journal article·2011-11

Artificial ageing of softwood joints and its effect on internal bond strength with special consideration of flat-to-end grain joints

Jürgen Follrich, Alfred Teischinger, Ulrich Müller

Publisher page

Abstract

The effect of ageing processes on internal bond strength of three-part specimens produced from Norway spruce wood (Picea abies Karst.) bonded with one-component polyurethane (PUR), two-component emulsion polymer isocyanate (EPI), melamine-urea-formaldehyde (MUF) or phenol-resorcinol-formaldehyde (PRF) adhesive was studied. By varying the grain angle of the middle part from 0° (parallel to grain of the surface layers) to 90° (perpendicular to grain of the surface layers) in incremental steps of 10° the effect of grain direction was investigated. The specimens were exposed to a three-step ageing cycle lasting for seven days (50°C/95% relative humidity (rH), −20°C/65–70% rH and 75°C/15% rH) which was repeated twelve and twenty-four times, respectively. In general, a decrease in internal bond strength of the exposed specimens was observed. For all tested adhesive systems, influence of ageing processes was more pronounced for flat-to-end grain joints compared to longitudinal joints. For samples bonded with PUR adhesive strength reduction was lower compared to the other adhesives used.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Natural Fiber Reinforced Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. American society of testing and materials—ASTM (1992) Standard test method for strength properties of adhesive bonds in shear by compression loading. ASTM D-905-89. Vol 15.06. Adhesives. ASTM, Philadelphia, Pa
2. Back E, Sandström E (1982) Critical aspects on accelerated methods for predicting weathering resistance of wood based panels. Holz Roh- Werkst 40(2):61–7510.1007/BF02612224 ↗
3. Blanchet P, Beauregard R, Erb A, Lefebvre M (2003) Comparative study of four adhesives used as binder in engineered wood parquet flooring. For Prod J 53(1):89–93
4. Clad W (1958) Prüfung gefüllter Leime. Holz Roh- Werkst 16(10):383–39510.1007/BF02617857 ↗
5. Clad W (1960) Die Beurteilung von Harnstoffharzleimen auf Grund ihrer Prüfung. Holz Roh- Werkst 18(10):391–40010.1007/BF02605817 ↗
6. Davis G (1997) The performance of adhesive systems for structural timbers. Int J Adhes Adhes 17(3):247–25510.1016/S0143-7496(97)00010-9 ↗
7. Deppe E, Schmidt K (1982) Zur Beurteilung von Holzwerkstoffen im Kurzzeit-Bewitterungsversuch – Teil 1: Grundlegendes, Vergleich der Kurzzeitverfahren. Holz Roh- Werkst 40(12):471–47310.1007/BF02606920 ↗
8. Deppe E, Schmidt K (1994) Ergänzende Untersuchungen zum Alterungsverhalten gestreckter Holzmontageverleimungen. Holz Roh- Werkst 52(6):355–36010.1007/BF02615384 ↗
9. DIN 52184 (1979) Testing of wood; determination of swelling and shrinking. Normenausschuß in Holz DIN
10. Dunky M, Niemz P (2002) Holzwerkstoffe und Leime – Technologie und Einflussfaktoren. Springer, Berlin10.1007/978-3-642-55938-9 ↗
11. Egner K, Kolb H (1966) Versuche über das Alterungsverhalten von Leimen für tragende Holzbauteile. Holz Roh- Werkst 24(10):439–44210.1007/BF02612869 ↗
12. EN 301 (1992) Adhesives, phenolic and aminoplastic, for load bearing timber structures—classification and performance requirements. Österreichisches Normungsinstitut, Wien
13. EN 302-1 (2004) Adhesives for load bearing timber structures—test methods—part 1: determination of bond strength in longitudinal tensile shear strength. Österreichisches Normungsinstitut, Wien
14. Endicott LE, Frost TR (1967) Correlation of accelerated and long term stability tests for wood based composite products. For Prod J 17(10):35–40
15. Follrich J, Teischinger A, Gindl W, Müller U (2007) Internal bond strength of flat to end grain softwood joints. Wood Res-Slovak 52(3):49–58
16. Follrich J, Müller U, Teischinger A (2009) Einfluss der spezifischen Leimauftragsmenge und des Faserwinkels auf die Querzugfestigkeit einer Holzverklebung. Holztechnologie 50(5):12–18
17. Gereke T, Schnider T, Hurst A, Niemz P (2009) Identification of moisture-induced stresses in cross-laminated wood panels from beech wood (Fagus sylvatica L.). Wood Sci Technol 43(5–6):301–31510.1007/s00226-008-0218-1 ↗
18. Gindl W, Sretenovic A, Vincenti A, Müller U (2005) Direct measurement of strain distribution along a wood bond line—part II: effects of adhesive penetration on strain distribution. Holzforschung 59(3):307–31010.1515/HF.2005.051 ↗
