Comparative study of the fire protection performance and thermal stability of intumescent fire‐retardant coatings filled with three types of clay nano‐fillers
Source abstract
Abstract
Summary The fire protection and thermal stability properties of intumescent fire‐retardant coatings filled with three various clay nano‐fillers (layer double hydroxide [LDH], montmorillonite [MMT], and sepiolite) were compared by fire protection tests and thermo‐gravimetric analysis. The fire protection tests show that the incorporation of three fillers improves the fire protection properties of the intumescent fire‐retardant coatings and the addition of 1 wt% sepiolite exhibits the lowest flame spread rating of 9.9 and equilibrium backside temperature of 164.5°C at 900 seconds. TG analysis shows that the incorporation of nano‐fillers imparts a considerable enhancement of thermal stability and char formation to the intumescent coatings. Especially, the coating with 1 wt% sepiolite acquires the highest residual weight of 34.2% among the samples. Char residue analysis presents that the introduction of clay nano‐fillers plays a positive role in enhancing the compactness and anti‐oxidation ability of the char residues, and this positive effect as well as the flame‐retardant efficiency depends on the types of clay nano‐fillers. The three types of layered clay nano‐fillers exhibit synergistic flame‐retardant effectiveness in the order of sepiolite > MMT > LDH.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Flame retardant materials and properties · Synthesis and properties of polymers · Layered Double Hydroxides Synthesis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Disaster Prevention Science and Safety Technology Central South University Changsha 410075 China
Funding
Open-End Fund for the Valuable and Precision Instruments of Central South University · Natural Science Foundation of Hunan Province · National Natural Science Foundation of China
References (25)
Show source-provided references
1. 10.1016/j.mser.2014.08.00110.1016/j.mser.2014.08.001 ↗
2. 10.1002/1099-1018(200007/08)24:4<201::AID-FAM739>3.0.CO;2-D10.1002/1099-1018(200007/08)24:4<201::AID-FAM739>3.0.CO;2-D ↗
3. 10.1002/fam.271210.1002/fam.2712 ↗
4. 10.1016/j.porgcoat.2018.05.01610.1016/j.porgcoat.2018.05.016 ↗
5. 10.1016/j.apsusc.2018.06.16510.1016/j.apsusc.2018.06.165 ↗
6. 10.1002/pc.2507710.1002/pc.25077 ↗
7. 10.1016/j.surfcoat.2013.11.03710.1016/j.surfcoat.2013.11.037 ↗
8. 10.1007/s11998-016-9815-310.1007/s11998-016-9815-3 ↗
9. 10.1002/fam.267010.1002/fam.2670 ↗
10. 10.1007/s11998-014-9626-310.1007/s11998-014-9626-3 ↗
11. 10.1016/j.polymdegradstab.2015.12.00410.1016/j.polymdegradstab.2015.12.004 ↗
12. 10.1007/s10973-017-6514-y10.1007/s10973-017-6514-y ↗
13. 10.1016/j.porgcoat.2018.02.00510.1016/j.porgcoat.2018.02.005 ↗
14. 10.1016/j.ssci.2018.08.01610.1016/j.ssci.2018.08.016 ↗
15. 10.1016/j.porgcoat.2005.01.00410.1016/j.porgcoat.2005.01.004 ↗
16. 10.1002/fam.112810.1002/fam.1128 ↗
17. 10.1021/ie101737n10.1021/ie101737n ↗
18. 10.1016/j.polymdegradstab.2012.05.02810.1016/j.polymdegradstab.2012.05.028 ↗
19. 10.1007/s10965-009-9317-410.1007/s10965-009-9317-4 ↗
20. 10.1002/polb.2095710.1002/polb.20957 ↗
21. Yang F · 2009 · 95
22. Kashiwagi T · 2005 · 81
23. 10.1007/s11998-013-9475-510.1007/s11998-013-9475-5 ↗
24. 10.1007/s11998-018-0069-010.1007/s11998-018-0069-0 ↗
25. 10.1016/j.porgcoat.2017.07.01710.1016/j.porgcoat.2017.07.017 ↗