journal article·2010-11Open access

Colour stabilisation of wood composites using polyethylene glycol and melamine resin

Uwe Müller, Melanie Steiner

Abstract

Photo-yellowing of native and polyethylene glycol (PEG) modified wood and wood/melamine resin composites was studied by means of FTIR-ATR technique and colourimetry (CIE L*a*b* method). The discolouration $$ \mathrm{\Delta } $$ E shows a systematic asymptotic trend towards higher values with increasing irradiation time. Yellowing proceeds faster in natural wood compared to wood/melamine resin composites. Nevertheless, long-term irradiation experiments show that the total colour shift is similar for both.Discolouration is significantly reduced by PEG treatment. In comparison to untreated wood, both glycol and melamine resin mainly reduce the irradiation-induced yellow shift. Moreover, PEG also shows an effect on the redness shift. Both effects result in decreased yellowing of the composite surface. An influence of the molecular weight of PEG was detected.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Cultural Heritage Materials Analysis · Dyeing and Modifying Textile Fibers · Wood Treatment and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Anonymus (2004) www.leaderplus.de/leaderplus/leaderforum/LEADERforum_2004-1_Aktiv.pdf , see also www.sema-gmbh.de
2. Andrady AL, Hamid SH, Hu X, Torikai AJ (1998) Effects of increased solar ultraviolet radiation on materials. J Photoch Photobio B 46:96–103
3. Becker HGO (ed), Böttcher H, Dietz F, Rehorek D, Roewer G, Schiller K, Timpe HJ (1991) Einführung in die Photochemie. Deutscher Verlag der Wissenschaften, Berlin
4. Beyer M, Bäurich C, Fischer K (1995) Mechanismen der licht- und wärmeinduzierten Vergilbung von Faserstoffen. Das Papier 49:V8–V14
5. Beyer M, Krasselt K, Fischer K, Jacob H, Süss H-U (2001) Brightness reversion of bleached mechanical pulps – New stabilizing substances and mechanical investigations. In: Proceedings of the 11th international symposium on wood and pulping chemistry, Nice, vol. III, pp 215–218
6. Charter HA (1996) The chemistry of paper preservation: Part 2. The yellowing of paper and conservation bleaching. J Chem Educ 73:1068–1073
7. Derbyshire H, Miller ER (1981) The photodegradation of wood during solar irradiation. Holz Roh- Werkst 39:341–35010.1007/BF02608404 ↗
8. Derbyshire H, Miller ER, Turkulin H (1995) Investigations into the photodegradation of wood using microtensile testing, Part 1: The application of microtensile testing to measurement of photodegradation rates. Holz Roh- Werkst 53:339–34510.1007/s001070050103 ↗
9. DIN 6174 (1979) Farbmetrische Bestimmung von Farbabständen bei Körperfarben nach der CIELAB-Formel. Deutsches Institut für Normen, Beuth Verlag, Berlin
10. Durovič M, Zellinger J (1993) Chemical processes in the bleaching of paper in library and archival collections. Restaurator 14:78–101
11. Feist WC, Hon DN-S (1984) Chemistry of weathering and protection. In: Rowell R (ed) Chemistry of solid wood, Advances in Chemistry Series No. 207. American Chemical Society, Washington, DC, pp 401–45110.1021/ba-1984-0207.ch011 ↗
12. Gindl W, Dessipri E, Wimmer R (2002) Using uv-microscopy to study diffusion of melamine-urea-formaldehyde resin in cell walls of spruce wood. Holzforschung 56:103–10710.1515/HF.2002.017 ↗
13. Gsöls I, Müller U, Steiner M, Rätzsch M (2002) Interaction between resins and wood. In: Lignovisionen, issue 4/special edition (Proceedings of the international symposium on wood based materials wood composites and wood chemistry, Vienna, 19–20 September 2002), BOKU, Vienna, November 2003, pp 193–201
14. Gsöls I, Rätzsch M, Ladner C (2003) Interactions between wood and melamine resins – effect on dimensional stability properties and fungal attack. In: Proceedings of the first european conference on wood modification, Ghent, Belgium, pp 221–225
15. Hansmann C, Deka M, Wimmer R, Gindl W (2006) Artificial weathering of wood surfaces modified by melamine resins. Holz Roh- Werkst 64:198–20310.1007/s00107-005-0047-y ↗
16. Harrick N (1980) Internal reflection spectroscopy. Interscience, New York
17. Hayoz P, Peter W, Rogez D (2003) A new innovative stabilization method for the protection of natural wood. Prog Org Coat 48:297–30910.1016/S0300-9440(03)00102-4 ↗
18. Heitner C (1993) Light-induced yellowing of wood containing papers. In: Heitner C, Scaiano JC (eds) Photochemistry of lignocellulosic materials, ACS symposium series 531. American Chemical Society, Washington, DC, pp 3–2510.1021/bk-1992-0531 ↗
19. Hillis WE (1971) Distribution, properties and formation of some wood extractives. Wood Sci Technol 5:272–28910.1007/BF00365060 ↗
20. Hon DNS (1981) Yellowing of modern papers. In: Williams JC (ed) Preservation of paper and textiles of historic and artistic value II. American Chemical Society, Washington DC, pp 119–141
21. Hon DNS (2001) Weathering and photochemistry of wood. In: Hon DNS, Shiraishi N (eds) Wood and cellulosic chemistry, 2nd edn. Marcel Dekker, New York, pp 512–546
