Role of Subordinate Phases on the Dry Impact-Abrasion Behavior of Low Chromium Cast Iron
Source abstract
Abstract
In order to study the resistance mechanism of materials having high resistance to impact-abrasion, synergistic effect of subordinate phases of 2.20 wt%C–3.45 wt%Cr–3.06 wt%Mn–1.32 wt%Si–0.51 wt%Cu–0.31 wt%Ni–0.002 wt%B cast iron was investigated under dry impact-abrasion. Subordinate phases consist of graphite, secondary precipitates and retained austenite. Results show that the synergistic effect of above subordinate phases can prevent matrix and carbide from peeling off, and minimize the damage of carbide to matrix. This effect reduces the depth and width of groove from 7 to 1.2 μm and from 14 to 2.5 μm respectively. Above significant improvement is owing that: (1) Graphite can disperse external/internal stress, and fill carbide peeling pits. (2) Secondary precipitates, such as [Fe, Ni] and [Cr, Ni], can disperse the concentrated stress of carbide, inhibiting peeling. (3) Retained austenite can disperse the internal concentrated stress which is transferred from the carbide and fine precipitates to matrix.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Surface Treatment and Residual Stress
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Y. Li, R. Song, Z. Zhao, Yu. Pei, Transition region It is crucial to study the failure of 2.86 wt%Cr–Si–Mn–Cu iron alloy under impact wear. Vacuum 160, 429–433 (2019)10.1016/j.vacuum.2018.11.060 ↗
2. J.J. Coronado, Effect of (Fe, Cr)7C3 carbide orientation on abrasion wear resistance and fracture toughness. Wear 270, 287–293 (2011)10.1016/j.wear.2010.10.070 ↗
3. Y. Li, R. Song, Z. Zhao, Yu. Pei, Internal cracking with crystal lattice failure of 2.93 wt%Cr–Mn–Cu–Si iron under impact-abrasion. Vacuum 164, 219–223 (2019)10.1016/j.vacuum.2019.03.028 ↗
4. I.I. Tsypin, V.I. Kantorovich, A.D. Zuev, V.A. Gold’shtein, Influence of M7C3 carbides orientation on the wear resistance of 300Kh20DNF white iron. Met. Sci. Heat Treat. 33, 759–761 (1991)10.1007/BF00800696 ↗
5. O.N. Dogan, G. Laird II, J.A. Hawk, Abrasion resistance of the columnar. Wear 181–183, 342–349 (1995)10.1016/0043-1648(94)07056-3 ↗
6. H.G. Fu, Q. Xiao, J.C. Kuang, Z.Q. Jiang, J.D. Xing, Effect of rare earth and titanium additions on the microstructures and properties of low carbon Fe–B cast steel. Mater. Sci. Eng. A 466, 160–165 (2007)10.1016/j.msea.2007.02.032 ↗
7. C. Scandian, C. Boher, J.D.B. de Mello, F. Rézaï-Aria, Effect of molybdenum and chromium contents in sliding wear of high-chromium white cast iron: the relationship between microstructure and wear. Wear 267, 401–408 (2009)10.1016/j.wear.2008.12.095 ↗
8. S.Q. Ma, J.D. Xing, H.G. Fu, Y.M. Gao, J.J. Zhang, Microstructure and crystallography of borides and secondary precipitation in 18 wt%Cr–4 wt%Ni–1 wt%Mo–3.5 wt%B–0.27 wt%C steel. Acta Mater 60, 831–843 (2012)10.1016/j.actamat.2011.11.004 ↗
9. Y. Li, R. Song, Z. Zhao, Yu. Pei, Effect of three-staged normalizing on the impact wear resistance of 3.23 mass% Cr–Mn–Cu–Si cast iron. Wear 426–427, 59–67 (2019)10.1016/j.wear.2019.01.004 ↗
10. M. Radulovic, M. Fiset, K. Peev, M. Tomovic, The influence of vanadium on fracture toughness and abrasion resistance in high chromium white cast irons. J. Mater. Sci. 29, 5085–5094 (1994)10.1007/BF01151101 ↗
11. D. Yi, J. Xing, S. Ma, H. Fu, Y. Li, W. Chen, J. Yan, J. Zhang, R. Zhang, Investigations on microstructures and two-body abrasive wear behavior of Fe–B cast alloy. Tribol. Lett. 45, 427–435 (2012)10.1007/s11249-011-9900-9 ↗
12. X. Zhi, J. Xing, Y. Gao, H. Fu, J. Peng, B. Xiao, Effect of heat treatment on microstructure and mechanical properties of a Ti-bearing hypereutectic high chromium white cast iron. Mater. Sci. Eng. A 487, 171–179 (2008)10.1016/j.msea.2007.10.009 ↗