19. Gindl W, Müller U (2006) Shear strain distribution in PRF and PUR bonded 3-ply wood sheets by means of electronic laser speckle interferometry. Wood Sci Technol 40(5):351–35710.1007/s00226-005-0051-8 ↗
20. George B, Simon C, Properzi M, Pizzi A, Elbez G (2003) Comparative creep characteristics of structural glulam wood adhesives. Holz Roh- Werkst 61(1):79–8010.1007/s00107-002-0348-3 ↗
21. Green DW, Winandy JE, Kretschmann DE (1999) Mechanical properties of wood. In: Wood handbook—wood as an engineering material. USDA Forest Products Laboratory, Madison, Chap 4
22. Gressel P (1980a) Prüfung und Beurteilung der Dauerhaftigkeit von Spanplattenverleimungen. Ein Beitrag zur Aufstellung klebstoffunabhängiger Prüfrichtlinien – Teil 1: Aufgabenstellung – Planung und Durchführung der Versuche – Ergebnisse. Holz Roh- Werkst 38(1):17–3510.1007/BF02612827 ↗
23. Gressel P (1980b) Prüfung und Beurteilung der Dauerhaftigkeit von Spanplattenverleimungen. Ein Beitrag zur Aufstellung klebstoffunabhängiger Prüfrichtlinien – Teil 2: Diskussion der Ergebnisse. Holz Roh- Werkst 38(2):61–7110.1007/BF02625306 ↗
24. Gressel P (1980c) Prüfung und Beurteilung der Dauerhaftigkeit von Spanplattenverleimungen. Ein Beitrag zur Aufstellung klebstoffunabhängiger Prüfrichtlinien – Teil 3: Folgerungen und Vorschlag von Prüfrichtlinien. Holz Roh- Werkst 38(3):61–7110.1007/BF02607525 ↗
25. Gustódio J, Broughton J, Cruz H (2009) A review of factors influencing the durability of structural bonded timber joints. Int J Adhes Adhes 29(2):173–18510.1016/j.ijadhadh.2008.03.002 ↗
26. Jönsson J, Svensson S (2004) A contact free measurement method to determine internal stress states in glulam. Holzforschung 58(2):148–15310.1515/HF.2004.022 ↗
27. Kaminski A, Matejak M, Popowska E (1982) Einfluß des Alterns von Holz unter künstlichen Klimabedingungen auf seine Druckfestigkeit längs der Faser. Holzforsch Holzverwert 34(2):21–24
28. Kaminski A, Popowska E, Szejka E (1983) Vergleichende Untersuchungen über Methoden des beschleunigten Alterns von Holz. Holzforsch Holzverwert 35(5):117–119
29. Konnerth J, Valla A, Gindl W, Müller U (2006) Measurement of strain distribution in timber finger joints. Wood Sci Technol 48(8):631–63610.1007/s00226-006-0090-9 ↗
30. Küch W (1954) Über die Feuchtfestigkeit von Holzleimen. Holz Roh- Werkst 12(11):434–44210.1007/BF02628763 ↗
31. Marra AA (1992) Technology of wood bonding—principles in practice. Van Nostrand–Reinhold, New York, pp 231–232
32. Müller U, Sretenovic A, Vincenti A, Gindl W (2005) Direct measurement of strain distribution along a wood bond line—part I: shear strain concentration in a lap joint specimen by means of electronic speckle pattern interferometry. Holzforschung 59(3):300–30610.1515/HF.2005.050 ↗
33. Noack D, Geissen A (1976) Einfluß von Temperatur und Feuchtigkeit auf den E-Modul des Holzes im Gefrierbereich. Holz Roh- Werkst 34(2):55–6210.1007/BF02612756 ↗
34. Northcott PL, Kreibich RE, Currier RA (1968) First replications comparing bond degrade accelerating systems. For Prod J 18(5):58–65
35. Özdemir S (2009) Alterungsmechanismen von Klebstoffen für tragende Holzbauteile. Masterthesis. BOKU, Vienna
36. Raknes E (1983) Durability of structural wood adhesives after 15 years aging. Ind Eng Chem Prod Res Dev 22(4):662–66410.1021/i300012a027 ↗
37. Raknes E (1997) Durability of structural wood adhesives after 30 years ageing. Holz Roh- Werkst 55(2–4):83–9010.1007/BF02990523 ↗
38. River BH, Vick CB, Gillespie RH (1991) Wood as an adherend. In: Minford CD (ed) Treatise on adhesion and adhesives. Dekker, New York, pp 1–238
39. Serrano E (2004) A numerical study of the shear-strength-predicting capabilities of test specimens for wood-adhesive bonds. Int J Adhes Adhes 24(1):23–3510.1016/S0143-7496(03)00096-4 ↗
40. Serrano E, Enquist B (2005) Contact-free measurement and non-linear finite element analyses of strain distribution along wood adhesive bonds. Holzforschung 59(6):641–64610.1515/HF.2005.103 ↗
41. Vick CB (1999) Adhesive bonding of wood materials. In: Wood handbook—wood as an engineering material. USDA Forest Products Laboratory, Madison, Chap 9
42. Wagenführ A, Scholz F (2008) Taschenbuch der Holztechnik. Fachbuchverlag Leipzig. Hanser Verlag, München, 82 pp