Understanding the effect of PF glue impregnation on the shear strength of wood growth ring boundary
Source abstract
Abstract
The growth ring boundary substantially affects the mechanical performance of wood. Glue impregnation has been widely applied to wood protection. Shear strength of the growth ring boundary with and without glue impregnation under normal pressure (NP) and vacuum pressure (VP) conditions was measured using the lap-shear test, meanwhile strain distribution was recorded with digital image correlation. Glue distribution and microstructure in the specimens were visualized using scanning electron microscopy. Glue impregnation can switch specimens' failure location from growth ring boundary to earlywood or notches. Compared to the control specimens, shear strength and breaking elongation in VP specimens are significantly higher. Looking at the ruptured cross section, there are less ruptures in the control specimens and they are sharper and cleaner than in NP and VP specimens. In NP and VP specimens, the relationship between strength and elongation consists of four sections. In control specimens, the relationship between strength and elongation includes two sections. More sections could be due to residual stress from impregnation processes and breakage of glue. Such mechanical performance relates to the fact that tension strain is much larger than shear strain in NP and VP specimens, which protects the specimens from failing in the growth ring boundary.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Bamboo properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Aicher S, Christian Z, Hirsch M (2016) Rolling shear modulus and strength of beech wood laminations. Holzforschung 70:773–78110.1515/hf-2015-0229 ↗
2. Auad ML, Zhao L, Shen H et al (2007) Flammability properties and mechanical performance of epoxy modified phenolic foams. J Appl Polym Sci 104:1399–140710.1002/app.24405 ↗
3. Buksnowitz C, Evans R, Muller U, Teischinger A (2012) Indented rings (hazel growth of Norway spruce reduce anisotropy of mechanical properteis). Wood Sci Technol 46:1239–124610.1007/s00226-012-0480-0 ↗
4. Eder M, Jungnikl K, Burgert I (2009) A close-up view of wood structure and properties across a growth ring of Norway spruce (Picea abies [L.] Karst.). Trees 23:79–8410.1007/s00468-008-0256-1 ↗
5. H’ng PS, Chai LY, Chin KL, et al (2013) Urea formaldehyde impregnated oil palm trunk as the core layer for three layered board. Mater Des 50:457–46210.1016/j.matdes.2013.03.020 ↗
6. Jeong GY (2013) Relationship between anatomical and mechanical properties of Loblolly pine (Pinus taeda). For Prod J 63:47–53
7. Li WZ, Zhang Z, Zhou GQ et al (2020a) The effect of structural changes on the compressive strength of LVL. Wood Sci Technol 54:1253–126710.1007/s00226-020-01205-1 ↗
8. Li WZ, Zhang Z, Zhou GQ et al (2020b) Understanding the interaction between bonding strength and strain distribution of plywood. Int J Adhes Adhes 98:10250610.1016/j.ijadhadh.2019.102506 ↗
9. Li WZ, Zhang Z, Wang XZ et al (2021) Understanding the effect of growth ring orientation on the compressive strength perpendicular to the grain of thermally treated wood. Wood Sci Technol 55:1439–145610.1007/s00226-021-01323-4 ↗
10. Liu QQ, Du HJ, Lyu WH (2021) Physical and mechanical properties of poplar wood modified by glucose-urea-melamine resin/sodium silicate compound. Forests 12:12710.3390/f12020127 ↗
11. Maa M, Saleh S, Militz H, Volkert CA (2020) The structural origins of wood cell wall toughness. Adv Mater 32:190769310.1002/adma.201907693 ↗
12. Pambou Nziengui C, Turesson J, Moutou Pitti R et al (2020) Experimental assessment of the annual growth ring’s impact on the mechanical behavior of temperate and tropical species. BioResources 15:4282–429310.15376/biores.15.2.4282-4293 ↗
13. Sandberg D, Kutnar A, Mantanis G (2017) wood modification technologies—a review. iForest 10:895–90810.3832/ifor2380-010 ↗
14. Stanzl-Tschegg S, Beikircher W, Loidl D (2009) Comparison of mechanical properties of thermally modified wood at growth ring and cell wall level by means of instrumented indentation tests. Holzforschung 63:443–44810.1515/HF.2009.085 ↗
15. Walker J (2006) Primary wood processing. Springer Netherlands, Dordrecht
16. Wang BJ, Chui YH (2012) Manufacturing of LVL using cost-effective resin impregnation and layup technologies. Wood Sci Technol 46:1043–105910.1007/s00226-012-0465-z ↗
17. Wang XZ, Deng YH, Li YJ et al (2016) In situ identification of the molecular-scale interactions of phenol-formaldehyde resin and wood cell walls using infrared nanospectroscopy. RSC Adv 6:76318–7632410.1039/C6RA13159J ↗
18. Zhan K, Lu QX, Xia SW et al (2021) A cost effective strategy to fabricate STA@PF@Cu2O hierarchical structure on wood surface: aimed at superhydrophobic modification. Wood Sci Technol 55:565–58310.1007/s00226-021-01269-7 ↗
19. Zhou F, Fu ZY, Zhao YD et al (2019) Moisture transfer and stress development during high-temperature drying of Chinese fir. Drying Technol 38:545–55410.1080/07373937.2019.1588900 ↗