Microstructure-dependent hydrogen embrittlement of stainless steels for green hydrogen applications
Source abstract
Abstract
Abstract The storage and transportation of green hydrogen (GH 2 ) pose significant challenges for structural materials, particularly due to hydrogen embrittlement (HE), which can degrade the mechanical properties of steels through hydrogen–metal interactions. Understanding the susceptibility of candidate materials to hydrogen-induced damage is therefore essential for the safe deployment of hydrogen infrastructure. This study investigates the hydrogen embrittlement behavior of three stainless steels: ferritic stainless steel 410D, ferritic–martensitic stainless steel 410T, and duplex stainless steel 2205. Hydrogen was introduced through electrochemical charging via chronoamperometry in a 3.5 wt.% NaCl solution, a widely used laboratory approach to promote controlled hydrogen ingress and simulate hydrogen–material interactions relevant to hydrogen service conditions. The influence of charging temperature and exposure time was also evaluated. A comprehensive characterization methodology was employed, including microstructural analysis, chemical composition, hardness and microhardness measurements, uniaxial tensile tests before and after hydrogen exposure, and hydrogen permeation experiments to evaluate hydrogen absorption, diffusion, and transport behavior. The results indicate that hydrogen diffusivity plays a key role in the embrittlement response of the investigated alloys. The ferritic stainless steel 410D exhibited the highest susceptibility to hydrogen-induced degradation, showing the greatest reduction in mechanical properties and the highest hydrogen diffusion coefficient. In contrast, duplex stainless steel 2205 showed comparatively lower hydrogen diffusivity and reduced mechanical degradation under the tested conditions. Overall, the study highlights the critical influence of alloy microstructure, temperature, and exposure time on hydrogen embrittlement behavior and provides a comparative ranking of steel resistance to hydrogen-induced damage under the conditions analyzed.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. ABNT: NBR ISO 6892-1: Materiais metálicos — Ensaio de tração — Parte 1: Método de ensaio em temperatura ambiente (2024)
2. Arniella, V., Álvarez, G., Belzunce, J., Rodríguez, C.: Hydrogen embrittlement of 2205 duplex stainless Steel in in-situ tensile tests. Theor. Appl. Fract. Mech. 124, 103794 (2023). https://doi.org/10.1016/j.tafmec.2023.10379410.1016/j.tafmec.2023.103794 ↗
3. Arora, A., Singh, H., Mahajan, D.K.: Towards the prediction of intergranular fatigue crack initiation in metals due to hydrogen. Mater. Sci. Eng. A 787, 139488 (2020). https://doi.org/10.1016/j.msea.2020.13948810.1016/j.msea.2020.139488 ↗
4. ASTM International: Practice for evaluation of hydrogen uptake, permeation, and transport in metals by an electrochemical technique. (ASTM G148-97R18) (2018). https://doi.org/10.1520/G0148-97R1810.1520/G0148-97R18 ↗
5. ASTM International: Test methods and definitions for mechanical testing of Steel products (ASTM A370-24a) (2024a) https://doi.org/10.1520/A0370-24A10.1520/A0370-24A ↗
6. ASTM International: Test methods for tension testing of metallic materials (ASTM E8/E8M-24) (2024b). https://doi.org/10.1520/E0008_E0008M-2410.1520/E0008_E0008M-24 ↗
7. Bevitori, A.: Influência da pré-deformação plástica na microestrutura e propriedades de um aço inoxidável superduplex. Master’s thesis, Universidade Estadual do Norte Fluminense. (2010). https://uenf.br/posgraduacao/engenharia-demateriais/wp-content/uploads/sites/2/2013/07/Dissertação-Alice-B.-Bevitori1.pdf
