An Alternative Preservative Treatment Procedure for Marine- and Shuttering-Grade Plywood in India
Source abstract
Abstract
Abstract The present research was performed with an aim to develop an alternative preservative treatment method for marine- and shuttering-grade plywood. Per Indian Standards, 12 kg/m3 of retention is required in marine- and shuttering-grade plywood, which is very difficult to achieve. The higher loadings of wood preservative chemical are being achieved only by the pressure impregnation method. The pressure impregnation method requires energy to run the equipment, skilled manpower, and sophisticated instruments; a large amount of damage takes place to the plywood during the process. Hence, an alternative to this glue-line poisoning followed by hot and cold dipping of plywood has been found suitable to achieve the 12 kg/m3 of retention without affecting the glue and plywood properties.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Bamboo properties and applications · Wood and Agarwood Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Beal, R. H. 1975. Fighting termites chemically. Build. Off. Code Adm. 9(9):14–17
2. Bureau of Indian Standards (BIS). 1983. Indian Standard. Methods of testing for plywood. IS: 1734. BIS, New Delhi.
3. Bureau of Indian Standards (BIS). 1991. Indian Standard. Methods for estimation of preservatives in treated timber and in treating solution. IS: 2753 (Part-1). BIS, New Delhi.
4. Bureau of Indian Standards (BIS). 2005. Indian Standard. Method for determination of flow time by use of flow cups. IS: 3944. BIS, New Delhi.
5. Bureau of Indian Standards (BIS). 2006. Indian Standard. Specification for synthetic resin adhesives for making plywood (phenolic and amino plastics). IS: 848. BIS, New Delhi.
6. Bureau of Indian Standards (BIS). 2010. Indian Standard. Specification for marine-grade plywood. IS: 710. BIS, New Delhi.
7. Carle, J. and P. Holmgren. 2008. Wood from planted forests: A global outlook 2005–2030. Forest Prod. J. 58(12):6–18.
8. Dimri, M. P. and K. S. Shukla. 1991. Study on the effect of wood preservatives on the glue bond strength of plywood. Van Vigyan29(1):35–39.
9. Food and Agriculture Organization of the United Nations (FAO). 2009. Status of the world's forests report 2009. FAO, Rome. ftp://ftp.fao.org/docrep/fao/011/i0350e/i0350e02a.pdf. Accessed November 5, 2014.
10. Hashim, R., D. Dickinson, R. Murphy, and J. Dinwoodie. 1992. Effect of vapour boron treatment on mechanical properties of wood based board materials. Document No. IRG/WP/3727‐92. International Research Group on Wood Protection, Stockholm.
11. Kalawate, A. 2013. Evaluation of copper ethanolamine boron based wood preservative to control wood destroying insects. Mol. Entomol. 4(2):6–12. DOI:10.5376/me.2013.04.000210.5376/me.2013.04.0002 ↗
12. Kamal, S. Z. M., S. Padmanabhan, and K. Mohandas. 2003. Dursban 50 WT as a glueline additive for protection of plywood against borers. IPIRTI Research Report No. 129. Indian Plywood Industries Research & Training Institute, Bangalore.
13. Kumar, S. 2005. Status of wood preservation industry in India. Document No. IRG/WP 05‐30388. International Research Group on Wood Protection, Stockholm.
14. Laks, P. E. 1999. The past, present, and future of preservative-containing composites. In: 33rd International Particleboard/Composite Materials Symposium Proceedings, M. P. Wolcott, R. Tichy, and D. F. Bender (Eds.), Washington State University, Pullman. pp. 151–158.
15. Laks, P. E., B. A. Haataja, R. D. Palardy, and R. J. Bianchini. 1988. Evaluation of adhesives for bonding borate-treated flake boards. Forest Prod. J. 38(11/12):23–24.
16. Prasad, T. R. N., P. E. Humphrey, and J. J. Morrell. 1994. The effects of chromated copper arsenate and ammoniacal copper zinc arsenate on shear strength development of phenolic resin to Sitka spruce bonds. Wood Fiber Sci. 26(2):223–228.
17. Vick, C. B. 1990. Adhesion of phenol-formaldehyde resin to waterborne emulsion preservatives in aspen veneer. Forest Prod. J. 40(11/12):25–30.