journal article·2018

Mechanical and Physical Properties of Oriented Strand Board Exposed to High Temperature and Relative Humidity and Coupled with Near-Infrared Reflectance Modeling

Qingzheng Cheng, Chengfeng Zhou, Wei Jiang, Xiping Zhao, Brian K. Via, Hui Wan

Forest Products Journal· Volume 68· Issue 1
Publisher page

Abstract

Abstract The mechanism underlying thermal degradation of oriented strand board was tested under a humid environment. Near-infrared reflectance (NIR) spectroscopy coupled with chemometric modeling was utilized to better understand the degradation of functional groups over time. The flexural properties, internal bond (IB), water absorption, and thickness swelling were tested after exposure to various times of 0, 3, 6, and 9 weeks in a climate-controlled laboratory to 76.7°C and 60 percent relative humidity. The largest reduction in all flexural and physical properties occurred during the first 3 weeks of exposure and then leveled off thereafter, while IB decreased significantly through the 9-week period (α = 0.05). Chemometric models built from NIR spectra revealed pertinent chemical changes in wood chemistry and resin components.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Natural Fiber Reinforced Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

The authors are, respectively, Research Fellow, Forest Products Development Center, Forest Products Lab., Auburn Univ., Auburn, Alabama (qzc0007@auburn.edu [corresponding author]); Lecturer and Associate Professor, Lab. of New Fiber Materials and Modern Textile, The Growing Base for State Key Lab., Qingdao Univ., Qingdao, People's Republic of China (chengfengzhou828@gmail.com, weijiangqd@gmail.com); Associate Professor, College of Forestry, Henan Univ. of Sci. and Technol., Luoyang...

References (26)

Show source-provided references
1. Aro, M., B. Brashaw, and P. Donahue. 2014. Mechanical and physical properties of thermally modified plywood and oriented strand board panels. Forest Prod. J. 64(7–8):281–289.
2. ASTM International. 2003. Standard test method for evaluating the flexural properties of fire-retardant treated softwood plywood exposed to elevated temperatures. ASTM D5516. ASTM International, West Conshohocken, Pennsylvania.
3. ASTM International. 2011. Standard test methods for structural panels in flexure. ASTM D3043. ASTM International, West Conshohocken, Pennsylvania.
4. ASTM International. 2012. Standard test methods for evaluating properties of wood-base fiber and particle panel materials. ASTM D1037. ASTM International, West Conshohocken, Pennsylvania.
5. Evans, P., M. Miesner, and D. Rogerson. 2013. Machined tapers reduce the differential edge swelling of oriented strand board exposed to water. Compos. Part B Eng. 50:15–21.
6. Forest Products Laboratory. 2010. Wood handbook—Wood as an engineering material. General Technical Report FPL-GTR-190. USDA Forest Service, Forest Products Laboratory, Madison, Wisconsin. 508pp.
7. Garay, R., H. Poblete, and J. Karsulovic. 2009. Evaluation of oriented strandboard and plywood subjected to severe relative humidity and temperature conditions. Forest Prod. J. 59(3):84–90.
8. Hein, P., A. Campos, R. Mendes, L. Mendes, and G. Chaix. 2011. Estimation of physical and mechanical properties of agro-based particleboards by near infrared spectroscopy. Eur. J. Wood Prod. 69(3):431–442.
9. Hiziroglu, S. 2008. Internal bond strength of laminated flooring as function of water exposure. Paper WS-26. In:Proceedings of the 2008 SWST International Annual Convention, November 10–12, 2008, Concepcion, Chile; Society of Wood Science and Technology, Madison, Wisconsin. 4 pp. ISBN #978‐0‐9817876‐0‐2.
10. Inoue, M., M. Norimoto, M. Tanahashi, and R. Rowell. 1993. Steam or heat fixation of compressed wood. Wood Fiber Sci. 25(3):224–235.
11. Kelley, S., T. Elder, and L. Groom. 2005. Changes in the chemical composition and spectroscopy of loblolly pine medium density fiberboard furnish as a function of age and refining pressure. Wood Fiber Sci. 37(1):14–22.
12. Kohan, N., B. Via, and S. Taylor. 2012. Prediction of strand feedstock mechanical properties with near infrared spectroscopy. BioResources7(3):2996–3007.
13. Kojima, Y. and S. Suzuki. 2011. Evaluation of wood-based panel durability using bending properties after accelerated aging treatments. J. Wood Sci. 57(2):126–133.
14. Meder, R., A. Thumm, and H. Bier. 2002. Veneer stiffness predicted by NIR spectroscopy calibrated using mini-LVL test panels. Eur. J. Wood Prod. 60(3):159–164.
15. Moya, L., W. Tze, and J. Winandy. 2009. The effect of cyclic relative humidity changes on moisture content and thickness swelling behavior of oriented strandboards. Wood Fiber Sci. 41(4):447–460.
16. So, C., B. Via, L. Groom, L. Schimleck, T. Shupe, S. Kelley, and T. Rials. 2004. Near infrared spectroscopy in the forest products industry. Forest Prod J. 54(3):6–16.
17. Via, B. 2010. Prediction of oriented strand board wood strand density by near infrared and Fourier transform infrared reflectance spectroscopy. J. Near Infrared Spec. 18(6):491–498.
18. Via, B. 2013. Characterization and evaluation of wood strand composite load capacity with near infrared spectroscopy. Mater. Struct. 46(11):1801–1810.
19. Via, B., O. Fasina, and H. Pan. 2011. Assessment of pine biomass density through mid-infrared spectroscopy and multivariate modeling. BioResources6(1):807–822.
20. Via, B., T. Shupe, L. Groom, M. Stine, and C. So. 2003. Multivariate modelling of density, strength and stiffness from near infrared spectra for mature, juvenile and pith wood of longleaf pine (Pinus palustris). J. Near Infrared Spec. 11(5):365–378.
21. Via, B., C. So, T. Shupe, L. Groom, and J. Wikaira. 2009. Mechanical response of longleaf pine to variation in microfibril angle, chemistry associated wavelengths, density, and radial position. Compos. Part A Appl. Sci. Manuf. 40(1):60–66.
22. Winandy, J. 2001. Thermal degradation of fire-retardant-treated wood: Predicting residual service life. Forest Prod. J. 51(2):47–54.
23. Wu, Q. and J. Lee. 2002. Thickness swelling of oriented strandboard under long-term cyclic humidity exposure condition. Wood Fiber Sci. 34(1):125–139.
24. Wu, Q. and C. Piao. 1999. Thickness swelling and its relationship to internal bond strength loss of commercial oriented strandboard. Forest Prod. J. 49(7–8):50–55.
25. Wu, Q. and O. Suchsland. 1997. Effect of moisture on the flexural properties of commercial oriented strandboards. Wood Fiber Sci. 29(1):47–57.
26. Xu, W., P. Winistorfer, and W. Moschler. 1996. A procedure to determine water absorption distribution in wood composite panels. Wood Fiber Sci. 28(3):286–294.