Flexural Properties of Three-Ply Bolt-Laminated Pine Mats
Source abstract
Abstract
Abstract In the current study, three-ply bolt-laminated southern pine (Pinus sp.) 244 by 427 cm (8 by 14 ft) mats were evaluated. Mats were destructively tested in ⅓-point bending on a universal testing machine according to ASTM International standards. Twenty-eight unique specimens were destructively tested, and mean modulus of rupture (MOR) and modulus of elasticity (MOE) were calculated. According to the results both MOR and MOE values for the specimens were highly uniform. The mean MOR was 11.74 MPa (1,704 psi) and the mean MOE was 1,144 MPa (0.166 × 106 psi). Additionally, the values of parametric and nonparametric Fb (design fiber stress in bending values ) were reported as 4.05 MPa and 4.54 MPa (588 psi and 659 psi), respectively. The mechanical properties of these three-ply pine mats were also compared with other studies of mats from other species groups and design architectures.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Engineering and Material Science Research · Tunneling and Rock Mechanics · Transportation Safety and Impact Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. ASTM D2915-10. 2017 a. Standard practice for sampling and data-analysis for structural wood and wood-based products. ASTM International. West Conshohocken, Pennsylvania.
2. ASTM D5456-17. 2017 b. Standard specification for evaluation of structural composite lumber products. ASTM International. West Conshohocken, Pennsylvania.
3. Engineered Wood Association (APA) PRG 320. 2018. Standard for performance-rated cross-laminated timber. The Engineered Wood Association, Tacoma, Washington.
4. Owens, F. C., Seale, R. D. and Shmulsky.R. 2020. Strength and stiffness of 8-inch-deep mixed hardwood composite timber mats. BioResources15(2): 2495– 2500. https://doi.org/10.15376/biores.15.2.2495-2500
5. Shmulsky, R., Correa, L. M. S. and Quin.F. 2021 a. Strength and stiffness of 3-ply industrial bamboo matting. Bioresources16(3): 6392– 6400. https://doi.org/10.15376/biores.16.3.6392-6400
6. Shmulsky, R., Lopes, D. J. V. Rodrigues, B. P. and Bobadilha.G. D. S. 2021 b. Strength and stiffness of 8-inch and 12-inch-deep mixed oak bolt-laminated timber mats. BioResources16(2): 3298– 3303. https://doi.org/10.15376/biores.16.2.3298-3303
7. Shmulsky, R., and Shi.S. 2008. Development of novel industrial laminated planks from sweetgum lumber. J. Bridge Eng. 13(1): 64– 66. https://doi.org/10.1061/(ASCE)1084-0702(2008)13:1(64)
8. Snow, D., Shmulsky, R. Bobadilha, G. S. and Lopes.D. J. V. 2022. Bending strength and stiffness of three-ply bolt-laminated mixed oak and hardwood industrial mats. BioResources17(1): 1354– 1363. https://doi.org/10.15376/biores.17.1.1354-1363
9. Southern Pine Inspection Bureau (SPIB). 2014. Standard grading rules for southern pine lumber. Table 1-c-Structural light framing, structural joists and planks, and studs—2″ to 4″ thick (8″-wide only). Southern Pine Inspection Bureau, Pensacola, Florida.
10. Spinelli, L. M. 2022. Cross-laminated timber (CLT) mechanical properties evaluation. Doctoral dissertation.Mississippi State University, Mississippi State. pp.66.
11. Yang, B. Z., Shmulsky, R. and Seale.R. D. 2015. Development of laminated planks from southern pine lumber. Eur. J. Wood Wood Prod. 73(4): 547– 549. https://doi.org/10.1007/s00107-015-0915-z