Abstract
Abstract Glued Laminated Timber, commonly referred to as Glulam, is an important structural wood product, suitable for use in exterior applications provided it is protected against decay by building design, natural durability, or treatment. Bonding treated lamina made from refractory species is challenging because resurfacing after treatment can remove much of the treated zone and create a waste disposal challenge. It was hypothesized that use of roll-pressing rather than resurfacing could address this. When an adhesive modifier was used to prevent the adverse effects of wood preservatives on adhesive bonding, treated lamina that were replaned before gluing had similar shear strength to untreated planed lamina. However, the treated lamina that were roll-pressed before gluing had lower shear strength than the replaned lamina. The consequence of this weakening was evident in an above-ground field test where delamination was observed in several test units after 12 years of exposure. Decay resistance was evaluated in above-ground, ground contact, and ground proximity tests. The decay resistance of treated glulam was high with only low levels of decay reported in all tests, while untreated controls showed advanced decay or failure. Yellow cedar glulam, included as a reference in the ground proximity test, showed moderate decay after 10 years of exposure.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Plant Pathogens and Fungal Diseases · Forest Ecology and Biodiversity Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. American Wood Council (AWC). 2018. National Design Specification (NDS) for Wood Construction. American Wood Council, Leesburg, Virginia.
2. American Wood Protection Association (AWPA). 2020 a. U1-20 Use category system: User specification for treated wood. American Wood Protection Association, Birmingham, Alabama.
3. American Wood Protection Association (AWPA). 2020 b. E32-18 Standard field test for evaluation of field-cut preservatives to be used above ground (UC3B): Modified post and rail test. American Wood Protection Association, Birmingham, Alabama.
4. American Wood Protection Association (AWPA). 2020 c. E7-15 Standard field test for evaluation of wood preservatives to be used in ground contact (UC4A, UC4B, UC4C); Stake test. American Wood Protection Association, Birmingham, Alabama.
5. APA – The Engineered Wood Association (APA). 2020. ANSI 117-2020 standard specification for structural glued laminated timber of softwood species. APA – The Engineered Wood Association, Tacoma, Washington.
6. ASTM International. 2005. D4761-05 Standard Test Methods for Mechanical Properties of Lumber and Wood-base Structural Material. ASTM International, West Conshohocken, Pennsylvania.
7. Bergman, Ö. and Jermer.J. 2010. Glued laminated poles—Progress report after 30 years testing. Document No. IRG/WP/10-20427. International Research Group on Wood Protection, Stockholm. 11pp.
8. CSA Group. 2006. Standard O177-06 Qualification Code for Manufacturers of Structural Glued-Laminated Timber. CSA Group, Toronto, Ontario, Canada.
9. CSA Group. 2015. Standard O80-15 Wood Preservation. CSA Group, Toronto, Ontario, Canada.
10. Cookson, L. J. 2013. Durability of light organic solvent preservative (LOSP) treatments for softwood glulam. Int. Biodeterior. Biodegrad. 80: 41– 47.
11. Cooper, P. and Morris.P. 2007. Challenges in treating Canadian species. Proc. Can. Wood Preserv. Assoc. 28: 9– 20.
12. Dias, A. M., Martins, C. E. and Dias.A. M. 2020. Influence of the treatment phase on the gluing performance of glued laminated timber. BioResources15(3): 5725– 5736.
13. Feng, M. W., Andersen, A. and Morris.P. 2008. Method for Producing Wood Composite Products with Phenolic Resins and Borate-Treated Wood Materials. Canadian Patent # CA 2,429,914C.
14. Feng, M. W. and Knudson.R. M. 2006. Gluing of B.C. wood species treated with new preservative systems. Report prepared for B.C. Forestry Innovation Investment, Vancouver.
15. Gaspar, F., Cruz, H. Gomes, A. and Nunes.L. 2010. Production of glued laminated timber with copper azole treated maritime pine. Eur. J. Wood Wood Prod. 68(2): 207– 218.
16. Henrique de Almeida, D., Cavalheiro, R. S. Borges de Macêdo, L. Neto, C. C. Christoforo, A. L. Calil, C. Jr., and Lahr.F. A. R. 2014. Evaluation of quality in the adhesion of glued laminated timber (glulam) of paricá and lyptus wood species. Int. J. Mater. Eng. 4(3): 114– 118.
