Evaluation of mechanical properties and formaldehyde emissions of particleboards with nanomaterial-added melamine-impregnated papers
Source abstract
Abstract
The effects of various surface hot-pressing parameters, including temperature, time, and pressure, on the properties of particleboards with nanomaterial-added melamine-impregnated papers were investigated. Melamine formaldehyde resin (MUF) mixed with nano-TiO2-pillared montmorillonite (TiO2/MMT) was used to impregnate decor papers. Orthogonal experimental design was employed to determine the effects of different factors and to find the optimum levels of the parameters to achieve the most desirable properties. Mechanical and physical properties including modulus of rupture, internal bond strength, thickness swelling, and formaldehyde emission were determined according to Chinese national standards GB/T 15102 (2006) and GB/T 18580 (2001), respectively. With the incorporation of nanoparticles into the MUF resin, the mechanical and physical properties of the coated particleboards improved and formaldehyde emission decreased. Surface pressing temperature and time had a significant influence on the MOR and TS properties, while the pressure was less significant. On the other hand, the presence of nanoparticles in the impregnated resin and heat treatment during surface pressing resulted in less formaldehyde emission. Thus, low-formaldehyde-emission particleboard coated with nano-melamine impregnated papers can be obtained with 60 s of surface pressing at a temperature of 190 °C and pressure of 3.0 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nanocomposite Films for Food Packaging · Natural Fiber Reinforced Composites · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Amazio P, Avella M, Errico ME, Gentile G, Balducci F, Gnaccarini A, Moratalla J, Belanche M (2011) Low formaldehyde emission particleboard panels realized through a new acrylic binder. J Appl Polym Sci 122(4):2779–278810.1002/app.34327 ↗
2. Böhm M, Salem MZ, Srba J (2012) Formaldehyde emission monitoring from a variety of solid wood, plywood, blockboard and flooring products manufactured for building and furnishing materials. J Hazard Mater 221(4):68–7910.1016/j.jhazmat.2012.04.013 ↗
3. Cai X, Riedl B, Zhang SY, Wan H (2007) Effects of nanofillers on water resistance and dimensional stability of solid wood modified by melamine–urea–formaldehyde resin. Wood Fiber Sci 39(2):307–318
4. Cai X, Zhang SY, Wan H (2008) The impact of the nature of nanofillers on the performance of wood polymer nanocomposites. Compos A 39:727–73710.1016/j.compositesa.2008.02.004 ↗
5. Cai XL, Rield B, Wan H, Zhang XY (2010) Montmorillonite nanoparticle distribution and morphology in melamine-urea-formaldehyde resin-impregnated wood nanocomposites. Wood Fiber Sci 42(3):285–291
6. Çavdar AD, Yel H, Kalaycıoglu H, Hiziroglu S (2013) Effect of waste melamine impregnated paper on properties of oriented strand board. Mater Design 51(4):751–75510.1016/j.matdes.2013.04.052 ↗
7. Conner AH (1996) Polymeric material encyclopedia. CRC Press, New York
8. GB/T 15102 (2006) Surface decorated wood-based panels with paper impregnated thermosetting resins. Wood-based Panels of Standardization Administration of China, Beijing
9. GB/T 18580 (2001) Indoor decorating and refurbishing materials–limit of formaldehyde emission of wood-based panels and finishing products. Wood-based Panels of Standardization Administration of China, Beijing
10. GB/T 4897.2 (2003) Particleboard–part 2: requirements for general purpose boards for use in dry conditions. Wood-based Panels of Standardization Administration of China, Beijing
