Effect of heat treatment on the properties of electroless Ni–P–carbon nanotube composite coatings
Source abstract
Abstract
Electroless Ni–P–carbon nanotube composite coatings were deposited on API-5L X65 steel substrates. The coatings were vacuum heat treated at temperatures of 200°C for 2 h, 400°C for 1 h and 600°C for 15 min. Microhardness measurement, X-ray diffraction (XRD) technique, scanning electron microscopy, potentiodynamic polarisation and electrochemical impedance spectroscopy (EIS) were used to study the effect of heat treatment on the properties of the coatings. XRD results indicated that the as-plated coating had either nanocrystalline or a mixture of amorphous and nanocrystalline structure. Heat treatment of the coatings above 400°C produced a mixture of polycrystalline phases. The highest microhardness was achieved for the samples heat treated at 600°C for 15 min because of the precipitation of NixPy phases and formation of an inter-diffusional layer at the substrate/coating interface. The lowest corrosion current density value was obtained for the coatings heat treated at 400°C for 1 h. EIS experiments confirmed the results.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Semiconductor materials and interfaces · Electrocatalysts for Energy Conversion
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Amir Abad Shomali, School of Metallurgy and Materials Engineering, University College of Engineering, University of Tehran, P.O. Box 11155-4563, Tehran, Iran
References (31)
Show source-provided references
1. 10.1023/A:102557241020510.1023/A:1025572410205 ↗
2. 10.1007/s11661-006-0134-710.1007/s11661-006-0134-7 ↗
3. 10.1016/j.triboint.2004.11.00810.1016/j.triboint.2004.11.008 ↗
4. 10.1016/S0167-577X(02)00968-010.1016/S0167-577X(02)00968-0 ↗
5. 10.1016/S0043-1648(03)00171-610.1016/S0043-1648(03)00171-6 ↗
6. 10.1016/j.diamond.2005.09.00410.1016/j.diamond.2005.09.004 ↗
7. 10.1016/j.triboint.2005.10.00110.1016/j.triboint.2005.10.001 ↗
8. 10.1016/S0043-1648(98)00389-510.1016/S0043-1648(98)00389-5 ↗
9. 10.1016/j.electacta.2004.04.02310.1016/j.electacta.2004.04.023 ↗
10. 10.1016/j.materresbull.2005.02.01510.1016/j.materresbull.2005.02.015 ↗
11. 10.1016/j.surfcoat.2005.03.00710.1016/j.surfcoat.2005.03.007 ↗
12. 10.1016/j.tsf.2004.02.01610.1016/j.tsf.2004.02.016 ↗
13. 10.1179/095066009X1257253017054310.1179/095066009X12572530170543 ↗
14. 10.1016/S0008-6223(02)00265-810.1016/S0008-6223(02)00265-8 ↗
15. 10.1016/S0257-8972(02)00408-510.1016/S0257-8972(02)00408-5 ↗
16. 10.1016/j.jallcom.2010.10.05710.1016/j.jallcom.2010.10.057 ↗
17. 10.1016/j.surfcoat.2004.04.05510.1016/j.surfcoat.2004.04.055 ↗
18. 10.1016/S0040-6090(99)00671-910.1016/S0040-6090(99)00671-9 ↗
19. 10.1016/j.surfcoat.2004.10.04510.1016/j.surfcoat.2004.10.045 ↗
20. 10.1016/j.matlet.2004.09.03210.1016/j.matlet.2004.09.032 ↗
21. 10.1016/S0257-8972(03)00746-110.1016/S0257-8972(03)00746-1 ↗
22. 10.1016/j.matdes.2010.02.02710.1016/j.matdes.2010.02.027 ↗
23. Mallory, G.O., and Hajdu, J.B.: ‘Electroless plating: fundamentals and applications’, (AESF 1990),reprint ed.
24. 10.1016/j.ijfatigue.2006.07.00410.1016/j.ijfatigue.2006.07.004 ↗
25. 10.1016/j.surfcoat.2006.01.00510.1016/j.surfcoat.2006.01.005 ↗
26. 10.1149/1.210901610.1149/1.2109016 ↗
27. 10.1149/1.209588010.1149/1.2095880 ↗
28. 10.1149/1.209546810.1149/1.2095468 ↗
29. 10.1016/0010-938X(89)90122-410.1016/0010-938X(89)90122-4 ↗
30. 10.1016/j.electacta.2006.07.00110.1016/j.electacta.2006.07.001 ↗
31. 10.5006/1.358530910.5006/1.3585309 ↗