13. S.M. Lee, B.H. Kim, J.S. Shin et al., Optimization of heat treatment parameters of Mo-free high Cr-cast iron mill balls. Adv. Mater. Res. 913, 26–28 (2007)
14. W. Wang, R. Song et al., Multiphase steel with improved impact-abrasive wear resistance in comparison with conventional Hadfield steel. Mater. Des. 105, 96–105 (2016)10.1016/j.matdes.2016.05.056 ↗
15. Z. Pei, R. Song et al., Dimensionality wear analysis: three-body impact abrasive wear behavior of a martensitic steel in comparison with Mn13Cr2. Wear 414–415, 341–351 (2018)10.1016/j.wear.2018.09.002 ↗
16. S.-g. Peng, R.-b. Song et al., Surface failure behavior of 70Mn martensite steel under abrasive impact wear. Wear 362–363, 129–134 (2016)10.1016/j.wear.2016.05.019 ↗
17. J. Liu, S. Li, Y. Man, Wear resistance of Ni-hard 4 and high-chromium cast iron reevaluated. Wear 166, 37–40 (1993)10.1016/0043-1648(93)90254-J ↗
18. S.Q. Ma, J.D. Xing, H.G. Fu, D.W. Yi, J.J. Zhang, Y.F. Li, Z.Y. Zhang, B.J. Zhu, S.C. Ma, Interfacial morphology and corrosion resistance of Fe–B cast steel containing chromium and nickel in liquid zinc. Corros. Sci. 53, 2826–2834 (2011)10.1016/j.corsci.2011.05.020 ↗
19. H.G. Fu, S.Q. Ma, J.Q. Hou, Y.P. Lei, J.D. Xing, Microstructure and properties of cast B-bearing high speed steel. J. Mater. Eng. Perform. 22, 1194–1200 (2013)10.1007/s11665-012-0378-x ↗
20. Y.X. Jian, Z.F. Huang, J.D. Xing, B.C. Zheng, L. Sun, Y.Z. Liu, Y.M. Liu, Effect of improving Fe2B toughness by chromium addition on the two-body abrasive wear behavior of Fe–3.0 wt%B cast alloy. Tribol. Int 101, 331–339 (2016)10.1016/j.triboint.2016.05.009 ↗
21. E. Albertin, A. Sinatora, Effect of carbide fraction and matrix microstructure on the wear of cast iron balls tested in laboratory ball mill. Wear 250, 492–501 (2001)10.1016/S0043-1648(01)00664-0 ↗
22. M. Hatate, T. Shiota, N. Takahashi, K. Shimizu, Influences of graphite shapes on wear characteristics of austempered cast iron. Wear 251(1–12), 885–889 (2001)10.1016/S0043-1648(01)00746-3 ↗
23. M. Pawlyta, J.-N. Rouzaud, S. Duber, Raman microspectroscopy characterization of carbon blacks: spectral analysis and structural information. Carbon 84, 479–490 (2015)10.1016/j.carbon.2014.12.030 ↗
24. A. Inam, R. Brydson, D.V. Edmonds, Effect of starting microstructure upon the nucleation sites and distribution of graphite particles during a graphitizing anneal of an experimental medium-carbon machining steel. Mater. Charact. 106, 86–92 (2015)10.1016/j.matchar.2015.05.014 ↗
25. J.X. Gao, B.Q. Wei, D.D. Li, K. He, Nucleation and growth characteristics of graphite spheroids in bainite during graphitization annealing of a medium carbon steel. Mater. Charact. 118, 1–8 (2016)10.1016/j.matchar.2016.05.003 ↗
26. B. Miao, K. Fang, W. Bian, G. Liu, On the microstructure of graphite spherulites in cast irons by TEM and HREM. Acta Metall. Mater. 38(11), 2167–2174 (1990)10.1016/0956-7151(90)90084-T ↗
27. P. Dierickx, C. Verdu, A. Reynaud, R. Fougeres, A study of physico-chemical mechanisms responsible for damage of heat-treated and as-cast ferritic spheroidal graphite cast irons. Scr. Mater 34(2), 261–268 (1996)10.1016/1359-6462(95)00496-3 ↗
28. S. Terpilowska, Andrzej Krzysztof Siwicki, Interactions between chromium (III) and iron (III), molybdenum (III) or nickel (II): cytotoxicity, genotoxicity and mutagenicity studies. Chemosphere 201, 780–789 (2018)10.1016/j.chemosphere.2018.03.062 ↗
29. J. Tian, T. Zheng, J. Yang, S. Kong, J. Xue, Y. Wang, K. Nordlund, Capacity of graphite’s layered structure to suppress the sputtering yield: a molecular dynamics study. Appl. Surf. Sci. 337, 6–11 (2015)10.1016/j.apsusc.2015.01.241 ↗
30. L. Lundin, B. Richarz, Atom-probe study of phosphorus segregation to the carbide/matrix interface in an aged 9% chromium steel. Appl. Surf. Sci. 87–88, 194–199 (1995)10.1016/0169-4332(94)00519-2 ↗