journal article·1997-12

AN ACCELERATED TEST METHOD FOR DETERMINING NEAR‐THRESHOLD STRESS INTENSITY VALUES IN HSLA STEELS

G. Liu‐Nash, J. A. Todd, S. Mostovoy

Publisher page

Abstract

Abstract— A new method for accelerating the collection of near‐threshold corrosion fatigue crack propagation data, using local hydrogen embrittlement in the crack tip region, has been investigated for ASTM A710 HSLA steel. Fatigue tests were conducted at 10 and 0.2 Hz (stress ratio, R= 0.1) on “constant K” contoured double cantilever beam (CDCB) specimens, to establish near‐threshold crack growth rates in a locally hydrogen charged region at the crack tip. Hydrogen charging was then discontinued and crack growth rates were monitored in the uncharged material. Near‐threshold fatigue crack growth rates were found to be 100 times faster in the locally hydrogen charged specimens than in the uncharged material. Fatigue thresholds, ΔKth, were defined in less than one fifth the time required for load shedding tests in air at 0.2 Hz. Although demonstrated for HSLA steels, the technique is applicable to any material which can be embrittled by hydrogen.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Fatigue and fracture mechanics · Non-Destructive Testing Techniques · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. 10.4043/1046-MS10.4043/1046-MS ↗
2. Cochera J. W. · 1969
3. Walter J. C. · 1976
4. 10.1179/msc.1977.11.8-9.30810.1179/msc.1977.11.8-9.308 ↗
5. C. E.Jaske D.Broek J. E.SlaterandW. E.Anderson(1978)Corrosion fatigue of structural steels in seawater and for offshore application.Corrosion Fatigue Technology ASTM STP 642 19–47.10.1520/STP28713S ↗
6. 10.1179/msc.1979.13.7.40210.1179/msc.1979.13.7.402 ↗
7. J. A.Todd P.Li G.LiuandV.Raman(1987)Microstructural studies of corrosion fatigue cracks in ASTM A710. In:Environmental Degradation of Engineering Materials III(Edited byM. R.Louthan R. P.McNittandR. D.Sisson Jr.) 533–541.
8. 10.1016/S0036-9748(88)80042-510.1016/S0036-9748(88)80042-5 ↗
9. 10.1016/0013-7944(89)90089-110.1016/0013-7944(89)90089-1 ↗
10. 10.1016/0167-8442(89)90040-210.1016/0167-8442(89)90040-2 ↗
11. Link L. R. · 1990 · 16
12. 10.1111/j.1460-2695.1990.tb00572.x10.1111/j.1460-2695.1990.tb00572.x ↗
13. 10.1520/STP24091S10.1520/STP24091S ↗
14. Chang R. W. · 419
15. Tubby P. T. · 1992 · 539
16. 10.1115/1.292010710.1115/1.2920107 ↗
17. 10.1115/1.292010210.1115/1.2920102 ↗
18. Todd J. A. · 1993 · 201
19. ASTM Standard E 647–91(1992)Annual Book of ASTM Standards Section 3 674–701.
20. Crosley P. B. · 1977 · 327
21. Use of crack‐line‐loaded specimens for measuring plane‐strain fracture toughness
22. G.Liu‐Nash R. P.FoleyandS.Mostovoy(Feb. 1997)Fatigue test compliance drop during the transition from a hydrogen rich to an air environment. Submitted toScripta Metall..