22. Hon DNS, Minemura N (2001) Color and discoloration. In: Hon DNS, Shiraishi N (eds) Wood and cellulosic chemistry, 2nd edn. Marcel Dekker, New York, pp 385–442
23. Hon DNS, Ifju G (1978) Measuring penetration of light into wood by detection of photo-induced free radicals. Wood Sci 11:118–127
24. Inoue M, Ogata S, Nishikawa M, Otsuka Y, Kawai S, Norimoto M (1993) Dimensional stability, mechanical properties, and color changes of a low molecular weight melamine formaldehyde resin impregnated wood. Mokuzai Gakkaishi 39:181–189
25. Johnston LJ, Wong K (1984) Surface chemistry: 13C enrichment by photolysis on silica gel. Can J Chem 62:1999–200510.1139/v84-341 ↗
26. Kataoka Y, Kiguchi M, Fujiwara T (2005) The effects within-species and between-species variation in wood density on the photodegradation depth profiles of sugi (Cryptomerica japonica) and hinoki (Chamaecyparis obtusa). J Wood Sci 51: 531–53610.1007/s10086-004-0685-4 ↗
27. Kataoka Y, Kiguchi M, Williams RS, Evans PD (2007) Violet ligth causes photodegradation of wood beyond the zone affected by ultraviolet radiation. Holzforschung 61:23–2710.1515/HF.2007.005 ↗
28. Kiguchi M, Evans PD (1998) Photostabilisation of wood surfaces using a grafted benzophenone UV absorber. Poly Degrad Stabil 61:33–4510.1016/S0141-3910(97)00124-9 ↗
29. Larkin PJ, Makowski MP, Colthup NB, Flood LA (1998) Vibrational analysis of some important group frequencies of melamine derivatives containing methoxymethyl, and carbamate substituents: mechanical coupling of substituent vibrations with triazine ring modes. Vib Spectrosc 17:53–7210.1016/S0924-2031(98)00015-0 ↗
30. Liang CY, Marchessault RH (1959) Infrared spectra of crystalline polysaccharides. II. Native celluloses in the region from 640 to 1700 cm−1. J Polym Sci 39:269–27810.1002/pol.1959.1203913521 ↗
31. Lukowsky D (1999) Holzschutz mit Melaminharzen. Dissertation. University of Hamburg
32. Mahoney LR (1969) Antioxidantien. Angew Chem 81/15:555–56310.1002/ange.19690811503 ↗
33. Müller U, Steiner M, Rätzsch M (2002) Photostabilization of wood without topcoat – influence of UV-absorber and radical scavenger. In: Lignovisionen, issue 4/special edition (Proceedings of the international symposium on wood based materials wood composites and wood chemistry, Vienna, 19–20 September 2002), BOKU, Vienna, November 2003, pp 329–336
34. Müller U, Rätzsch M, Schwanninger M, Steiner M, Zöbl H (2003) Yellowing and IR-changes of spruce wood as result of UV-irradiation. J Photoch Photobio B 69:97–105
35. Norimoto M (1996) Viscoelastic properties of chemically modified wood. In: Hon DN-S (ed) Chemical modification of lignocellulosic materials. Marcel Dekker, New York, pp 311–330
36. Norimoto M (2001) Chemical modification of wood. In: Hon DNS, Shiraishi N (eds) Wood and Cellulosic Chemistry. Part I: Structure and Chemistry. Marcel Dekker, New York Basel, pp 3–53
37. Oltean L, Teischinger A, Hansmann C (2008) Wood surface discolouration due to simulated indoor sunlight exposure. Holz Roh- Werkst 66:51–5610.1007/s00107-007-0201-9 ↗
38. Pandey KK (2005) A note on the influence of extractives on the photo-discoloration and photo-degradation of wood. Polym Degrad Stabil 87:375–37910.1016/j.polymdegradstab.2004.09.007 ↗
39. Pittman C, Kim M, Nicholas D, Wang L, Kabir A, Schultz T, Ingram L (1994) Wood enhancement treatments I. Impregnation of southern yellow pine with melamine-formaldehyde and melamine-ammeline-formaldehyde resins. J Wood Chem Technol 14:577–60310.1080/02773819408003114 ↗
40. Rabek JF (1995) Polymer degradation. Chapman and Hall, London
41. Rapp AO, Peek RD (1999) Melaminharzimprägniertes sowie mit Wetterschutzlasur oberflächenbehandeltes und unbehandeltes Vollholz während zweijähriger Freilandbewitterung. Holz Roh- Werkst 57:331–33910.1007/s001070050353 ↗
42. Rosca I, Bergmann I, Tanczos I (2005) Penetrability of resins and polyethylene glycols in ammonia treated spruce wood. Holz Roh- Werkst 63:403–40710.1007/s00107-005-0053-0 ↗
43. Schaller C, Rogez D (2007) New approaches in wood coating stabilization. J Coat Technol Res 4:401–40910.1007/s11998-007-9049-5 ↗
44. Scherzer T (2002) Depth profling of the degree of cure during the photopolymerization of acrylates studied by real-time FT-IR attenuated total reflection spectroscopy. Appl Spectrosc 56:1403–141210.1366/00037020260377698 ↗
45. Scott GG (1990) Polymer degradation and stabilization. Elsevier Applied Science, London
46. Tolvaj L, Mitsui K (2005) Light source dependence of the photodegradation of wood. J Wood Sci 51:468–473
47. Turkulin H, Sell J (2002) Tensile properties and fractography of weathered wood. Holz Roh- Werkst 60:96–10510.1007/s00107-002-0282-4 ↗
48. Turkulin H, Derbyshire H, Miller ER (2004) Investigations into the photodegradation of wood using microtensile testing. Part 5: The influence of moisture on photodegradation rates. Holz Roh- Werkst 62:307–31210.1007/s00107-004-0493-y ↗
49. Wallström L, Lindberg KAH (1999) Measurement of cell wall penetration in wood of water-based chemicals using SEM/EDS and STEM/EDS technique. Wood Sci Technol 33:111–12210.1007/s002260050103 ↗