journal article·2009-07

Experimental research on post-fire behaviour of reinforced concrete columns

Yih-Houng Chen, Yun-Fei Chang, George C. Yao, Maw-Shyong Sheu

Fire Safety Journal· Volume 44· Issue 5
Publisher page

Abstract

Abstract This paper reports an experimental research into the effect of fire exposure time on the post-fire behaviour of reinforced concrete columns. Nine full-size reinforced concrete columns (45×30×300 cm) with two longitudinal reinforcement ratios (1.4% and 2.3%) were unexposed and exposed to the ISO 834 standard fire for 2 and 4 h with a constant preload. One month after cooling, the specimens were tested in axial load combined with uniaxial or biaxial bending. The test results show that the residual load-bearing capacity decreases with increase in fire exposure time. This deterioration in strength following an increase in fire exposure time can be slowed down by the strength recovery of hot rolled reinforcing bars after cooling. In addition, the reduction in residual stiffness is higher than that in ultimate load; consequently, much attention should be given to the deformation and stress redistribution of the reinforced concrete building subject to earthquakes after a fire.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fire effects on concrete materials · Structural Behavior of Reinforced Concrete · Structural Response to Dynamic Loads

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Postfire full stress–strain response of fire-damaged concrete10.1002/fam.911 ↗
2. Residual stress–strain relationship for concrete after exposure to high temperatures10.1016/j.cemconres.2006.05.029 ↗
3. Strength and durability recovery of fire-damaged concrete after post-fire-curing10.1016/S0008-8846(01)00582-8 ↗
4. Mechanical properties of reinforcing and prestressing steels after heating10.1061/(ASCE)0899-1561(1996)8:4(189) ↗
5. Quenched reinforcement exposed to fire10.1680/macr.2006.58.1.43 ↗
6. C.Y. Xu, Bond deterioration of reinforcing bars and it's effect on the characteristics of beam-column connection after exposure to fire. Ph.D. Thesis, Department of Construction Engineering, National Taiwan University of Science and Technology, Taiwan, 1991.
7. Time-temperature analysis of bond strength of a rebar after fire exposure10.1016/S0008-8846(03)00139-X ↗
8. Effect of fire on flexural behaviour of RC beams10.1016/0950-0618(95)00041-0 ↗
9. Effect of fire on shear behaviour of RC beams10.1016/S0045-7949(95)00356-8 ↗
10. Residual strength of reinforced concrete members subjected to elevated temperatures10.1680/iicep.1982.1708 ↗
11. Deterioration of strength and stiffness of reinforced concrete columns after fire10.1080/02533839.1990.9677257 ↗
12. Lie · 1984
13. Strain of heated concrete during two thermal cycles. Part 1: strain over two cycles, during first heating and at subsequent constant temperature10.1680/macr.2006.58.6.367 ↗
14. Lie · 1985