Testing the durability of timber above ground: evaluation of different test methods
Source abstract
Abstract
A large number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no test methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published only in an encoded or incomplete way. This makes it difficult to obtain comparable results to work on a comprehensive above-ground test methodology. Therefore, a comparative study on moisture performance and the resulting decay response was conducted. Five different wood species were exposed according to 24 different test methods representing a wide range of different exposure situations including in- and on-ground exposure. After three years of exposure the moisture load as well as decay development differed between the test methods and tested materials. Different parameters were identified influencing the moisture performance of wood in the respective test set-ups and finally an attempt was made to set up a test methodology providing sets of test methods for differently severe applications within use class 3.1 and 3.2 as defined in the European standard EN 335 (2013).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Industrial Vision Systems and Defect Detection · Forest ecology and management
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Augusta U (2007) Untersuchung der natürlichen Dauerhaftigkeit wirtschaftlich bedeutender Holzarten bei verschiedener Beanspruchung im Außenbereich. (Natural durability of European wood species in different use classes) (In German): Doctoral thesis, University Hamburg, Faculty of Mathematics, Informatics and Natural Sciences, Department Biology, Germany
2. AWPA E9 (2013) Standard field test for the evaluation of wood preservatives to be used above ground (UC3A and UC3B): L-joint test. American Wood Protection Association. Birmingham, USA
3. AWPA E16 (2013) Standard field test for evaluation of wood preservatives to be used above ground (UC3B): horizontal lap-joint test. American Wood Protection Association. Birmingham, USA
4. AWPA E18 (2013) Standard field test for evaluation of wood preservatives to be used above ground (UC3B), ground proximity decay test. American Wood Protection Association. Birmingham, USA
5. AWPA E25 (2013) Standard field test for evaluation of wood preservatives to be used above ground (UC3B): decking test. American Wood Protection Association. Birmingham, USA
6. AWPA E27 (2013) Standard field test for evaluation of wood preservatives to be used above ground (UC3B): accelerated horizontal lap joint test. American Wood Protection Association. Birmingham, USA
7. AWPC (2007) Protocols for assessment of wood preservatives. Australian Wood Preservation Committee, Ensis
8. Blom Å, Bergström M (2006) Untreated Scots pine (Pinus sylvestris) and Norway spruce (Picea abies) wood-panels exposed out of ground contact in Sweden for two years. Holz Roh Werkst 64:53–6110.1007/s00107-005-0026-3 ↗
9. Bornemann T, Brischke C, Lück JM (2012) Comparative studies on the moisture performance and durability of wooden facades. The International Research Group on Wood Protection, IRG/WP 12-20492
10. Brischke C, Lampen SC (2014) Resistance based moisture content measurements on native, modified and preservative treated wood. Eur J Wood Prod 72:289–29210.1007/s00107-013-0775-3 ↗
11. Brischke C, Welzbacher CR, Meyer L, Bornemann T, Larsson-Brelid P, Pilgård A, Frühwald Hansson E, Westin M, Rapp AO, Thelandersson S, Jermer J (2011) Service life prediction of wooden components—Part 3: approaching a comprehensive test methodology. The International Research Group on Wood Protection, IRG/WP 11-20464
12. Brischke C, Meyer L, Alfredsen G, Humar M, Francis LP, Flæte PO, Larsson Brelid P (2012) Durability of timber products—Part 1: inventory and evaluation of above ground literature data on natural durability of timbers. The International Research Group on Wood Protection, IRG/WP 12-20498
13. Brischke C, Meyer L, Bornemann T (2013a) The potential of moisture content measurements for testing the durability of timber products. Wood Sci Technol 47:869–88610.1007/s00226-013-0548-5 ↗
14. Brischke C, Meyer L, Alfredsen G, Humar M, Francis L, Flæte PO, Larsson Brelid P (2013b) Natural durability of timber exposed above ground—a survey. Drvna Industrija 64:113–12910.5552/drind.2013.1221 ↗
