The potential of improving wood preservative penetration into glued wood products bonded with one-component polyurethane by discontinuous adhesive bondline design
Source abstract
Abstract
As a vast majority of glued wood products are intended for outdoor use or for building construction, impregnation with different agents is important for ensuring proper performance. It has been shown that the impregnation prior to gluing has several disadvantages, therefore the possibility of carrying out impregnation after gluing is analysed in the present research. Impregnation efficiency as well as the effect on the bond quality is evaluated for the one-component polyurethane glued wood specimens. The results showed that the impregnation with Cu preservative after gluing did not affect the shear strength of the glued wood specimens, but did significantly restrict Cu preservative penetration due to the adhesive bondlines. Considering the results, the possibility of improving the impregnation efficiency was also investigated. By using specific adhesive application designs, which cover the bondline only partially, it was possible to improve the impregnation efficiency. However, the Cu distribution was inhomogeneous and the improvement was noticeable only up to the second bondline. The partial adhesive application design also affected the bond strength of glued wood specimens, which resulted in a decrease both in dry and wet state. However, the reduction was not so sever as to cause delamination during three consecutive wetting and drying cycles.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Antons A, Cirule D, Verovkins A, Kuka E (2018) Effect of thermal treatment on physical and mechanical properties of birch and pine wood. Res Rural Dev 1:78–85. https://doi.org/10.22616/rrd.24.2018.01210.22616/rrd.24.2018.012 ↗
2. Bockel S, Harling S, Grönquist P, Niemz P, Pichelin F, Weiland G, Konnerth J (2020) Characterization of wood-adhesive bonds in wet conditions by means of nanoindentation and tensile shear strength. Eur J Wood Prod 78:449–459. https://doi.org/10.1007/s00107-020-01520-110.1007/s00107-020-01520-1 ↗
3. Bomba J, Šedivka P, Böhm M, Devera M (2014) Influence of moisture content on the bond strength and water resistance of bonded wood joints. BioResources 9:5208–5218. https://doi.org/10.15376/biores.9.3.5208-521810.15376/biores.9.3.5208-5218 ↗
4. Bowditch MR (1996) The durability of adhesive joints in the presence of water. Int J Adhes Adhes 16:73–79. https://doi.org/10.1016/0143-7496(96)00001-210.1016/0143-7496(96)00001-2 ↗
5. Cavalheiro SR, Neto CC, Christoforo LA, Junior CC, Lahr ARF (2016) Evaluation of shear strength and cyclic delamination of Paricá (Schizolobium amazonicum) glued laminated timber. Int J Mater Eng 6:60–65. https://doi.org/10.5923/j.ijme.20160602.0710.5923/j.ijme.20160602.07 ↗
6. Chen C, Yang J, Chen J, Zeng J, Wang W, Zhao X (2017) Fire resistance performance of glulam beam. J Cent South Univ 24:929–936. https://doi.org/10.1007/s11771-017-3495-810.1007/s11771-017-3495-8 ↗
7. Dias AMA, Martins CEJ, Dias AMPG (2020) Influence of the treatment phase on the gluing performance of glued laminated timber. BioResources 15:5725–5736. https://doi.org/10.15376/biores.15.3.5725-573610.15376/biores.15.3.5725-5736 ↗
8. Faria DL, Scatolino MV, Lopes TA, Junior LM, Mota GS, Junior JBG, Mendes LM, Soriano J (2020) Performance of glulam beams produced with free-formaldehyde adhesive and underexploited rubber wood treated with preservatives solutions of chromated copper borate and pyrethroids. J Adhes Sci Technol 34:1145–1162. https://doi.org/10.1080/01694243.2019.170007510.1080/01694243.2019.1700075 ↗
9. Hansmann C, Gindl W, Wimmer R, Teischinger A (2002) Permeability of wood—a review. Drev Vysk Res 47:1–16
10. Hart J, Pomponi F (2020) More timber in construction: Unanswered questions and future challenges. Sustain 12(8):3473. https://doi.org/10.3390/su1208347310.3390/su12083473 ↗
11. Hunt CG, Frihart CR, Dunky M, Rohumaa A (2018) Understanding wood bonds-going beyond what meets the eye: a critical review. Rev Adhes Adhes 6(4):369–440. https://doi.org/10.7569/RAA.2018.09731210.7569/RAA.2018.097312 ↗
12. Keskin H (2009) Impact of impregnation chemical on the bending strength of solid and laminated wood materials. Mater Des 30(3):796–803. https://doi.org/10.1016/j.matdes.2008.05.04310.1016/j.matdes.2008.05.043 ↗
13. Kläusler O, Clauß S, Lübke L, Trachsel J, Niemz P (2013) Influence of moisture on stress-strain behaviour of adhesives used for structural bonding of wood. Int J Adhes Adhes 44:57–65. https://doi.org/10.1016/j.ijadhadh.2013.01.01510.1016/j.ijadhadh.2013.01.015 ↗
14. Kläusler O, Hass P, Amen C, Schlegel S, Niemz P (2014) Improvement of tensile shear strength and wood failure percentage of 1C PUR bonded wooden joints at wet stage by means of DMF priming. Eur J Wood Prod 72:343–354. https://doi.org/10.1007/s00107-014-0786-810.1007/s00107-014-0786-8 ↗
