Stress corrosion cracking of alloy 600 in an aqueous solution containing lead oxide

Dong-Jin Kim, Hong Pyo Kim, Seong Sik Hwang, Joung Soo Kim, Jangyul Park

Publisher page

Abstract

The stress corrosion cracking (SCC) behavior of Alloy 600 was studied in aqueous solutions containing lead. Electrochemical polarization and current transient experiments were performed at 315 °C in a 40% sodium hydroxide solution to assess the effect of lead on a passive film formed on Alloy 600. The influences of the alloy microstructure and the addition of an inhibitor to the environments on lead-induced SCC were investigated using C-ring and slow strain-rate tensile (SSRT) tests in demineralized high-purity water and caustic solutions containing PbO at 315 °C. The surface films on Alloy 600 were examined using Auger electron spectroscopy (AES) and energy dispersive x-ray spectroscopy (EDXS). The PbO markedly accelerated SCC of Alloy 600 in the caustic solution and the high-purity water at 315 °C. The addition of nickel boride (NiB) or cerium boride (CeB6) to the test solutions decreased the susceptibility of Alloy 600 to SCC. Thermally treated Alloy 600 (Alloy 600 TT) tended to crack in a transgranular mode, while the solution-annealed Alloy 600 (Alloy 600 SA) tended to crack in an intergranular mode in water containing PbO.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. H. Coriou, L. Grall, Y. Legall, and S. Vettier, Third Metallurgy Symposium on Corrosion, North Holland Publishing Co., Amsterdam (1960).
2. D. R. Diercks, W. J. Shack, and J. Muscara, Nucl. Eng. Design. 194, 19 (1999).10.1016/S0029-5493(99)00167-3 ↗
3. R. W. Staehle, Proc. 11 th International Symposium on Environmental Degradation of Metals in Nuclear Power Systems-Water Reactors, p. 381, Stevenson, Washington (2003).
4. D.-J. Kim, H. C. Kwon, M. A. Kim, J. S. Kim, S. S. Hwang, J. Park, and H. P. Kim, Proc. EUROCORR 2008, p. 257, Edinburgh, England (2008).
5. P. M. Scott and P. Combrade, Proc. 8th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems — Water Reactors, p. 65, Amelia Island, Florida (1997).
6. Y. S. Yi, S. H. Eom, H. P. Kim, and J. S. Kim, J. Nucl. Mat. 347, 151 (2005).10.1016/j.jnucmat.2005.08.011 ↗
7. J. Lumsden and G. Pollock, Workshop on Effects of Pb and S on the Performance of Secondary Side Tubing of Steam Generators in PWRs, ANL, Illinois (2005).
8. T. P. Moffat and R. M. Latanision, J. Electrochem. Soc. 139, 1869 (1992).10.1149/1.2069514 ↗
9. D.-J. Kim, H.C. Kwon, and H. P. Kim, Corros. Sci. 50, 1221 (2008).10.1016/j.corsci.2008.01.008 ↗
10. B. P. Miglin and J. M. Sarver, EPRI report, NP-7367-S, Palo Alto (1991).
11. D.-J. Kim, Y. S. Lim, H. C. Kwon, S. S. Hwang and H. P. Kim, J. Nanosci. Nanotech 10, 85 (2010).10.1166/jnn.2010.1530 ↗
12. M. Helie, Proc. 6th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems — Water Reactors, p. 179, San Diego, CA (1993).
13. T. Sakai, K. Aoki, T. Shigemitsu, and Y. Kishi, Corrosion 48, 734 (1992).10.5006/1.3315995 ↗
14. H. Takamatsu, T. Matsunaga, B. P. Miglin, J. M. Sarver, P. A. Sherburne, K. Aoki, and T. Sakai, Proc. 8th International Symposium on Environmental Degradation of Metals in Nuclear Power Systems-Water Reactors, p. 216, Amelia Island, Florida (1997).
15. Y. S. Lim, J. S. Kim, H. P. Kim, and H. D. Cho, J. Nucl. Mater. 335, 108 (2004).10.1016/j.jnucmat.2004.07.038 ↗
16. S. S. Hwang, H. P. Kim, Y. S. Lim, J. S. Kim, and L. Thomas, Corros. Sci. 49, 3797 (2007).10.1016/j.corsci.2007.03.040 ↗
17. D. H. Hur, J. S. Kim, J. S. Baek, and J. G. Kim, Corrosion 58, 1031 (2002).10.5006/1.3280792 ↗
18. S. S. Hwang, U. C. Kim, and Y. S. Park, J. Nucl. Mater. 246, 77 (1997).10.1016/S0022-3115(97)00023-8 ↗