journal article·2020

Effects of Sanding Process on Adhesion of Waterborne Paint Film on a Polypropylene Membrane Surface

Xiaorui Peng, Zhankuan Zhang, Ran Zhang

Forest Products Journal· Volume 70· Issue 2
Publisher page

Abstract

Abstract In this article, the surfaces of 2D and 3D polypropylene (PP) membranes were sanded with different brush-type sanding belts and a waterborne primer and topcoat were applied; the effect of the sanding process on the adhesion of the waterborne paint film on a PP decorative membrane surface was tested. A contact angle meter was used to determine the effect of the sanding process on the hydrophilicity of a PP decorative membrane surface. A scanning electron microscope and a roughness tester were used separately to observe the changes in the surface microfeatures and the roughness on PP decorative membranes before and after the sanding process. A 3D profilometer was used to test the changes in the surface roughness and 3D microtopography on PP decorative membranes before and after the sanding process, and a crosscut tester was used to test the changes in the surface adhesion of waterborne paint film on PP decorative membranes before and after the sanding process so as to research the effects of different sanding parameters on the adhesion of waterborne paint films on PP decorative membrane surfaces. The research results showed that the surface sanding process could be used to decrease the surface contact angle, increase the roughness, and improve the wettability of PP decorative membranes. In general, under experimental conditions, a 400-grit sanding belt and two sanding passes were the suitable parameters for 2D PP decorative membranes, and a 320-grit sanding belt and two sanding passes were suitable for 3D PP decorative membranes.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Surface Modification and Superhydrophobicity · Material Properties and Processing · Surface Roughness and Optical Measurements

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Bai, X. 2016. Research situation and development trend of environmental plastics in furniture materials. China Plastics Ind. 44(10):1–4.
2. Chen, A. M. , X. M. Zhang, Q. M. Lei, and J. X. Fu. 2000. Modification approaches to improving performance of surface adhesion of sheets based on polyethylene and polypropylene. China Plastics Ind. 14(11):16–20.
3. Cheng, C. Z. 2009. Hydrophilic modification and characterization of polypropylene film surface. PhD thesis. Northwest Normal University, Lanzhou, China.
4. Dimitriou, A., M. D. Hale, and M. J. Spear. 2016. The effect of four methods of surface activation for improved adhesion of wood polymer composites (WPCs). Int. J. Adhes. Adhes. 68:188–195.
5. Li, D. H., S. Z. Liu, A. P. Li, H. Q. Xu, and D. H. Li. 2017. Research progress in modification of polypropylene film. New Chem. Mater. 45(1):44–47.
6. Ma, X. J. and L. Y. Ma. 2018. Application of atomic force microscope in membrane technology. J. Tianjing Univ. Sci. Technol. 33(4):1–6. https://doi.org/10.13364/j.issn.1672-6510.20180070
7. Owens, D. K. and R. Wendt. 1969. Estimation of the surface free energy of polymers. J. Appl. Polym. Sci. 13(8):1741–1747. https://doi.org/10.1002/app.1969.070130815
8. Peng, X. R. and Z. K. Zhang. 2018. Surface properties of different natural precious decorative veneer by plasma modification. Eur. J. Wood Wood Prod. 77(3):315–326. https://doi.org/10.1007/s00107-018-1355-3
9. Peng, X. R. and Z. K. Zhang. 2019. Improvement of paint adhesion of environmentally friendly paint film on wood surface by plasma treatment. Prog. Org. Coatings134:255–263. https://doi.org/10.1016/j.porgcoat.2019.04.024
10. Peng, X. R., Z. K. Zhang, B. G. Wang, and W. G. Li. 2012. Effect of sanding parameter on wood surface roughness using brush sander. China Wood Ind. 26(6):46–49.
11. Samyn, P., J. V. Erps, and H. Thienpont. 2016. Relation between optical non-contact profilometry and AFM roughness parameters on coated papers with oil-filled nanoparticles. Measurement82:75–93. https://doi.org/10.1016/j.measurement.2015.12.035
12. Sheng, Y., D. Zhu, X. Su, Y. Zou, Z. Wang, and Q. Chen. 2012. Effects of different treatment agents on the properties of PP/wood flour composites. Polym. Mater. Sci. Eng. 28(10):51–54. https://doi.org/10.1093/eurpub/8.3.265-d
13. Standardization Administration of China (SAC). 1995. Wooden furniture—General technical requirements. GB/T 3324-1995. SAC, Beijing.
14. Standardization Administration of China (SAC). 1998. Paints and varnishes—Cross cut test for films. GB/T 9286-1998. SAC, Beijing.
15. Standardization Administration of China (SAC). 2003. Geometrical product specifications—Surface texture: Profile method—Surface roughness parameters and their values for wooden pieces. GB/T 12472-2003. SAC, Beijing.
16. Wolkenhauer, A., G. Avramidis, H. Militz, and W. Viöl. 2008. Plasma treatment of heat treated beech wood-investigation on surface free energy. Holzforschung62(4):472–474. https://doi.org/10.1515/hf.2008.074
17. Young, T. 1805. An essay on the cohesion of fluids. Philos. Trans. R. Soc. Lond. 95:23–87.
18. Zhang, Z. G. 2012. Wood Surface Decoration Technology. China Forestry Publishing House, Beijing.
19. Zhang, Z. K., X. R. Peng, B. G. Wang, and W. G. Li. 2012. Surface quality evaluation after sanding wooden doors. China Wood Ind. 26(2):14–17.
20. Zhen, H. M., J. Han, X. B. Ding, G. P. Xu, and B. Yu. 2014. Study on surface treatment and hydrophilic properties of PVC architectural membrane materials. J. Zhejiang Sci-Tech Univ. (Nat. Sci.)31(7):413–416.