15. Lehringer C, Schwarze FWMR, Militz H (2009) A review on promising approaches for liquid permeability improvement in softwood. Wood and Fiber Sci 41(4):373–385
16. Lehringer C, Gabriel J (2014) Review of recent research activities on one-component PUR-adhesives for engineered wood products. In: Aicher S, Reinhardt HW, Garrecht H (eds) Materials and joints in timber structures. RILEM Bookseries, vol 9. Springer, Dordrecht, pp 405–420. https://doi.org/10.1007/978-94-007-7811-5_3710.1007/978-94-007-7811-5_37 ↗
17. Long B, Morrell JJ (2012) Effects of postlayup borate treatment on appearance and flexural properties of Douglas-fir glued laminated beams. Forest Prod J 63(1):46–48. https://doi.org/10.13073/FPJ-D-11-00133.110.13073/FPJ-D-11-00133.1 ↗
18. Lorenz LF, Frihart C (2006) Adhesive bonding of wood treated with ACQ and copper azole preservatives. For Prod J 56:90–93
19. Mahnert KC, Hundhausen U (2018) A review on the protection of timber bridges. Wood Mater Sci Eng 13:152–158. https://doi.org/10.1080/17480272.2017.140395510.1080/17480272.2017.1403955 ↗
20. Olsson T, Megnis M, Varna J, Lindberg H (2001) Study of the transverse liquid flow paths in pine and spruce using scanning electron microscopy. J Wood Sci 47:282–288. https://doi.org/10.1007/BF0076671410.1007/BF00766714 ↗
21. Örs Y, Atar M, Keskin H (2004) Bonding strength of some adhesives in wood materials impregnated with Imersol-Aqua. Int J Adhes Adhes 24:287–294. https://doi.org/10.1016/j.ijadhadh.2003.10.00710.1016/j.ijadhadh.2003.10.007 ↗
22. Pisharody AP, Blandford B, Smith DE, Jack DA (2019) An experimental investigation on the effect of adhesive distribution on strength of bonded joints. Appl Adhes Sci 7:6. https://doi.org/10.1186/s40563-019-0122-y10.1186/s40563-019-0122-y ↗
23. Pitzner B, Rambol A, Lind P (2004) Evaluation of glulam beams after 6 years exposure to outdoor climate. FP-43/03, FP-58/03, FP-59/03 (TEFT) project report no. 57, Norwegian Institute of Wood Technology
24. Pizzi A (2016) Wood products and green chemistry. Ann for Sci 73:185–203. https://doi.org/10.1007/s13595-014-0448-310.1007/s13595-014-0448-3 ↗
25. Rasouli D, Bahmani M, Humar M (2017) Impregnability of Paulownia and Populus wood with copper based preservatives. Drvna Indus- Trija 68(3):211–218. https://doi.org/10.5552/drind.2017.170110.5552/drind.2017.1701 ↗
26. Sanne M, Ahn-Ercan G, Pfriem A (2020) A mathematical solution for calculating the springback of laminated beech stacks molded within the elastic range. Forests 11(7):725. https://doi.org/10.3390/f1107072510.3390/f11070725 ↗
27. Schuler A, Adair C (2003) Engineered and other wood products - An opportunity to ‘grow the pie’. In: 37th Int Wood Compos Mater Symp Proc, pp 43–53.
28. Silva A, Martins AC, Feio AO, Machado JS (2015) Feasibility of creosote treatment for glued-laminated pine-timber railway sleepers. J Mater Civ Eng 27(3):04014134. https://doi.org/10.1061/(ASCE)MT.1943-5533.000107310.1061/(ASCE)MT.1943-5533.0001073 ↗
29. Sonderegger W, Hering S, Mannes D, Vontobel P, Lehmann E, Niemz P (2010) Quantitative determination of bound water diffusion in multilayer boards by means of neutron imaging. Eur J Wood Prod 68:341–350. https://doi.org/10.1007/s00107-010-0463-510.1007/s00107-010-0463-5 ↗
30. Tarmian A, Zahedi TI, Oladi R, Efhamisisi D (2020) Treatability of wood for pressure treatment processes: a literature review. Eur J Wood Prod 78:635–660. https://doi.org/10.1007/s00107-020-01541-w10.1007/s00107-020-01541-w ↗
31. Temiz A, Alfredsen G, Yildiz UC, Gezer ED, Kose G, Akbas A, Yildiz S (2014) Leaching and decay resistance of alder and pine wood treated with copper based wood preservatives. Maderas Cienc y Tecnol 16(1):63–76. https://doi.org/10.4067/S0718-221X201400500000610.4067/S0718-221X2014005000006 ↗
32. Uysal B (2006) Influence of pretreatment on shear strength of various wood species. J Appl Polym Sci 100(1):245–252. https://doi.org/10.1002/app.2303010.1002/app.23030 ↗
33. Vick CB (1995) Coupling agent improves durability of PRF bonds to CCA-treated southern pine. For Prod J 45(3):78–84
34. Wimmer R, Kläusler O, Niemz P (2013) Water sorption mechanisms of commercial wood adhesive films. Wood Sci Technol 47:763–775. https://doi.org/10.1007/s00226-013-0538-710.1007/s00226-013-0538-7 ↗
35. Winandy JE, Morrell JJ (2017) Improving the utility, performance, and durability of wood- and bio-based composites. Ann for Sci 74:25. https://doi.org/10.1007/s13595-017-0625-210.1007/s13595-017-0625-2 ↗
36. Yildiz S (2007) Retention and penetration evaluation of some softwood species treated with copper azole. Build Environ 42(6):2305–2310. https://doi.org/10.1016/j.buildenv.2006.11.01510.1016/j.buildenv.2006.11.015 ↗