Determining the Extent of damage in Snapped Southern Yellow Pine Trees with Acoustic Testing
Source abstract
Abstract
Abstract Salvage of downed timber following a windstorm allows recovery of management options for landowners and wood products for industry. Because wood volumes are large and logging, transportation, mill storage, and processing capacities are limited, avoiding the selection of logs with damage can conserve those resources. Visual damage indicators are typically used to select and differentiate products, but damaged logs are still delivered to mills. Following experimental tree winching in 2021 and a tornado in 2023, we assessed lengths of broken trees with a Fakopp microsecond timer. Using a recognized defect limit (10% deviation from the maximum acoustic velocity) about 80 percent of volume in broken tops could be recovered. Standard rules of thumb applied from the end of visible damage resulted in the recovery of about 50 percent of the volume with a relatively low defect rate (<10%). Applying bucking rules developed from acoustic measurements based on distance from snap might be easier to apply and increase recovery rates to over 70 percent of broken top volume.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Tree Root and Stability Studies · Wood Treatment and Properties · Forest ecology and management
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Aho, P. E. and Cahill J. M. 1984. Deterioration rates of blowndown timber and potential problems associated with product recovery. GTR-167. USDA Forest Service Pacific Northwest Range and Experiment Station, Portland, Oregon. 11 pp.
2. Alabama Forest Recovery Task Force. 2008. Alabama forest recovery: The Ivan experience. Alabama Forestry Commission, Montgomery, Alabama. 32 pp.
3. Arnold, M. and Steiger R. 2007. The influence of wind-induced compression failures on the mechanical properties of spruce structural timber. Mater. Struct. 40(1): 57–68.
4. Butler, M. A.,Dahlen J.,Eberhardt T. L.,Montes C.,Antony F., and Daniels R. F. 2017. Acoustic evaluation of loblolly pine tree- and lumber-length logs allows for segregation of lumber modulus of elasticity, not for modulus of rupture. Ann. Forest Sci.74(1):20. https://doi.org/10.1007/s13595-016-0615-9
5. Čakša, L.,Šēnhofa S.,Šņepsts G.,Elferts D.,Liepa L., and Jansons A. 2021. Effect of stem snapping on aspen timber assortment recovery in hemiboreal forests. Forests 12(1):28. https://doi.org/10.3390/f12010028
6. Cannon, J. B.,Barrett M. E., and Peterson C. J. 2015. The effect of species, size, failure mode, and fire-scarring on tree stability. Forest Ecol. Manag. 356:196–203. https://doi.org/10.1016/j.foreco.2015.07.014
7. Cannon, J. B.,Peterson C. J.,Godfrey C. M., and Whelan A.W. 2023. Hurricane wind regimes for forests of North America. Proc. Nat. Acad. Sci. U. S. A. 120(42):e2309076120. https://doi.org/10.1073/pnas.2309076120
8. Cannon, J. B.,Scully S. H.,Taylor R. S.,Peterson C. J., and Newson T. 2024. Soil moisture increases stability of some tree species in sand soils. Forest Ecol. Manag. 565. https://doi.org/10.1016/j.foreco.2024.122009
9. Carter, P.,Wang X., and Ross R. J. 2013. Field application of processor head acoustic technology in forest harvest operations. General Technical Report FPL GTR-226. In Proceedings 18th International Nondestructive Testing and Evaluation of Wood Symposium, Ross R. J. and Wang W. (Eds.), September 24–27, 2013, Madison, Wisconsin; USDA Forest Products Laboratory, Madison, Wisconsin. pp. 24–27.
10. Clarke, M.,Sharma A.,Stein T.,Vogel J., and Nowak J. 2023. Forest disturbances and nonindustrial forest landowners: Management of invasive plants, fire hazards and wildlife habitats after a hurricane. J. Forestry 121(5–6):419–431. https://doi.org/10.1093/jofore/fvad022
11. Dale, V. H.,Joyce L. A.,McNulty S.,Neilson R. P.,Ayres M. P.,Flannigan M. D.,Hanson P. J.,Irland L. C.,Lugo A. E.,Peterson C. J.,Simberloff D.,Swanson F. J.,Stocks B. J., and Wotton B. M. 2001. Climate change and forest disturbances: Climate change can affect forests by altering the frequency, intensity, duration, and timing of fire, drought, introduced species, insect and pathogen outbreaks, hurricanes, windstorms, ice storms, or landslides. BioScience 51(9):723–734. https://doi.org/10.1641/0006-3568(2001)051[0723:CCAFD]2.0.CO;2
12. Farrar, R. M.,Jr. 1987. Stem-profile equations for predicting multiple-product volumes in natural longleaf pines. South. J. Appl. Forestry 11(3):161–167.
13. Faust, T. D.,Fuller M. M.,McAlister R. H., and Zarnoch S. J. 1994. Assessing internal damage to standing pine poletimber. Wood Fiber Sci. 26(4): 536–545.
