article·1997-03-01

The effects of steaming prior to pressure treatment on the penetration of borates into western hemlock.

Paul Morris, Adam M. Byrne, J. F. G. Mackay, S. M. McFarling

Abstract

The recent interest in borate treatment for the production of termite-resistant lumber has led to the need for improved treatment processes. Pre-steaming prior to pressure treatment is known to have a number of potential benefits in terms of improved permeability, moisture distribution, and effectiveness of the vacuum. This process was therefore tried on western hemlock dodai (105-mm squares) in an attempt to achieve 80 percent cross-sectional penetration with a minimal diffusion period after pressure treatment. Western hemlock pre-steamed to a core temperature of 82°C in 4 hours took up almost double the amount of treating solution of end-matched unsteamed samples. There was an improvement in mean heartwood penetration of 45 percent immediately after treatment and a 134 percent increase in penetration after 1 week of storage. This was not entirely due to diffusion within the wood but to mass flow of treating solution continuing after the end of the pressure process. After 1 week of storage, 64 percent of samples had 80 percent of the cross section penetrated. Reducing the vacuum time from 30 minutes to zero had a detrimental effect on penetration. Increasing time under vacuum to 60 minutes provided no beneficial effect. Pre-steaming of hemlock dodai therefore appears to be a very effective means of improving uptake during pressure treatment.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Insect and Arachnid Ecology and Behavior · Forest Insect Ecology and Management · Insect and Pesticide Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.