Heating duration effects on post-fire structural steel mechanical properties
Source abstract
Abstract
Post-fire mechanical assessment of steel structures is challenging due to the changes in mechanical properties from the heating and cooling phases of a fire. While the effects of cooling rate and temperature of exposure have been researched in depth, the effects of heating duration are not comprehensive. This paper investigates the effects of heating duration on post-fire A572 Gr. 50 steel mechanical properties over a temperature range of 500–800 °C for durations of 0.5 and 2.0 h. Specimens are subjected to tensile testing in accordance with ASTM A370, Vickers microhardness testing, and optical microscopy. The findings suggest that heating duration has an influence on the post-fire mechanical properties of steel at elevated temperatures (700, 800 °C). At these temperature exposures, retention of yield stress, retention of ultimate stress, and microhardness all decrease. Members subjected to 700 °C for 0.5 h have more retention in yield stress and microhardness compared to those exposed for 2.0 h, while the 800 °C conditions show little difference in mechanical properties between exposure times. The results of this study show that the duration of fire exposure is an important factor when estimating the mechanical properties of fire-exposed steels, in addition to the temperature and cooling rate.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fire effects on concrete materials · Engineering and Material Science Research · Electrical Fault Detection and Protection
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. The natural fire safety concept - Full-scale tests at Cardington10.1016/S0379-7112(03)00028-6 ↗
2. Cen · 1993
3. 2016
4. Structural steel after a fire
5. Structural steel after a fire
6. Distortion control during welding of large structures
7. Integrity of structural steel after exposure to fire10.62913/engj.v35i1.691 ↗
8. 1989
9. Avent · 1991
10. Kirby · 1986
11. Smith · 1981
12. Mechanical properties of ASTM A992 steel after fire10.62913/engj.v49i1.1222 ↗
13. Experimental investigation of the residual mechanical properties of cast steels after exposure to elevated temperature10.1016/j.conbuildmat.2017.03.118 ↗
14. Microstructure–mechanical property relationships for post-fire structural steels10.1061/(ASCE)MT.1943-5533.0003190 ↗
15. Post-fire performance of structural steel10.24237/djes.2021.14203 ↗
16. 2022
17. Thermo-Calc & DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
18. Callister · 2010
19. 2022
20. Gordon · 2022
21. 2022
22. Tabor · 1951
23. 2017
24. Metallurgical characterization of coupled carbon diffusion and precipitation in dissimilar steel welds10.1007/s10853-016-9792-z ↗
25. Gosain · 2008