8. Calegaro, A.B., De, A., De, F.: Trabalho de conclusão de curso em Engenharia Mecânica. Universidade Federal de Juiz de Fora (2018). https://www2.ufjf.br/mecanica//files/2009/06/UFJF_2018_TCC_Ana-Beatriz-Calegaro.pdf
9. Campari, A., Ustolin, F., Alvaro, A., Paltrinieri, N.: A review on hydrogen embrittlement and risk-based inspection of hydrogen technologies. Int. J. Hydrog. Energy 48(90), 35316–35346 (2023). https://doi.org/10.1016/j.ijhydene.2023.05.29310.1016/j.ijhydene.2023.05.293 ↗
10. Chen, Y.S., Huang, C., Liu, P.Y., Yen, H.W., Niu, R., Burr, P., Moore, K.L., Martínez-Pañeda, E., Atrens, A., Cairney, J.M.: Hydrogen trapping and embrittlement in metals – a review. Int. J. Hydrog. Energy 136, 789–821 (2025). https://doi.org/10.1016/j.ijhydene.2024.04.07610.1016/j.ijhydene.2024.04.076 ↗
11. De Abreu, E.: Corrosão em armaduras de tração de dutos flexíveis em diferentes pressões parciais de H2S. Master’s thesis, Programa de Pós-Graduação em Engenharia e Tecnologia de Materiais. (2021)
12. De Oliveira, L.: Estudo da permeação do hidrogênio no aço 1%Cr-0, 5%Mo em diferentes soluções eletrolíticas. Master’s thesis, Universidade Federal do Rio de Janeiro (2013). https://pantheon.ufrj.br/bitstream/11422/9716/1/monopoli10007235.pdf
13. Djukic, M.B., et al.: The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion. Eng. Fract. Mech. 216, 106528 (2019). https://doi.org/10.1016/j.engfracmech.2019.10652810.1016/j.engfracmech.2019.106528 ↗
14. Filgueiras, B.: Estudo da difusibilidade e solubilidade do hidrogênio no aço inoxidável bifásico martensítico-ferrítico. Master’s thesis, Universidade Federal do Rio de Janeiro (2019). https://pantheon.ufrj.br/bitstream/11422/13542/1/BeatrizAkelFilgueiras-min.pdf
15. Fukai, Y.: From metal hydrides to the metal–hydrogen system. J. Less-Common Met. 172–174, 8–17 (1991)10.1016/0022-5088(91)90427-6 ↗
16. Garcia, D.: Estudo da correlação entre corrosão sob tensão e permeação de hidrogênio em aço carbono utilizando técnicas eletroquímicas para verificação da influência do meio H2S no aço utilizado. Master’s thesis, Universidade Federal de Minas Gerais (2012) https://repositorio.ufmg.br/items/b5506d84-3559-4402-a93a-10b36b328439
17. Hagen, A.B., Nyhus, B., Gerhardt, M., Musinoi Hagen, C.H.M.: Experimental determination of equivalent hydrogen gas pressure from electrochemical hydrogen charging. Int. J. Hydrog. Energy 82, 1146–1156 (2024). https://doi.org/10.1016/j.ijhydene.2024.02.11710.1016/j.ijhydene.2024.02.117 ↗
18. Hoschke, J., Roethig, M., Tapia-Bastidas, C.V., Chowdhury, M.F.W., Venezuela, J., Shu, Y., Gray, E., Atrens, A.: Determination of the hydrogen fugacity during cathodic hydrogen charging of X65 D pipeline Steel. Corros. Sci. 243, 112580 (2025). https://doi.org/10.1016/j.corsci.2024.11258010.1016/j.corsci.2024.112580 ↗
19. ISO: Method of measurement of hydrogen permeation and determination of hydrogen uptake and transport in metals by an electrochemical technique (ISO 17081) (2014). https://www.iso.org
20. Jack, T.A., Fazeli, F., Szpunar, J.A.: Equivalence of hydrogen uptake in X70 pipeline Steel via gaseous and electrochemical charging. Int. J. Hydrog. Energy 123, 150–161 (2025). https://doi.org/10.1016/j.ijhydene.2025.03.39810.1016/j.ijhydene.2025.03.398 ↗
21. Jia, G., Lei, M., Li, M., Xu, W., Li, R., Lu, Y., Cai, M.: Hydrogen embrittlement in hydrogen-blended natural gas transportation systems: a review. Int. J. Hydrog. Energy 48(82), 32137–32157 (2023). https://doi.org/10.1016/j.ijhydene.2023.04.26610.1016/j.ijhydene.2023.04.266 ↗
22. Kazum, O., Bobby Kannan, M.: Effect of cathodic hydrogen-charging current density on the hydrogen diffusivity in nanostructured bainitic steels. Mater. Sci. Technol. 33(13), 1548–1552 (2017). https://doi.org/10.1080/02670836.2017.134294410.1080/02670836.2017.1342944 ↗