15. CEN TS 12037 (2003) Wood preservatives—Field test method for determining the relative protective effectiveness of a wood preservative exposed out of ground contact—horizontal Lap-joint method. Beuth, Berlin
16. Clausen CA (1996) Bacterial associations with decaying wood: a review. Int Biodeterior Biodegrad 37:101–10710.1016/0964-8305(95)00109-3 ↗
17. Cookson LJ, Carr J (2009) Accelerated H3 above ground decay trials in Australia. The International Research Group on Wood Protection, IRG/WP 09-20411
18. De Groot RC (1992) Test assemblies for monitoring decay in wood exposed above ground. Int Biodeterior Biodegrad 29:151–17510.1016/0964-8305(92)90014-F ↗
19. EN 335 (2013) Durability of wood and wood-based products—use classes: definitions, application to solid wood and wood-based products. Beuth, Berlin
20. EN 330 (2014) Wood preservatives—Determination of the relative protective effectiveness of a wood preservative for use under a coating and exposed out-of-ground contact—field test: L-joint method. Beuth, Berlin
21. EN 252 (2015) Field test method for determining the relative protective effectiveness of a wood preservative in ground contact. Beuth, Berlin
22. Fougerousse M (1976) Wood preservatives: field tests out of ground contact—Brief survey of principles and methodology. The International Research Group on Wood Protection, IRG/WP 76-269
23. Francis LP, Norton J (2005) Above-ground durability estimation in Australia. Results after 16 years exposure. The International Research Group on Wood Protection, IRG/WP 05-20314
24. Fredriksson M (2010) Methods for determination of moisture conditions in wood exposed to high moisture levels. Licentiate thesis, Lund University, Lund Institute of Technology, Division of Building Materials, Lund
25. Friese F, Larnøy E, Alfredsen G, Pfeffer A, Militz H (2009) Comparison between different decay assessment methods. In: Proceedings of the 5th Meeting of the Nordic-Baltic Network in Wood Science and Engineering (WSE), Copenhagen, Denmark, pp 85–91
26. Highley TL (1995) Comparative durability of untreated wood in use above ground. Int Biodeterior Biodegrad 35:409–41910.1016/0964-8305(95)00063-1 ↗
27. Johansson P, Jermer J, Johansson I (2001) Field trial with wood preservatives for class AB. SP Swedish national testing and research institute, Boras
28. Kutnik M, Suttie E, Brischke C (2014) European standards on durability and performance of wood and wood-based products–Trends and challenges. Wood Mat Sci Eng 9(3):122–13310.1080/17480272.2014.894574 ↗
29. Laks PE, Mirros PI, Larkin GM, Ingram JK (2008) Field tests of naturally durable north american wood species. The International Research Group on Wood Protection, IRG/WP 08-10675
30. Larsson Brelid P, Brischke C, Pilgård A, Hansson M, Westin M, Rapp AO, Jermer J (2011) Methods of field data evaluation—time versus reliability. The International Research Group on Wood Protection, IRG/WP 11-20466
31. Meyer L, Brischke C, Rieken J (2013) Testing the performance of timber using 27 different field test methods. The International Research Group on Wood Protection, IRG/WP 13-20517
32. Meyer L, Brischke C, Kasselmann M, Rösmann C (2014) Moisture performance testing of wood—practical experiences. The International Research Group on Wood Protection, IRG/WP 14-20546
33. Meyer L, Brischke C, Preston A (2016) Testing the durability of timber above ground: a review on methodology. Wood Mater Sci Eng 11(5):283–30410.1080/17480272.2014.983163 ↗
34. Seidel A, Wiegand T (2001) Die Holzachterbahn “Colossos” in Soltau. (The wooden rollercoaster “Collossos” in Soltau) (in German). Bautechnik 78(10):747–74910.1002/bate.200104930 ↗
35. Van Acker J, Stevens M (2003) Biological durability of wood in relation to end-use—Part 2: the use of an accelerated outdoor L-joint performance test. Holz Roh-Werkst 61:125–13210.1007/s00107-002-0351-8 ↗
36. Wang CH, Leicester RH, Ngyen MN (2008) Decay above ground. Manual No.4. CSIRO Sustainable Ecosystems, Urban Systems Program, Highett, Victoria
37. Westin M, Rapp AO, Nilsson T (2004) Durability of pine modified by 9 different methods. The International Research Group on Wood Protection, IRG/WP 04-40288
38. Zahora A (2008) Above ground field testing—Influence of test method and location on the relative performance of various preservative systems. The International Research Group on Wood Protection, IRG/WP 08-20393