Reaction sintering of alumina/mullite nanocomposites from nano-sized starting powders
Source abstract
Abstract
Alumina/mullite ceramic nanocomposites were prepared by the mixtures of nano-sized starting powders of alumina with silica and alumina with silicon carbide. Silica from deliberate addition and as the product of silicon carbide oxidation reacted completely with alumina to form mullite. Silica from direct addition segregated at the grain boundary and intergranular mullite was formed whereas silica from oxidation was surrounded by alumina matrix and intragranular mullite was formed after reaction sintering. The most significant difference was fracture behaviour where intragranular mullite nanoparticles promoted transgranular fracture in alumina matrix due to thermal mismatch around nanoparticles and intergranular mullite nanoparticles gave rise to intergranular fracture similar to pure alumina. Wear resistance of the nanocomposites was better than that of alumina. Pull-out formation in the nanocomposites was less and pull-out size was also smaller. Fracture toughness of the nanocomposites was significantly higher than that of alumina.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Physics and Materials Science, Faculty of Science, Chiang Mai University, 50200 Thailand
Funding
Thailand Research Fund
References (23)
Show source-provided references
1. 10.2109/jcersj.99.97410.2109/jcersj.99.974 ↗
2. 10.1002/352760735810.1002/3527607358 ↗
3. 10.1016/j.msea.2007.05.10410.1016/j.msea.2007.05.104 ↗
4. 10.1016/j.wear.2011.03.01610.1016/j.wear.2011.03.016 ↗
5. 10.1016/j.jeurceramsoc.2009.10.01310.1016/j.jeurceramsoc.2009.10.013 ↗
6. 10.1016/j.compscitech.2008.08.01210.1016/j.compscitech.2008.08.012 ↗
7. 10.1179/1743676114Y.000000016410.1179/1743676114Y.0000000164 ↗
8. 10.1016/j.ijrmhm.2015.07.02610.1016/j.ijrmhm.2015.07.026 ↗
9. 10.1016/j.ceramint.2013.03.08710.1016/j.ceramint.2013.03.087 ↗
10. 10.1016/j.ceramint.2014.04.13310.1016/j.ceramint.2014.04.133 ↗
11. 10.1111/j.1151-2916.1995.tb08827.x10.1111/j.1151-2916.1995.tb08827.x ↗
12. 10.1016/j.actamat.2005.03.03110.1016/j.actamat.2005.03.031 ↗
13. 10.1111/j.1151-2916.1981.tb10320.x10.1111/j.1151-2916.1981.tb10320.x ↗
14. 10.1016/j.jeurceramsoc.2009.05.01610.1016/j.jeurceramsoc.2009.05.016 ↗
15. 10.1016/j.jeurceramsoc.2007.04.01510.1016/j.jeurceramsoc.2007.04.015 ↗
16. 10.1016/S0043-1648(99)00236-710.1016/S0043-1648(99)00236-7 ↗
17. 10.1515/secm-2014-035310.1515/secm-2014-0353 ↗
18. 10.1016/j.jeurceramsoc.2009.03.02310.1016/j.jeurceramsoc.2009.03.023 ↗
19. 10.1179/09679789968047110.1179/096797899680471 ↗
20. 10.1111/j.1151-2916.1991.tb06784.x10.1111/j.1151-2916.1991.tb06784.x ↗
21. 10.1046/j.1365-2818.1997.d01-610.x10.1046/j.1365-2818.1997.d01-610.x ↗
22. 10.1016/j.jeurceramsoc.2008.04.01810.1016/j.jeurceramsoc.2008.04.018 ↗
23. P. Hvizdoš, P. Tatarko, A. Duszova and J. Dusza: ‘Failure mechanisms of ceramic nanocomposites’, in 'Ceramic Nanocomposites', (ed. R. Banerjee and R. Manna), 117–152 2013, Cambridge, Woodhead Publishing.10.1533/9780857093493.1.117 ↗