journal article·2025-02

Transforming inferior short-rotation teak: unleashing superior durability and stability with lactic acid-based bio-treatments

Efrida Basri, Gabriel Tobing, Saefudin, Titik Kartika, Yelin Adalina, Istie Sekartining Rahayu, Mahdi Mubarok, Wayan Darmawan, Philippe Gérardin

Publisher page

Abstract

Abstract This study focused on enhancing the properties of inferior short-rotation teak (SRT) wood through impregnation with lactic acid (LA)-based treatments, aiming to improve its dimensional stability, biological durability, and thermal stability. Using a vacuum-pressure process at 12.2 bar for two hours, followed by curing at 150 oC and 180 oC, the research found that wood treated at 180°C with a 10% LA and 10% citric acid (CA) composition demonstrated superior performance. Specifically, the treated wood exhibited higher anti-swelling efficiency (ASE), reduced water uptake (WU), swelling value (Sv), and water leaching (Wlc), as well as increased resistance to white-rot fungi, subterranean termites, and improved thermal stability. The best results were achieved with a 69% ASE, 27% WU, 3% Sv, and 1% Wlc, with wood resistance classified as Class I. Microscopic analysis revealed that the impregnants effectively filled the wood pores. Chemical analysis demonstrated a decrease in hemicellulose content and an increase in α-cellulose and lignin of the modified wood. FTIR analysis further confirmed strong chemical bonds formed between the LA + CA impregnants and wood cellulose and lignin. These findings highlight the potential of LA + CA-impregnated SRT wood cured at 180 oC for high-quality interior and exterior wood applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Natural Fiber Reinforced Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Anonim. Asam laktat [Internet]. [cited 2022 Sep 30]. https://p2k.unkris.ac.id/id3/3065-2962/Asam-Laktat_94291_p2kunkris.html.
2. Applefied M, Coleman VR, Motsinger RE, Beckwith JR (1986) Wood preservation and wood products treatment. American Wood Preservatives Institution, US. Forest Service and Sarious EPA and USDA.
3. American Wood Protection Association (2008) AWPA E7–07 Standard method of evaluating wood. Preservatives by field tests with stakes. American Wood Protection Association, Birmingham (US).
4. Bansal R, Mamatha N, Kumar R, Pandey KK (2024) Fungal resistance of Hevea brasiliensis (rubberwood) treated with nano-ZnO and nano-CuO dispersed linseed oil and parafn wax nanoemulsion. Euro J Wood Prod 82:1095–1109. https://doi.org/10.1007/s00107-024-02048-410.1007/s00107-024-02048-4 ↗
5. Bari E, Daniel G, Yilgor N, Kim JS, Tajick-Ghanbary MA, Singh AP, Ribera J (2020) Comparison of the decay behavior of two white-rot fungi in relation to wood type and exposure conditions. Microorganisms 8:1931. https://doi.org/10.3390/microorganisms812193110.3390/microorganisms8121931 ↗
6. Basri E, Balfas J (2014) Impregnation of teak extract and resin on fast growing teak wood and rubber. J Forest Prod Research 32(4):283–296 ((in Indonesian))
7. Basri E, Rahayu ES, Saefudin, Santoso A, Sulastiningsih IM, Damayanti R, Martha R, Darmawan W (2024) Enhancement on physicomechanical properties of short-rotation teak woods by non-biocide chemical and thermal treatments. Bioresources 19(2):3290–3305. https://doi.org/10.15376/biores.19.2.3290-3305.10.15376/biores.19.2.3290-3305 ↗
8. Beceiro JL, Diaz AMD, Garcia AA, Saavedra JT, Naya S, Artiaga R (2021) Complexity Lignin Thermal Degredation Isothermal Context 9(7):1154. https://doi.org/10.3390/pr907115410.3390/pr9071154 ↗
9. Standards B (1957) BS 373 Method of testing small clear specimens of timber. British Standards Institution, London
10. Browning BL (1967) Methods of wood chemistry. Interscience Publishers. A Division of John Wiley & Sons, New York – London – Sydney.
