The potential of phenol–formaldehyde as plasticizing agent for moulding applications of wood veneer: two-dimensional and three-dimensional moulding
Source abstract
Abstract
Two phenol–formaldehyde resols, namely a low and a medium molecular weight phenol–formaldehyde, were investigated for their applicability as plasticizers in moulding of European beech veneer (Fagus sylvatica L.). Therefore, beech veneers specimens were impregnated with both phenol–formaldehyde resol types in various concentrations. Subsequently, two-dimensional mouldability of the veneer was tested in a three-point-bending test along and perpendicular to the grain. Additionally, three-dimensional moulding of the phenol–formaldehyde impregnated veneer was tested throughout a modified Erichsen cupping test, where the veneer is pressed through a circular shaped coining die. The obtained results indicate a significantly improved mouldability of the treated beech veneers compared to untreated, water-saturated control specimens. Even at low phenol–formaldehyde concentrations plasticizing effects were detected in longitudinal direction and perpendicular to the grain. These findings are substantiated by results from three-dimensional moulding. Furthermore, the low molecular weight phenol–formaldehyde treated veneers displayed a higher mouldability than medium molecular weight phenol–formaldehyde specimens at similar phenol–formaldehyde concentration.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Material Properties and Processing · Cultural Heritage Materials Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Beery WH, Ifu G, McLain TE (1983) Quantitative wood anatomy—relating anatomy to transverse tensile strength. Wood Fiber Sci 15(4):395–407
2. Biziks V, Bicke S, Militz H (2015) Penetration of phenol formaldehyde (PF) resin into beech wood studied by light microscopy. In: Annual Meeting of International Research group on Wood Protection, Vina del Mar, Chile. IRG/WP 15-20558
3. Buchelt B, Wagenführ A (2008) The mechanical behaviour of veneer subjected to bending and tensile loads. Holz Roh Werkst 66:289–29410.1007/s00107-008-0235-7 ↗
4. Davidson RW, Baumgardt WG (1970) Plasticizing wood with ammonia—a progress report. For Prod J 20(3):1925
5. DIN 50101, issue 1979-09 (withdrawn) Testing of metals; Erichsen cupping test on sheet and strip metal having a width of ≥ 90 mm; Thickness range: 0.2 to 2 mm. German Institute for Standardization
6. DIN 52186-06 (1978) Testing of wood; bending test (in German). German Institute for Standardization
7. Fekiac J, Zemiar J, Gaff M, Gabirik J, Gasparik M, Marusak R (2015) 3D-moldability of veneers plasticized with water and ammonia. BioResources 10(1):866–876
8. Franke T, Mund A, Lenz C, Herold N, Pfriem A (2017) Microscopic and macroscopic swelling and dimensional stability of beech wood impregnated with phenol-formaldehyde. Pro Ligno 13(4):373–378
9. Furuno T, Imamura Y, Kajita H (2004) The modification of wood by treatment with low molecular weight phenol-formaldehyde resin: a properties enhancement with neutralized phenolic-resin and resin penetration into wood cell walls. Wood Sci Technol 37:349–36110.1007/s00226-003-0176-6 ↗
10. Gabrielli CP, Kamke FA (2010) Phenol-formaldehyde impregnation of densified wood for improved dimensional stability. Wood Sci Technol 44:95–10410.1007/s00226-009-0253-6 ↗
11. Gasparik M, Barcik S (2013) Impact of plasticization by microwave heating on the total deformation of beech wood. BioResources 8(4):6297630810.15376/biores.8.4.6297-6308 ↗
12. Gasson P (1987) Some implications of anatomical variations in the wood of pedunculate oak (Quercus robur L.), including comparisons with common beech (Fagus sylvatica L.). IAWA Bull 8(2):149–16610.1163/22941932-90001042 ↗
13. Herold N, Pfriem A (2013) Impregnation of veneer with furfuryl alcohol for an improved plasticization and moulding. Eur J Wood Prod 71(2):281–28210.1007/s00107-013-0677-4 ↗
14. Herold N, Pfriem A (2014) Shape retention of furfurylated and moulded wood veneer. BioResources 9(1):545 553
15. Huang Y, Fei B, Zhao R (2014) Investigations of low-molecular weight phenol formaldehyde distribution in tracheid cell walls of Chinese fir wood. BioResources 9(3):4150415810.15376/biores.9.3.4150-4158 ↗
16. Huttunen J (1975) Method for plasticizing wood. US 3,894,569
17. Jebrane M, Harper D, Labbé N, Sèbea G (2011) Comparative determination of the grafting distribution and viscoelastic properties of wood blocks acetylated by vinyl acetate or acetic anhydride. Carbohydr Polym 84:1314–132010.1016/j.carbpol.2011.01.026 ↗
18. Kelley SS, Rials TG, Glasser WG (1987) Relaxation behaviour of the amorphous components of wood. J Mater Sci 22:617–62410.1007/BF01160778 ↗
19. Knop A, Pilato LA (1985) Phenolic resins. Chemistry, applications and performance—future directions. Springer, Berlin
20. Loughborough WK (1942) Process for plasticizing lignocellulosic materials. US 2,298,017 A
21. Norimoto M, Gril J (1989) Wood bending using microwave heating. J Microwave Power EE 24(4):203–212
22. Pfriem A, Dietrich T, Buchelt B (2012) Furfuryl alcohol impregnation for improved plasticization and fixation during densification of wood. Holzforschung 66:215–21810.1515/HF.2011.134 ↗
23. Pizzi A (2003) Phenolic resins. In: Pizzi A, Mittal KL (eds) Handbook of adhesive technology, 2nd edn. Taylor & Francis, New York
24. Sadoh T (1981) Viscoelastic properties of wood in swelling systems. Wood Sci Technol 15:57–66. https://doi.org/10.1007/BF0036650110.1007/BF00366501 ↗
25. Sass U, Eckstein D (1995) The variability of vessel size in beech (Fagus sylvatica L.) and its ecophysiological interpretation. Trees 9:24725210.1007/BF00202014 ↗
26. Schuerch C (1963) Plasticizing wood with liquid ammonia. Ind Eng Chem 55(10):3910.1021/ie50646a004 ↗
27. Shams MI, Yano H (2011) Compressive deformation of phenol formaldehyde (PF) resin-impregnated wood related to the molecular weight of resin. Wood Sci Technol 45:73–8110.1007/s00226-010-0310-1 ↗
28. Shams MI, Yano H, Endou K (2004) Compressive deformation of wood with low molecular weight phenol formaldehyde (PF) resin I: effects of pressing and pressure holding. J Wood Sci 50:337–34210.1007/s10086-003-0570-6 ↗
29. Sontag LA, Norton J (1935) Phenolic resin adhesives in the plywood industry. Ind Eng Chem 277(10):11141119
30. Stamm AJ, Seborg RM (1942) Resin treated wood (Impreg) Forest Products Laboratory. Report 1380 (Revised 1962)
31. Stamm AJ, Seborg RM (1955) Resin-treated, laminated compressed wood (Compreg). Forest Products Laboratory. Report 1381 (Revised 1960)
32. Wagenführ A, Buchelt B, Pfriem A (2006) Material behaviour of veneer during multidimensional moulding. Holz Roh Werkst 64:83–8910.1007/s00107-005-0008-5 ↗