A METHOD TO MEASURE ELECTROCHEMICAL POTENTIAL AT THE TIP OF A GROWING CRACK DURING AN ENVIRONMENTAL FATIGUE TEST
Source abstract
Abstract
Abstract— Electrochemical potential at the tip of a fatigue crack was measured in a compact tension specimen, situated in demineralized, oxygen saturated water at 93°C. Results show that the crack tip region is active with respect to the external specimen surface. Passivation occurs on the crack surfaces by the formation of an oxide layer. The oxygen concentration inside the crack is likely to be lower than in the bulk solution.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · Ultrasonics and Acoustic Wave Propagation · Fire effects on concrete materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (5)
Show source-provided references
1. 10.1016/0025-5416(78)90124-610.1016/0025-5416(78)90124-6 ↗
2. Smith Peterson · Corros. NACE · 1970 · 26 · 53910.5006/0010-9312-26.12.539 ↗
3. Turnbull · Br. Corros. J. · 1980 · 14 · 140
4. 4. Indig (1979 ) Electrochemical/CERT evaluations of carbon steel. Paper presented at the Corrosion Advisory Committee Workshop on SCC and CF of Carbon and Low Alloy Steel E.P.R.I., Palo Alto, Ca.
5. 5. Gabetta, and Fossati (1981 ) Oxide formation inside a cyclically loaded crack and its effect on environmental enhanced crack growth rate in 93oC water. Paper presented at the IAEA Specialists Meeting on Subcritical Crack Growth, Freiburg (F.R.G.), May 13-15, 1981.