11. Candelier K, Thévenon MF, Collet R, Gérardin P, Dumarçay S (2020) Anti-fungal and anti-termite activity of extractives compounds from thermally modified ash woods. Maderas Ciencia y Tecnología 22(2):223–240
12. Chen S, Rui Liu R, Lei Y, Morrell JJ, Yan L (2021) Accelerating thermal decomposition of wood cell wall with glycerol. J Market Res 11:1637–1644. https://doi.org/10.1016/j.jmrt.2021.02.01110.1016/j.jmrt.2021.02.011 ↗
13. Choowang R, Hiziroglu S (2015) Properties of thermally-compressed oil palm trunks (Elaeis guineensis). J Trop Forest Sci 27:39–46
14. Dence CW (1992) The determination of lignin. In: Lin SY, Dence CW (eds) Methodes in lignin chemistry. Springer-Verlag, Berlin (DE), pp 33–6110.1007/978-3-642-74065-7_3 ↗
15. Dirna FC, Rahayu I, Zaini LH, Darmawan W, Prihatini E (2020) Improvement of fast-growing wood species characteristics by MEG and Nano SiO2 Impregnation. J Korean Wood Sci Tech 48(1):41–49. https://doi.org/10.5658/WOOD.2020.481.4110.5658/WOOD.2020.481.41 ↗
16. Djarwanto DR, Balfas J, Basri E, Jasni S et al (2017) Classification of types of Indonesian trade wood. FORDA Press, Bogor (ID)
17. European Standard (1996) EN 113 Wood preservatives - determination of toxic values of wood preservatives against wood destroying basidiomycetes cultured on agar medium. European Committee for Standardization, Brussels (BE).
18. Fatriasari W, Hermiati E (2016) Lignocellulosic biomass for bioproduct: its potency and technology development: a review. J Lignocellulose Tech 1:1–14
19. Fatriasari W, Masruchin N, Hermiati E (2019) Cellulose, its characteristics and uses. LIPI Press, Jakarta (ID)
20. Fazeli M, Mukherjee S, Baniasadi H, Abidnejad R, Muztaba M, Lipponen J, Seppälä J, Rojas OJ (2024) Lignin beyond the status quo: recent and emerging composite applications. Green Chem 26:593–630. https://doi.org/10.1039/D3GC03154C(CriticalReview)10.1039/D3GC03154C(CriticalReview) ↗
21. Gerardin P (2016) New alternatives for wood preservation based on thermal and chemical modification of wood - a review. Ann for Sci 73(3):559–570. https://doi.org/10.1007/s13595-015-0531-410.1007/s13595-015-0531-4 ↗
22. Goodell BS, Qian Y, Jellison J (2008) Fungal decay of wood: soft rot-brown rot-white rot. Development of commercial wood preservatives, 2nd Ch. pp 9–31. ACS Symposium Series Vol. 982. ISBN13: 9780841239517. eISBN: 9780841221208.10.1021/bk-2008-0982.ch002 ↗
23. Grosse C, Noel M, Thevenon MF, Gerardin P (2019) Improvement of modified wood properties with addition of chestnut tannins in lactic acid-based treatments. J Wood Chem Tech 39(2):124–135. https://doi.org/10.1080/02773813.2018.151303510.1080/02773813.2018.1513035 ↗
24. Gupta BS, Jelle BP, Gao T (2015) Wood façade materials ageing analysis by FTIR spectroscopy. ICE Proc Constr Mater 168:219–23110.1680/jcoma.13.00021 ↗
25. Hill CAS (2006) Wood modification: chemical, thermal and other processes. John Wiley and Sons Ltd, West Sussex (UK).10.1002/0470021748 ↗
26. Hunt GW, Garrat GA (1962) Wood preservation. McGraw-Hill Book Co., New York - St. Louis—San Fransisco—Toronto—London—Sydney.