14. Fortuin, C. C.,Montes C. R.,Vogt J. T., and Gandhi K. J. K. 2023. Stand and tree characteristics influence damage severity after a catastrophic hurricane disturbance. Forest Ecol. Manag. 532:120844. https://doi.org/10.1016/j.foreco.2023.120844
15. Hamilton, R. and Bardon R. 2011. Utilization of storm-damaged timber. https://content.ces.ncsu.edu/utilization-of-storm-damaged-timber. Accessed December 1, 2023.
16. Henderson, J. D.,Abt R. C.,Abt K. L.,Baker J., and Sheffield R. 2022. Impacts of hurricanes on forest markets and economic welfare: The case of Hurricane Michael. Forest Policy Econ. 140:102735. https://doi.org/10.1016/j.forpol.2022.102735.
17. Lupold, H. M. 1996. Salvage of storm damaged timber. GTR SRS-5. In Hurrican Hugo: South Carolina forest land research and management related to the storm, Haymond J. L.,Hook D., and Harms W. R. (Eds), USDA Forest Service Southern Research Station, Asheville, North Carolina. pp. 21–27.
18. Mahon, J. M.,Jordan L.,Schimleck L. R.,Clark A., and Daniels R. F. 2009. A comparison of sampling methods for a standing tree acoustic device. South. J. Appl. Forestry 33(2):62–68.
19. Mergen, F. 1954. Mechanical aspects of wind-breakage and windfirmness. J. Forestry 52(2):119–125.
20. Nieuwenhuis, M. and Fitzpatrick P. 2002. An assessment of stem breakage and the reduction in timber volume and value recovery resulting from a catastrophic storm: An Irish case study. Forestry 75(5):513–523.
21. Ojha, S. K.,Naka K., and Dimov L. D. 2020. Assessment of disturbances across forest inventory plots in the southeastern United States for the period 1995–2018. Forest Science. 66(2):242–255. https://doi.org/10.1093/forsci/fxz072
22. Peralta, P. N.,Syme J. H., and McAlister R. H. 1993. Water storage and plywood processing of hurricane-downed southern pine timber. Forest Prod. J. 43(4):53–61.
23. Prestemon, J. and Holmes T. 2004. Market dynamics and optimal timber salvage after a natural catastrophe. Forest Sci. 50(5):742–742.
24. Rudnicki, M.,Wang X.,Ross R. J.,Allison R. B., and Perzynski K. 2017. Measuring wood quality in standing trees. General Technical Report FPL-GTR-248. USDA Forest Products Laboratory, Madison, Wisconsin. 11 p.
25. Rutledge, B. T.,Cannon J. B.,McIntyre R. K.,Holland A. M., and Jack S. B. 2021. Tree, stand, and landscape factors contributing to hurricane damage in a coastal plain forest: Post-hurricane assessment in a longleaf pine landscape. Forest Ecol. Manag. 481:118724. https://doi.org/10.1016/j.foreco.2020.118724
26. SAS Institute. 2016. SAS version 9.4. Cary, North Carolina.
27. Schad, K. C.,Schmoldt D. L., and Ross R. J. 1996. Nondestructive methods for detecting defects in softwood logs. Research Paper FPL-RP-546. USDA Forest Products Laboratory, Madison, Wisconsin. 13 p.
28. Sonderegger, W. and Niemz P. 2004. The influence of compression failure on the bending, impact bending and tensile strength of spruce wood and the evaluation of non-destructive methods for early detection. Holz Als Roh-Und Werkstoff 62(5):335–342.
29. Suvanto, S.,Henttonen H. M.,Nöjd P., and Mäkinen H. 2016. Forest susceptibility to storm damage is affected by similar factors regardless of storm type: Comparison of thunder storms and autumn extra-tropical cyclones in Finland. Forest Ecol. Manag. 381:17–28. https://doi.org/10.1016/j.foreco.2016.09.005
30. Walsh, D.,Strandgard M., and Carter P. 2014. Evaluation of the Hitman PH330 acoustic assessment system for harvesters. Scand.J. Forest Res. 29(6):593–602. https://doi.org/10.1080/02827581.2014.953198
31. Wang, X.,Divos F.,Pilon C.,Brashaw B. K.,Ross R. J., and Pellerin R. F. 2004. Assessment of decay in standing timber using stress wave timing nondestructive evaluation tools. General Technical Report, FPL-GTR-147. USDA Forest Products Laboratory, Madison, Wisconsin. 12 p.
32. Wang, X. P.,Verrill S.,Lowell E.,Ross R. J., and Herian V. L. 2013. Acoustic sorting models for improved log segregation. Wood Fiber Sci. 45(4):343–352.
33. Xu, F.,Wang X. P.,Thomas E.,Liu Y. F.,Brashaw B. K., and Ross R. J. 2018. Defect detection and quality assessment of hardwood logs: Part 1-acoustic impact test and wavelet analysis. Wood Fiber Sci. 50(3):291–309. https://doi.org/10.22382/wfs-2018-029