journal article·2004-02

Preliminary study of the crack healing and strength recovery of Al2O3‐matrix composites

L. JUN, Z. X. ZHENG, H. F. DING, Z. H. JIN

Publisher page

Abstract

ABSTRACT This study focused on the crack‐healing behaviour of three commercial Al2O3–ceramic‐matrix composites: TiCP/Al2O3, ZrO2/Al2O3 and SiCW/Al2O3. Vickers indentation was used to introduce surface flaws with different loads of 49, 98 and 196 N. Then the cracked specimens were annealed in air for 1 h at 1000, 1200 and 1400 °C. The annealing treatment was also conducted at 1200 °C in vacuum for 1 h. Results showed that the annealing treatments increased the indentation strength, but the extent of the increase was different. When annealed in air, the main crack‐healing mechanism of TiCP/Al2O3 and SiCW/Al2O3 composites was chemical reaction. When annealed in vacuum, stress relaxation caused much less strength recovery. The main crack‐healing mechanism of ZrO2/Al2O3 was the existence of low melting eutectic and the rearrangement of grains caused by ZrO2(m)→ ZrO2(t) transformation in the crack‐opening process zone. The effects of annealing temperature, atmosphere and indentation load on the degree of strength recovery were all related to the crack‐healing mechanisms.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. 10.1111/j.1151-2916.1975.tb19578.x10.1111/j.1151-2916.1975.tb19578.x ↗
2. 10.1111/j.1151-2916.1976.tb10949.x10.1111/j.1151-2916.1976.tb10949.x ↗
3. 10.1111/j.1151-2916.1988.tb05064.x10.1111/j.1151-2916.1988.tb05064.x ↗
4. 10.1016/0921-5093(93)90394-T10.1016/0921-5093(93)90394-T ↗
5. 10.1111/j.1151-2916.1999.tb01959.x10.1111/j.1151-2916.1999.tb01959.x ↗
6. 10.1111/j.1151-2916.1997.tb03064.x10.1111/j.1151-2916.1997.tb03064.x ↗
7. 10.1111/j.1151-2916.1995.tb08215.x10.1111/j.1151-2916.1995.tb08215.x ↗
8. 10.1111/j.1151-2916.1998.tb02469.x10.1111/j.1151-2916.1998.tb02469.x ↗
9. 10.1007/BF0036894110.1007/BF00368941 ↗
10. 10.1007/BF0115468210.1007/BF01154682 ↗
11. 10.1111/j.1151-2916.2000.tb01632.x10.1111/j.1151-2916.2000.tb01632.x ↗
12. 10.1046/j.1460-2695.1999.00210.x10.1046/j.1460-2695.1999.00210.x ↗
13. High temperature crack annealing effects on fracture toughness of alumina and alumina‐SiC composite
14. 10.1111/j.1151-2916.1987.tb05716.x10.1111/j.1151-2916.1987.tb05716.x ↗
15. 10.1111/j.1151-2916.1990.tb06558.x10.1111/j.1151-2916.1990.tb06558.x ↗
16. 10.1111/j.1151-2916.1998.tb02558.x10.1111/j.1151-2916.1998.tb02558.x ↗
17. 10.1111/j.1151-2916.1970.tb12104.x10.1111/j.1151-2916.1970.tb12104.x ↗
18. 10.1111/j.1151-2916.1990.tb06583.x10.1111/j.1151-2916.1990.tb06583.x ↗
19. 10.1111/j.1151-2916.1998.tb02562.x10.1111/j.1151-2916.1998.tb02562.x ↗
20. 10.1111/j.1151-2916.1987.tb05017.x10.1111/j.1151-2916.1987.tb05017.x ↗
21. 10.1111/j.1151-2916.1990.tb05150.x10.1111/j.1151-2916.1990.tb05150.x ↗
22. 10.1016/0921-5093(94)06515-210.1016/0921-5093(94)06515-2 ↗
23. 10.1007/BF0068842910.1007/BF00688429 ↗
24. 10.1111/j.1151-2916.1981.tb10321.x10.1111/j.1151-2916.1981.tb10321.x ↗
25. 10.1111/j.1151-2916.1992.tb05550.x10.1111/j.1151-2916.1992.tb05550.x ↗
26. 10.1111/j.1151-2916.1996.tb07883.x10.1111/j.1151-2916.1996.tb07883.x ↗
27. 10.1111/j.1151-2916.1992.tb05439.x10.1111/j.1151-2916.1992.tb05439.x ↗
28. 10.1007/BF0054291510.1007/BF00542915 ↗
29. 10.1007/BF0054081610.1007/BF00540816 ↗
30. 10.1111/j.1151-2916.1970.tb12148.x10.1111/j.1151-2916.1970.tb12148.x ↗
31. 10.1016/0001-6160(77)90179-110.1016/0001-6160(77)90179-1 ↗
32. 10.1111/j.1151-2916.1992.tb05610.x10.1111/j.1151-2916.1992.tb05610.x ↗
33. 10.1111/j.1151-2916.1993.tb07758.x10.1111/j.1151-2916.1993.tb07758.x ↗