journal article·2018-02-17

Impedance and electromechancial studies on Ca0.1Sr0.9LaxBi2-xTa2O9 ceramics

Rizwana, Syed Mahboob, P. Sarah

Ferroelectrics· Volume 524· Issue 1
Publisher page

Abstract

Ca0.1Sr0.9LaxBi2-xTa2O9 ceramics were synthesized through solid state double sintering route. Impedance, resonance and anti-resonance studies under clamped state were carried out on the prepared ceramics. The activation energy for relaxation is within the range 0.850–1.230 eV depending up on composition x. Equivalent circuit modelling was done to the experimental Cole-Cole data so as to obtain the grain, grain boundary resistance and capacitance. The activation energy for grain conduction increased with the increase of x value except for x = 0.05 ceramic composition. The activation energy for grain boundary conduction is lower for the ceramic compositions with lanthanum doped when compared to pure CSBT ceramic. The activation energy for grain and grain boundary conduction are within the range 0.748–1.338 eV depending up on composition x and temperature. The electromechanical coupling factors are above 0.9990 and vary in fourth decimal place with the increase of temperature and composition x. The electromechanical coupling factor decreased with the increase of x value.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Dielectric properties of ceramics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Aeronautical Engineering, Dundigal, Hyderabad

Department of Physics, MRL, Osmania University, Hyderabad, A.P., India

Vardhaman College of Engineering, Kacharam, Shamshabad, A.P., India

Funding

National Natural Science Foundation of China · Post-gradute's Innovation Fund Project of Hebei Univeristy · Natural Science Foundation of Hebei Province

References (23)

Show source-provided references
1. Aurivillius B. · ArkivKemi1. · 1949 · 54 · 463
2. Aurivillius B. · ArkivKemi1. · 1949 · 58 · 499
3. Aurivillius B. · ArkivKemi2. · 1950 · 37 · 39
4. 10.1016/S0025-5408(98)00072-510.1016/S0025-5408(98)00072-5 ↗
5. 10.1063/1.33319810.1063/1.333198 ↗
6. 10.1080/0015019960821340810.1080/00150199608213408 ↗
7. 10.1080/0015019980801822410.1080/00150199808018224 ↗
8. 10.1111/j.1151-2916.1996.tb08086.x10.1111/j.1151-2916.1996.tb08086.x ↗
9. 10.1063/1.36330110.1063/1.363301 ↗
10. Aucellio O. · Phys. Today. · 1998 · 51 · 2
11. 10.1063/1.37130410.1063/1.371304 ↗
12. 10.1103/PhysRevB.61.655910.1103/PhysRevB.61.6559 ↗
13. 10.1080/1058458060065949810.1080/10584580600659498 ↗
14. 10.1016/j.physb.2012.09.02410.1016/j.physb.2012.09.024 ↗
15. 10.1016/j.materresbull.2012.12.04910.1016/j.materresbull.2012.12.049 ↗
16. 10.1016/j.ceramint.2013.05.05610.1016/j.ceramint.2013.05.056 ↗
17. 10.1080/00150193.2013.82192910.1080/00150193.2013.821929 ↗
18. 10.1080/00150193.2016.113402710.1080/00150193.2016.1134027 ↗
19. 10.1080/00150193.2014.93261110.1080/00150193.2014.932611 ↗
20. 10.1080/00150193.2015.110092210.1080/00150193.2015.1100922 ↗
21. 10.1080/00150193.2017.132777910.1080/00150193.2017.1327779 ↗
22. 10.1002/crat.20061089110.1002/crat.200610891 ↗
23. ANSI/IEEE Standards on Piezoelectricity. · 1987 · 176 · 51