journal article·2004-12

Dependance on the adhesive formulation of the upgrading of MUF particleboard adhesives and decrease of melamine content by buffer and additives

M. Zanetti, A. Pizzi

Holz als Roh- und Werkstoff· Volume 62· Issue 6
Publisher page

Abstract

The type of MUF adhesive formulation has been shown to have a determinant effect in the performance of MUF adhesives for wood panels upgraded with iminoamino methylene basis of the “hexamine sulphate” type. The high performance sequential MUF formulations are upgraded little or not at all by these additives. Much weaker non-sequential MUF formulations instead are so strongly upgraded for IB boiled strength by the use of these additives to markedly outperform the normally stronger sequential type formulations and even phenolic resins. To the buffering action leading to optimization of the hardening ⇄ degradation equilibrium described previously as the main cause of the functioning of these additives must then be added the effect of the type of formulation. This is quantified and described. It is partly related to the presence of higher or lower levels of unreacted primary amine groups of the melamine and their consequent level of contribution to buffering. It is also partly related to the level of plasticization of the hardened glue line by unreacted urea and the consequent viscoelastic dissipation of energy that would derive from this.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microplastics and Plastic Pollution · Recycling and Waste Management Techniques · Advanced Cellulose Research Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Kamoun C (2000) Mise au point de nouveaux adhesifs aminoplastiques pour panneaux de particules, PhD thesis, University of Nancy
2. Oldörp K, Marutzky R (1998) Untersuchungen an Spanplatten mit harnstoffmodifizierten PF-Harzen. Holz Roh- Werkstoff 56(1):75–7610.1007/PL00002609 ↗
3. Pizzi A (1994) Advanced wood adhesives technology. Marcel Dekker, New York10.1201/9781482293548 ↗
4. Pizzi A (1997) On the correlation of some theoretical and experimental parameters in polycondensation cross-linked networks. J Appl Polymer Sci 63:603–61710.1002/(SICI)1097-4628(19970131)63:5<603::AID-APP8>3.0.CO;2-Y ↗
5. Pizzi A (2000) High performance MUF resins of low melamine content by a number of novel techniques. Wood Adhesives 2000, Forest Products Society, Tahoe, California, USA, pp 219–239
6. Pizzi A, Kamoun C (1999) European Contract FAIR TC 96-1604
7. Pizzi A, Probst F, Deglise X (1997) Molecular mechanics modelling of interfacial energy and flexibility. J Adhes Sci Tech 11:573–59010.1163/156856197X00093 ↗
8. Prestifilippo M, Pizzi A, Norback H, Lavisci P (1996) Low addition of melamine salts for improved UF adhesives water resistance. Holz Roh- Werkstoff 54(6):393–39810.1007/s001070050208 ↗
9. Zanetti M, Pizzi A (2002) Buffer upgrading of MUF panel adhesives at lower melamine content. In: Proceedings of the Sixth European Panel Products Symposium, Llandudno, Wales, UK, pp 231–248
10. Zanetti M, Pizzi A, Kamoun C (2003) Upgrading of MUF polycondensation resins and decrease of melamine content by buffer and additives. Holz Roh Werkstoff 61:55–6510.1007/s00107-002-0352-7 ↗
11. Zhao C, Pizzi A, Garnier C (1999) Fast advancement and hardening acceleration of low condensation alkaline PF resins by esters and copolymerized urea. J Appl Polymer Sci 74:359–37810.1002/(SICI)1097-4628(19991010)74:2<359::AID-APP18>3.3.CO;2-1 ↗