chemical composition und ultrastructure of a fossil wood from the genus of ancestral Sequoia. Holz Roh-Werkst 54:411–42110.1007/s001070050212 ↗
47. Ucar G, Balaban M, Goren N (1998) Ethanol extractives of fossil sequoia wood. Holz Roh-Werkst 56:430–436. https://doi.org/10.1007/s00107-004-0530-x10.1007/s00107-004-0530-x ↗
48. Wagner L, Almkvist G, Bader TK, Bjurhager I, Rautkari L, Gamstedt EK (2016) The influence of chemical degradation and polyethylene glycol on moisture-dependent cell wall properties of archeological wooden objects: a case study of the Vasa shipwreck. Wood Sci Technol 50:1103–112310.1007/s00226-016-0861-x ↗
49. Welling J, Schwarz T, Bauch J (2018) Biological, chemical and technological characteristics of waterlogged archaeological piles (Quercus petraea (Matt.) Liebl.) of a medieval bridge foundation in Bavaria. Eur J Wood Prod 76(4):1173–1186. https://doi.org/10.1007/s00107-018-1299-710.1007/s00107-018-1299-7 ↗
50. Wise LE, Murphy M, D’addieco AA (1946) Chlorite holocellulose, its fractionation and beaning on summative wood analysis and studies on the hemicellulose. Pap Trade J 122(2):35–43
51. Yonenobu H, Tsuchikawa S (2003) Near-infrared spectroscopic comparison of antique and modern wood. Appl Spectrosc 57(11):1451–145310.1366/000370203322554635 ↗