Manufacture and Properties of Metasequoia-Based Three-Layer Parquet Flooring
Source abstract
Abstract
Abstract Metasequoia-based three-layer parquet flooring (MPF) was prepared under the following conditions: hot-pressing temperature of 95°C, hot-pressing time of 7 minutes, hot-pressing pressure of 9 kg·cm−2, and addition of 200 g·m−2 urea-formaldehyde resin adhesive. The results showed that the moisture content, density, formaldehyde emission, static bending strength, and elastic modulus of the three kinds of parquet flooring were not much different than poplar-based multilayer parquet flooring (PPF) or fir-based three-layer parquet flooring (FPF) on the market. The thermal conductivity of the MPF was 0.195 W·m−1·K−1, which was the lowest among the three kinds of parquet flooring. The sound absorption coefficient of MPF under 11 frequency conditions in the range of 0.2 to 2 kHz was higher than that of PPF and FPF under the same frequency condition. The research results provide a reference value for the efficient use of low-quality M. glyptostroboides wood.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Tree Root and Stability Studies · Bamboo properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Abdou, A. and Budaiwi.I. 2005. Comparison of thermal conductivity measurements of building insulation materials under various operating temperatures. J. Building Phys. 29(2): 171– 184.
2. Ahnert, W., Behrens, T. and Pana.R. 2015. The national opera theatre in Bucharest—Update of the room-acoustical properties. J. Acoustical Soc. Am. 138(3): 1878– 1878.
3. Anders, H. and Terje.K. S. 2018. Evaluation of floor vibration properties using measurements and calculations. Eng. Struct. 175: 168– 176.
4. Bajpai, V. K. and Kang.S. C. 2010. Antibacterial abietane-type diterpenoid, taxodone from Metasequoia glyptostroboides Miki ex Hu. J. Biosci. 35(4): 533– 538.
5. Bartholomew, B., Boufford, D. E. and Spongberg.S. A. 1983. Metasequoia glyptostroboides—Its present status in central China. J. Arnold Arboretum64: 105– 128.
6. Berger, G., Katz, H. and Petutschnigg.A. J. 2006. What consumers feel and prefer: Haptic perception of various wood flooring surfaces. Forest Prod. J. 56(10): 42– 47.
7. Blumer, S., Niemz, P. Serrano, E. and Gustafsson.P. J. 2009. Moisture induced stresses and deformations in parquet floors. Wood Res. 54(1):89–102.
8. Caniato, M., Orfeo, S. Kaspar, J. and Monte.R. D. 2013. Green cork-based innovative resilient and insulating materials: Acoustic, thermal, and mechanical characterization. J. Acoustical Soc. Am. 133(5): 3453.
9. Cao, Y.-Z., Gao, H. B. Tang, Y.-N. and Wu.H. 2014. Study on the effect of tree species and thickness of plywood sound absorption performance at ambient temperature. Forestry Machinery Woodworking Equipment10: 44– 46.
10. Honglu, X., and Tiejun.S. 2006. Wood liquefaction by ionic liquids. Holzforschung60(5): 509– 512.
11. Hou, Q. Q., Yu, H. P. Wang, J. M. and Guo.M. H. 2010. Research on influence factors of absorption performance for wooden perforated panels. Adv. Mater. Res. 113–116: 1959– 1963.
12. Ji, Z., Juan, B. Xiaohua, W. and Chunjiang.L. 2018. Sustainable management of Metasequoia glyptostroboides plantation forests in shanghai. Forests9(2): 64.
13. Li, Y., Chen, X. Zhang, X. Wu, T. Lu, H. and Cai.Y. 2005. Genetic differences between wild and artificial populations of Metasequoia glyptostroboides: Implications for species recovery. Conserv. Biol. 19(1): 224– 231.
14. Ma, J. 2007. A worldwide survey of cultivated Metasequoia glyptostroboides Hu & Cheng (Taxodiaceae: Cupressaceae) from 1947 to 2007. Bull. Peabody Mus. Nat. Hist. 48(2): 235– 253.