27. Kong L, Guan H, Wang X (2018) In Situ polymerization of furfuryl alcohol with ammonium dihydrogen phosphate in poplar wood for improved dimensional stability and flame retardancy. ACS Sustain Chem 6(3):3349–3357. https://doi.org/10.1021/acssuschemeng.7b0351810.1021/acssuschemeng.7b03518 ↗
28. Kučerová V, Lagaňa R, Výbohová E et al (2016) The effect of chemical changes during heat treatment on the color and mechanical properties of fir wood. Bioresources. 11:9079–9094. https://doi.org/10.15376/biores.11.4.9079-9094.10.15376/biores.11.4.9079-9094 ↗
29. Li T, Cheng D, Avramidis S (2017) Response of hygroscopicity to heat treatment and its relation to durability of thermally modified wood. Constr Build Mater 144:671–676. https://doi.org/10.1016/j.conbuildmat.2017.03.21810.1016/j.conbuildmat.2017.03.218 ↗
30. Manimaran P, Saravanan SP, Sanjay MR, Siengchin S, Jawaid M, Khan A (2019) Characterization of new cellulosic fiber: Dracaena reflexa as a reinforcement for polymer composite structures. J Mater Res Tech 8(2):1952–1963. https://doi.org/10.1016/j.jmrt.2018.12.01510.1016/j.jmrt.2018.12.015 ↗
31. Mantanis GI, Lykidis C, Papadopoulos AN (2020) Durability of accoya wood in ground stake testing after 10 years of exposure in Greece. Polymers. 12:1638. https://doi.org/10.3390/polym12081638.10.3390/polym12081638 ↗
32. Martawijaya A, Kartasujana I, Kadir K, Prawira SA (2014) Indonesian Wood Atlas, Vol. 1. Agency for Forestry Research and Development, Forest Products Research and Development Center. Bogor-Indonesia.
33. Martha R, Basri E, Setiono L, Batubara I, Rahayu IS, Gerardin P, Darmawan W (2021) The effect of heat treatment on the characteristics of short rotation teak. Intern Wood Prod J. 12(3):1–10. https://doi.org/10.1080/20426445.2021.1953723.10.1080/20426445.2021.1953723 ↗
34. Moradbak A, Tahir PM, Mohamed AZ, Abdi MM, Razalli RL, Halis R (2018) Eur J Wood Prod 76(3):1021–1027. https://doi.org/10.1007/s00107-017-1244-110.1007/s00107-017-1244-1 ↗
35. Mubarok M, Militz H, Dumarcay S, Darmawan W, Hadi YS, Gerardin P (2021) Mechanical properties and biological durability in soil contact of chemically modified wood treated in an open or in a closed system using glycerol/maleic anhydride systems. Wood Mater Sci Eng. https://doi.org/10.1080/17480272.2021.187270110.1080/17480272.2021.1872701 ↗
36. Mubarok M, Militz H, Darmawan W, Hadi YS, Dumarçay S, Gérardin P (2020) Resistance against subterranean termite of beech wood impregnated with different derivatives of glycerol or polyglycerol and maleic anhydride followed by thermal modification: a field test study. Euro J Wood Prod 78(2):387–392. https://doi.org/10.1007/s00107-020-01503-210.1007/s00107-020-01503-2 ↗
37. Nandiyanto ABD, Ragadhita R, Fiandini M (2023) Interpretation of fourier transform infrared spectra (FTIR): a practical approach in the polymer/plastic thermal decomposition. Ind J Sci Tech. 8(1):113–126. https://doi.org/10.17509/ijost.v8i1.53297. p- ISSN 2528–1410 e- ISSN 2527–8045.10.17509/ijost.v8i1.53297 ↗
38. Nomanbhay SM, Hussain R, Palanisamy K (2013) Microwave-Assisted alkaline pretreatment and microwave assisted enzymatic saccharification of oil palm empty fruit bunch fiber for enhanced fermentable sugar yield. J Sustain Bioenergy Systems 3:7–1710.4236/jsbs.2013.31002 ↗
39. Olaniran SO, Iyiola EA, Hassan GF, Oladapo OD, Seriki JL (2023) Resistance of rubberwood (Hevea Brasiliensis Mull. Arg.) to brown-rot fungus (Serpula lacrymans) after treatment with teak heartwood extracts. Pro Ligno, 19(2): 29–37.
40. Owoyemi JM, Olaniran SO (2014) Natural resistance of ten selected nigerian wood species to subterranean termite’s attack. Intern J Bio Sci Applications 1(2):35–39
41. Papadopoulos AN, Bikiaris DN, Mitropoulos AC, Kyzas GZ (2019) Nanomaterials and chemical modification technologies for enhanced wood properties: a review. Nanomaterials 9(4):607. https://doi.org/10.3390/nano904060710.3390/nano9040607 ↗
42. Pavlov B, Terentyev A (1970) Organic chemistry. Foreign Language Publishing House, Moscow, USSR, A Textbook
43. Pfriem A, Dietrich T, Buchelt B (2012) Furfuryl alcohol impregnation for improved plasticization and fixation during the densification of wood. Holzforschung 66(2):215–128. https://doi.org/10.1515/HF.2011.13410.1515/HF.2011.134 ↗
44. Rizanti DE, Darmawan W, George B, Merlin A, Dumarcay S, Chapuis H, Gerardin C, Gelhaye E, Raharivelomanana P, Kartika Sari R et al (2018) Comparison of teak wood properties according to forest management: short versus long rotation. Ann for Sci 75(2):1–12. https://doi.org/10.1007/s13595-018-0716-810.1007/s13595-018-0716-8 ↗
45. Ross R (2021) Wood handbook: wood as an engineering material, general technical report. Forest Products Laboratory, Madison.