23. Kniep, D., Schewe, S., Rudolphi, M., Galetz, M.C.: Hydrogen permeation and embrittlement behavior of ferritic SOEC/SOFC interconnect candidates. Int. J. Hydrog. Energy 136, 0360-3199 (2025). https://doi.org/10.1016/j.ijhydene.2024.03.33710.1016/j.ijhydene.2024.03.337 ↗
24. Koren, E., Hagen, C.H.M., Wang, D., Johnsen, R., Yamabe, J.: Experimental comparison of gaseous and electrochemical hydrogen charging in X65 pipeline Steel using the permeation technique. Corros. Sci. 215, 111025 (2023). https://doi.org/10.1016/j.corsci.2023.11102510.1016/j.corsci.2023.111025 ↗
25. Liu, Q., Atrens, A.D., Shi, Z., Verbeken, K., Atrens, A.: Determination of the hydrogen fugacity during electrolytic charging of Steel. Corros. Sci. 87, 239–258 (2014). https://doi.org/10.1016/j.corsci.2014.06.03310.1016/j.corsci.2014.06.033 ↗
26. Martin, M.L., Dadfarnia, M., Nagao, A., Wang, S., Sofronis, P.: Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials. Acta Mater. 165, 734–750 (2019). https://doi.org/10.1016/j.actamat.2018.12.01410.1016/j.actamat.2018.12.014 ↗
27. Martin, M.L., Connolly, M.J., Delrio, F.W., Slifka, A.J.: Hydrogen embrittlement in ferritic steels. Appl. Phys. Rev. 7(4), 041406 (2020). https://doi.org/10.1063/5.001285110.1063/5.0012851 ↗
28. Molter, D.: Estudo da fragilização por hidrogênio de um aço inoxidável supermartensítico através da teoria da redução da energia interfacial. Master’s thesis, Universidade Federal do Rio de Janeiro (2017). https://pantheon.ufrj.br/bitstream/11422/6495/1/871949.pdf
29. Olden, V., Thaulow, C., Johnsen, R.: Modelling of hydrogen diffusion and hydrogen induced cracking in supermartensitic and duplex stainless steels. Mater. Des. 29(10), 1934–1948 (2008). https://doi.org/10.1016/j.matdes.2008.04.02610.1016/j.matdes.2008.04.026 ↗
30. Pu, S.D., Turk, A., Lenka, S., Ooi, S.W.: Study of hydrogen release resulting from the transformation of austenite into martensite. Mater. Sci. Eng. A 754, 628–635 (2019). https://doi.org/10.1016/j.msea.2019.03.09810.1016/j.msea.2019.03.098 ↗
31. Resende, M.: Efeito do carregamento de hidrogênio no comportamento eletroquímico de diferentes aços de alta resistência e baixa liga (ARBL) e da superliga INCONEL 718. (UNS N07718). Master’s thesis, Universidade Federal de Uberlândia (2021)
32. Shin, D.H., Hwang, H.K., Kim, S.J.: Effect of plasma ion nitriding on hydrogen embrittlement and wear resistance of martensitic stainless Steel for hydrogen valve core of fuel cell electric vehicles. Eng. Fract. Mech. 306, 110247 (2024). https://doi.org/10.1016/j.engfracmech.2024.11024710.1016/j.engfracmech.2024.110247 ↗
33. Valverde-González, A., Martínez-Pañeda, E., Quintanas-Corominas, A., Reinoso, J., Paggi, M.: Computational modelling of hydrogen assisted fracture in polycrystalline materials. Int. J. Hydrog. Energy 47(75), 32235–32251 (2022). https://doi.org/10.1016/j.ijhydene.2022.07.11710.1016/j.ijhydene.2022.07.117 ↗
34. Wu, L.K., Bao, Y.T., Jiang, M.Y., Sun, Q.Q., Cao, F.H.: Insights into the surface pretreatment on the oxidation behavior of anodized TiAl alloy. Corros. Sci. 207, 110571 (2022). https://doi.org/10.1016/j.corsci.2022.11057110.1016/j.corsci.2022.110571 ↗
35. Wu, W., Fu, H., Zhang, X., Li, W., Liu, S., Li, J.: Effect of anisotropy and slip transfer on hydrogen-assisted cracking of a 2205 duplex stainless Steel: a critical analysis. Corros. Sci. 213, 110988 (2023). https://doi.org/10.1016/j.corsci.2023.11098810.1016/j.corsci.2023.110988 ↗
36. Yu, H., Díaz, A., Lu, X., Sun, B., Ding, Y., Koyama, M., He, J., Zhou, X., Oudriss, A., Feaugas, X., Zhang, Z.: Hydrogen embrittlement as a conspicuous material challenge—comprehensive review and future directions. Chem. Rev. 124(10), 6271–6392 (2024). https://doi.org/10.1021/acs.chemrev.3c0062410.1021/acs.chemrev.3c00624 ↗