15. Ma, J., and Shao.G. 2003. Rediscovery of the first collection of the “Living Fossil”, Metasequoia glyptostroboides. Taxon52(3): 585– 588.
16. Magnusson, T. 2001. Engineered hardwood flooring system having acoustic attenuation characteristics. J. Acoustical Soc. Am. 110(5): 2252.
17. Montgomery, R. B. 1947. Viscosity and thermal conductivity of air and diffusivity of water vapor in air. J. Atmos. Sci. 4(6): 193– 196.
18. Nelson, E. C. 1998. Metasequoia glyptostroboides, the dawn redwood: Some Irish glosses on its discovery and introduction into cultivation. Curtis's Bot. Mag. 15(1): 77– 80.
19. Okudaira, Y., Ando, H. and Satoh.M. 1998. Sound absorption by multi-layered constructions composed of powder layers and porous sheets. Electrical Eng. Jpn. 122(2): 1– 11.
20. Pierre, B. R., Beauregard, A. E. and Marcel.L. 2003. Comparative study of four adhesives used as binder in engineered wood parquet flooring. Forest Prod. J. 53(1): 89– 93.
21. Sanmartín, I. 2012. Historical biogeography: Evolution in time and space. Evol. Educ. Outreach5(4): 555– 568.
22. Wang, J., Han, S. Yin, W. Xia, X. and Liu.C. 2019. Comparison of reliable reference genes following different hormone treatments by various algorithms for qRT-PCR analysis of Metasequoia. Int. J. Mol. Sci. 20(34): 1– 18.
23. Wang, S., Lin, F. and Lin.M. 2000. Thermal properties of interior decorative material and contacted sensory cold-warmth I: Relation between skin temperature and contacted sensory cold-warmth. J. Wood Sci. 46(5): 357– 363.
24. Wang, Z. H., Fei, B. H. Zhu, S. J. and Zhang.G. L. 1998. Wood properties of dawn redwood and its comprehensive utilizations. J. Anhui Agric. Univ. 25(4): 408– 412.
25. Wassilieff, C. 1996 Sound absorption of wood-based materials. Appl. Acoustics48(4): 339– 356.
26. Wei, X. U., Jiatong, H. Yuefei, F. Zhihui, W. U. and Jianfeng.L. 2016. Effect of coating thickness on the sound absorption characteristics of spruce wood. J. Forestry Eng. 1(4): 156– 160.
27. Williams, C. J., Lepage, B. A. Vann, D. R. Tange, T. Ikeda, H. Ando, M. Kusakabe, T. Tsuzuki, H. and Sweda.T. 2003. Structure, allometry, and biomass of plantation Metasequoia glyptostroboides in Japan. Forest Ecol. Manag. 180(1–3): 287– 301.
28. Wu, Y., Sha, T. Zhao, Z. He, Z. and Yi.S. 2016. Influence of different pretreatments on the acoustic properties of dawn redwood (Metasequoia glyptostroboides Hu et Cheng). Bioresources11(1): 2734– 2743.
29. Xie, H., and Shi.T. 2010. Liquefaction of wood (Metasequoia glyptostroboides) in allyl alkyl imidazolium ionic liquids. Wood Sci. Technol. 44(1): 119– 128.
30. Yamamura, I. and Ohta.M. 2015. Sound absorption performance of wood in a high frequency range I.: Composing a measurement method in a high frequency range. Mokuzai Gakkaishi61(4): 261– 267.
31. Yildiz, U. C., Temiz, A. Gezer, E. D. and Yildiz.S. 2004. Effects of the wood preservatives on mechanical properties of yellow pine (Pinus sylvestris L.) wood. Building Environ. 39(9): 1071– 1075.
32. Zhang, X., Wei, H. Zhang, X. Liu, J. and Gu.W. 2020. Non-pessimistic predictions of the distributions and suitability of Metasequoia glyptostroboides under climate change using a random forest model. Forests11(1): 62– 76.
33. Zoltán, P., Tibor, H. Glass, S. V. and Zelinka.S. L. 2015. Thermal insulation system made of wood and paper for use in residential construction. Forest Prod. J. 65(7/8): 352– 357.