46. Saefudin, Basri E, Santoso A (2018) Natural dyes for batik and weaving. Rolliadi H, Effendi R, Setio P (ed). Forda Press, Bogor (ID). ISBN 978-602-6961-29-7.
47. Salman S, Thevenon MF, Petrissans A, Dumarcay S, Candelier K, Gerardin P (2017) Improvement of the durability of heat-treated wood against termites. Maderas-Cienc Tecnol 19(3):1–22. https://doi.org/10.4067/S0718-221X201700500002710.4067/S0718-221X2017005000027 ↗
48. Sarvaramini A, Larachi F (2017) Pyrolysis kinetics of pre-torrefied woody biomass based on torrefaction severity- experiments and model verification. Ind Eng Chem Res 56(45):12972–12983. https://doi.org/10.1021/acs.iecr.7b0112310.1021/acs.iecr.7b01123 ↗
49. Shin SK, Ko YJ, Hyeon JE, Han SO (2019) Studies of advanced lignin valorization based on various types of lignolytic enzymes and microbes. Bioresource Tech. 289.10.1016/j.biortech.2019.121728 ↗
50. Shmulsky R, Jones PD (2019) Forest products and wood science: an introduction, (7th ed). Wiley-Blackwell, West Sussex.10.1002/9781119426400 ↗
51. Sjöström E (1993) Wood chemistry: fundamentals and applications, 2nd edn. Academic Press Inc, Sand Diego-New York-Boston
52. Soerianegara I, Lemmens RHMJ (1995) Plant resource of south- east asia, major commercial timber. Prosea Foundation, Leiden.
53. Standard Nasional Indonesia (2014) SNI 7207–2014 Testing the resistance of wood and wood products to wood-destroying organisms. National Standardization Agency, Jakarta (ID).
54. Technical Association of Pulp and Paper Industry (1999) T- 203 alpha-, beta-, gamma-cellulose in pulp. TAPPI, Atlanta (GA).
55. Thulasidas PK, Bhat KM (2007) Chemical extractive compounds determining the brown-rot decay resistance of teak wood. Holz Roh- Werkst 65(2):121–124. https://doi.org/10.1007/s00107-006-0127-710.1007/s00107-006-0127-7 ↗
56. Vančik H (2022) Derivatives of Carboxylic Acids. In Basic Organic Chemistry for the Life Science. Textbook, (Latest Ed). https://doi.org/10.1007/978-3-030-92438-6. Springer Link. ISBN: 978-3-030-92437-9. P 117-125.10.1007/978-3-030-92438-6 ↗
57. Yildiz S, Tomak ED, Yildiz UC, Ustaomer D (2013) Effect of artificial weathering on the properties of heattreated wood. Polym Degrad Stab 98(8):1419–1427. https://doi.org/10.1016/j.polymdegradstab.2013.05.00410.1016/j.polymdegradstab.2013.05.004 ↗
58. Zelinka SL, Altgen M, Emmerich L, Guigo N, Keplinger T, Kymäläinen M, Emil E, Thybring EE, Thygesen LG (2022) Review of wood modification and wood functionalization technologies. Forests 13(1004):1–46. https://doi.org/10.3390/f1307100410.3390/f13071004 ↗
59. Zhang Y, Li N, Chen Z, Ding C (2020) Synthesis of high-water-resistance lignin-phenol resin adhesive with furfural as a crosslinking agent. Polymers 12(12):2805. https://doi.org/10.3390/polym1212280510.3390/polym12122805 ↗
60. Zhao X, van der Heide E, Zhang T, Liu D (2010) Delignification of sugarcane bagasse with alkali and peracetic acid and characterization of the pulp. BioResources 5(3):1565–1580. https://doi.org/10.15376/biores.5.3.1565-158010.15376/biores.5.3.1565-1580 ↗