11. Hse CY, Fu F, Pan H (2008) Melamine-modified urea formaldehyde resin for bonding particleboards. Forest Prod J 58(4):56–61
12. Jiang T, Gardner DJ, Baumann MGD (2002) Volatile organic compound emissions arising from the hot-pressing of mixed-hardwood particleboard. For. Prod. J. 52(11):66–77
13. Kaneko T, Shimotsuma H, Kajikawa M (2001) Synthesis and photocatalytic activity of titania pillared clays. J Porous Mater 8(4):295–30110.1023/A:1013165014982 ↗
14. Kim S (2010) Control of formaldehyde and TVOC emission from wood-based flooring composites at various manufacturing processes by surface finishing. J Hazard Mater 176(1):14–1910.1016/j.jhazmat.2009.03.113 ↗
15. Kumar S (1994) Chemical modification of wood. Wood Fiber Sci 26(2):270–280
16. Lin Q, Yang G, Liu J, Rao J (2006) Property of nano-SiO2/urea formaldehyde resin. Front For China 2(1):230–23710.1007/s11461-006-0024-6 ↗
17. Lum WC, Lee SH, Hng PS (2013) Effects of formaldehyde catcher on some properties of particleboard with different ratio of surface to core layer. Asian J Appl Sci 6(1):1–810.3923/ajaps.2013.1.15 ↗
18. Mogyorosi K, Dekany I, Fendler JH (2003) Preparation and characterization of clay mineral intercalated titanium dioxide nanoparticles. Langmuir 19(7):2938–294610.1021/la025969a ↗
19. Nikvash N, Kharazipour A, Euring M (2012) Effects of wheat protein as a biological binder in the manufacture of particleboards using a mixture of canola, hemp, bagasse, and commercial wood. For Prod J 62(1):49–57
20. Ooka C, Yoshida H, Horio M, Suzuki K, Hattori T (2003) Adsorptive and photocatalytic performance of TiO2 pillared montmorillonite in degradation of endocrine disruptors having different hydrophobicity. Appl Catal Environ 41(3):313–32110.1016/S0926-3373(02)00169-8 ↗
21. Ooka C, Yoshida H, Suzuki K, Hattori T (2004) Highly hydrophobic TiO2 pillared clay for photocatalytic degradation of organic compounds in water. Micropor Mesopor Mater 67(2):143–15010.1016/j.micromeso.2003.10.011 ↗
22. Ray SS, Okamoto M (2003) Polymer/layered silicate nanocompoistes: a review from preparation to processing. Prog Polym Sci 28(11):1539–164110.1016/j.progpolymsci.2003.08.002 ↗
23. Roumeli E, Pavlidou E, Papadopoulou E, Vourlias G, Bikiaris D, Paraskevopoulos KM (2012) Synthesis, characterization and thermal analysis of urea formaldehyde/nano SiO2 resins. Thermochim Acta 57(10):33–3910.1016/j.tca.2011.10.007 ↗
24. Salthammer T, Mentese S, Marutzky R (2010) Formaldehyde in the indoor environment. Chem Rev 110(1):2536–257210.1021/cr800399g ↗
25. Shi J, Zhou LJ, Zhang WD (2007) Improvement of wood properties by urea formaldehyde resin and nano-SiO2. Front For China 2(1):104–10910.1007/s11461-007-0017-0 ↗
26. Tian WG (2002) Quality control on wood-based panel overlaid with paper impregnated melamine resin. China Wood Ind 16(3):37–38
27. Vansteenkiste R (1981) Surface treatment of woodbased panels. Chemical and Industry Press, Beijing
28. Wang SY, Yang TH, Lin LT, Lin CJ, Tsai MJ (2007) Properties of low-formaldehyde-emission particleboard made from recycled wood-waste chips sprayed with PMDI/PF resin. Build Environ 42(7):2472–247910.1016/j.buildenv.2006.06.009 ↗
29. Yu CWF, Kim JT (2012) Long-term impact of formaldehyde and VOC emissions from wood-based products on indoor environments; and issues with recycled products. Indoor Built Environ 21(1):137–14910.1177/1420326X11424330 ↗
30. Zeng YH (2010) Study on abrasion resistance enhancement of melamine-formaldehyde impregnation resin, Fujian agriculture and forestry university
31. Zhou X, Pizzi A, Du G (2012) The effect of nanoclay on melamine-urea-formaldehyde wood adhesives. J Adhes Sci Technol 26(10):1341–134810.1163/156856111X618498 ↗