Drying quality of rubberwood: an industrial perspective
Source abstract
Abstract
In this study, the kiln drying yield of 30 mm Rubberwood (Hevea brasiliensis) used for the furniture manufacturing industry in South East Asia was evaluated. The results showed that the average yield loss was 10%, and end-checks, splits and warping were the most common drying defects. It was found that sawn timber from older trees (> 21 years) were less prone to drying defects, and the use of stress relieving treatments significantly reduced the incidence of drying defects.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Structural Engineering and Vibration Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (5)
Show source-provided references
1. Hong LT, Sim HC (1999) Rubberwood – processing and utlization. Malayan Forest Record No. 39, Forest Research Institute of Malaysia
2. Ratnasingam J (2004) Economic of the Rubberwood processing industry – a South East Asian perspective. Asian Timber 23(2):16–18
3. Ratnasingam J, Florin I, Macpherson TH (2007) Influence of wood species on the perceived value of wooden furniture: the case of Rubberwood. Holz Roh- Werkst 65:487–48910.1007/s00107-007-0186-4 ↗
4. Ratnasingam J, Scholz F (2008) Yield studies of Rubberwood lumber during rough milling operation. Holz Roh- Werkst 66:467–46810.1007/s00107-008-0249-1 ↗
5. Zobel BJ, van Buijtenen JP (1989) Wood variation – its causes and control. Spinger, Berlin10.1007/978-3-642-74069-5 ↗