17. Knudson, R. M., Feng, M. W. and Morris.P. I. 2008. Manufacture and testing of glulam made from MPB laminating stock treated with copper-cobiocide. Report prepared for B.C. Forestry Innovation Investment, Vancouver.
18. Kržišnik, D., Grbec, S. Lesar, B. Plavčak, D. Šega, B. Šernek, M. Straže, A. and Humar.M. 2020. Durability and mechanical performance of differently treated glulam beams during two years of outdoor exposure. Wood Ind./Drvna Industrija. 71(3): 243– 252.
19. Lee, D. H., Lee, M. J. Son, D. W. and Park.B. D. 2006. Adhesive performance of woods treated with alternative preservatives. Wood Sci. Technol. 40(3): 228– 236.
20. Lorenz, L. F. and Frihart.C. 2006. Adhesive bonding of wood treated with ACQ and copper azole preservatives. Forest Prod. J. 56(9): 90– 93.
21. Miyazaki, J. and Nakano.T. 2003. Effects of wood preservatives on adhesive properties. IV. Effects of preservation and incising on shear strength and delamination. Mokuzai Gakkaishi. 49(3): 212– 218.
22. Miyazaki, J., Nakano, T. Hirabayashi, Y. and Kishino.M. 1999. Effects of wood preservatives on adhesion properties of phenolformaldehyde resin. Mokuzai Gakkaishi. 45(1): 34– 41.
23. Morris, P. I., Dale, A. and Ingram.J. K. 2014. A serendipitous field test against the cellar fungus Coniophora olivacea. Forest Prod. J. 64(3–4): 141– 143.
24. Morris, P. I., Ingram, J. Larkin, G. and Laks.P. 2011. Field tests of naturally durable species. Forest Prod. J. 61(5): 344– 351.
25. Morris, P. I., Ingram, J. K. Ruddick, J. N. R. and Choi.S. M. 2004. Protection of untreated wood by adjacent CCA-treated wood. Forest Prod. J. 54(3): 29– 32.
26. Morris, P. I., Stirling, R. and Ingram.J. 2017. Ten-year performance of stakes and decking treated with copper azole type B and alkaline copper quat type D (Carbonate). Forest Prod. J. 67(1–2): 13– 23.
27. Morris, P. I. and Wang.J. 2008. A new decay hazard map for North America using the Scheffer index. Document No. IRG/WP/08-10672. International Research Group on Wood Protection, Stockholm. 13pp.
28. Podgorski, L. and Legrand.G. 2006. Paintability and gluability of wood treated with arsenic-free and chromium-free preservative treatments. Document No. IRG/WP/06-40342. International Research Group on Wood Protection, Stockholm. 17pp.
29. Selbo, M. L. 1957. Laminating of preservative-treated wood. Proc. Amer. Wood Preserv. Assoc. 53: 48– 55.
30. Sellers, T., Jr. and Miller,G. D.Jr. 1997. Evaluations of three adhesive systems for CCA-treated lumber. Forest Prod. J. 47(10): 73– 76.
31. Tascioglu, C., Goodell, B. and Lopez-Anido.R. 2003. Bond durability characterization of preservative treated wood and E-glass/phenolic composite interfaces. Compos. Sci. Technol. 63(7): 979– 991.
32. Vick, C. B. 1995. Coupling agent improves durability of PRF bonds to CCA-treated southern pine. Forest Prod. J. 45: 78– 78.
33. Vick, C. B. and Christiansen.A. W. 1993. Cure of phenol–formaldehyde adhesive in the presence of CCA-treated wood by differential scanning calorimetry. Wood Fiber Sci. 25(1): 77– 86.
34. Wacker, J. P. 2004. Recent trends in preservative treatments for timber bridges.Wood Des. Focus(Summer 2004):17–20.
35. Winandy, J. E. and River.B. H. 1986. Evaluation of a method for testing adhesive. Forest Prod. J. 36(1): 27– 32.
36. Woo, K. L., Watson, P. and Mansfield.S. D. 2005. The effects of mountain pine beetle attack on lodgepole pine wood morphology and chemistry: Implications for wood and fiber quality. Wood Fiber Sci. 37(1): 112– 126.
37. Yang, T. H., Lin, C. H. Wang, S. Y. and Lin.F. C. 2012. Effects of ACQ preservative treatment on the mechanical properties of hardwood glulam. Eur. J. Wood Wood Prod. 70(5): 557– 564.