Efflorescence of Alkali-Activated Cements (Geopolymers) and the Impacts on Material Structures: A Critical Analysis
Source abstract
Abstract
Even with the rapid development of the alkali-activated cement (AAC) technology in the past few years, it still needs to be better understood some phenomena that may alter the durability of the material. In many industrial uses and laboratory researches was observed the formation of the salts on the surfacealkali-activated type cements, which was identified as efflorescence. This occurs due to the presence of an alkali transported in contact with the humidity and CO2 environment. It may present externally from the formation of salts on the surface and internally with the carbonation of the alkalis in capillary pores. The effects of efflorescence on the material in use, as well as all factors that can influence its formation are not yet fully understood. This paper presents a critical review about this issue from previous reports (which are very limited in fact, compared with the increasing number of papers and reports on AACs published in the recent years) and scientific knowledge of this physicochemical phenomena.To understand the nature of efflorescence, upon which proper methods of minimising of this issue can be based, the following aspects are discussed and re-examined: (1) the development of efflorescences in PC concrete, (2) the role of alkalis in AACs (3) efflorescence in AACs and (4) effect from physical and microstructural point of view of efflorescences on the ACCs. This paper highlights that the nature of the pore structure and the design parameters (such as alkali concentration, presence of soluble silicates and water content in the activator) are the two most important factors that control efflorescence rate and changes in mechanical behaviour.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Salt weathering on monuments
2. Microstructural changes induced by CO2 exposure in alkali-activated slag/metakaolin pastes10.3389/fmats.2016.00043 ↗
3. Durability and testing - degradation via mass transport10.1007/978-94-007-7672-2_9 ↗
4. Statistical analysis of strength development as a function of varios parameters on activated metakaolin/slag cements10.1111/j.1551-2916.2009.03414.x ↗
5. Real-time investigation of reaction rate and mineral phase modifications10.1016/j.conbuildmat.2012.04.036 ↗
6. Alkali activation of fly ash: effect of the SiO2/Na2O ratio10.1016/j.micromeso.2007.02.055 ↗
7. Sustainable development and climate change initiatives10.1016/j.cemconres.2007.09.008 ↗
8. Calcium carbonate efflorescence on Portland cement and building materials10.1016/S0008-8846(02)00937-7 ↗
9. Effect of alkali cations on aluminus incorporation in geopolymeric gels10.1021/ie0494216 ↗
10. The effect of alkali and Si/Al ratio on the development of mechanical properties of metakaolin-based geopolymers10.1016/j.colsurfa.2006.05.044 ↗
11. The role played by the reactive alumina content in the alkaline activation of fly ashes10.1016/j.micromeso.2005.11.015 ↗
12. Crystallisation of calcium hydroxide in early age model and ordinary cementitious systems10.1016/j.cemconres.2007.01.001 ↗
13. Modification of composition and microstructure of Portland cement pastes as a result of natural and supercritical carbonation procedures10.1021/ie0603363 ↗
14. Effect of temperature and alkaline concentration on metakaolin leaching kinetics10.1016/j.ceramint.2014.02.071 ↗
15. Minimising the global warming potential of clay based geopolymers10.1016/j.jclepro.2014.04.046 ↗
16. Efflorescence control in geopolymers binders based on natural pozzolan10.1016/j.cemconcomp.2011.07.007 ↗
17. Pore solution composition and alkali diffusion in inorganic polymer cement10.1016/j.cemconres.2010.04.008 ↗
18. Valorisation of a kaolin mining waste for the production of geopolymers10.1016/j.jclepro.2015.12.011 ↗
19. Costs and carbon emissions for geopolymers pastes im comparison to ordinary portland cement10.1016/j.jclepro.2011.02.010 ↗
20. Evaluation og the potential improvement in the environmental footprint of geopolymers using waste-derived activators10.1016/j.jclepro.2017.08.007 ↗
21. Geopolymers and related alkali-activated material10.1146/annurev-matsci-070813-113515 ↗
22. Do geopolymers actually contain nanocrystalline zeolites: a reexamination of existing results10.1021/cm050230i ↗
23. Experimental evidence of crystallization pressure inside porous media10.1103/PhysRevLett.94.075503 ↗
24. 9Si, 27Al, 1H and 23Na MAS NMR study of the bonding character in aluminosilicate inorganic polymers10.1007/s00723-007-0043-y ↗
25. Chemical optimisation of the compressive strength of aluminosilicate geopolymers synthesised by sodium silicate activation of metakaolinite10.1039/b212629j ↗
26. The interfacial transition zone in alkali-activated slag mortars10.3389/fmats.2015.00070 ↗
27. Carbonation of cement paste: understanding, challenge and opportunities10.1016/j.conbuildmat.2016.04.138 ↗
28. Stress from crystallization of salt10.1016/j.cemconres.2003.12.034 ↗
29. Magnesia modification of alkali-activated slag fly ash cement10.1007/s11595-011-0182-8 ↗
30. Aluminosilicate polymers - influence of elevated temperatures, efflorescence
31. Microstructure of geopolymer materials based on fly ash
32. A weak alkali bond in (N, K)-A-S-H gels: evidende from leaching and modeling
33. Characterization of glass F fly ash geopolymer pastes immersed in acid and alkali solutions10.1016/j.cemconcomp.2011.08.008 ↗
34. Effect of curing temperature and silicate concentration on fly-ash-based geopolymerization10.1021/ie051251p ↗
35. Technical and commercial progress in the adoption of geopolymer cement10.1016/j.mineng.2011.09.009 ↗
36. Compressive strength development and shrinkage of alkali-activated fly ash-slag blends associated with efflorescence10.1617/s11527-015-0694-3 ↗
37. Review on carbonation curing of cement-bases materials10.1016/j.jcou.2017.07.003 ↗
38. Reaction kinetics of dolomite and portlandite10.1016/j.cemconres.2014.07.017 ↗
39. Efflorescence and subflorescence induced microstructural and mechanical evolution in fly ash-based geopolymers10.1016/j.cemconcomp.2018.06.010 ↗
40. Fly Ash-based geopolymers: the relation between composition, pore structure ans eflforescence10.1016/j.cemconres.2014.06.004 ↗
41. Quantitative kinetic and structural analysis of geopolymers. Part 2. Thermodynamics of sodium silicate activation of metakaolin10.1016/j.tca.2013.01.040 ↗
42. The pore characteristics of geopolymer foam concrete and their impact on the compressive strength and modulus10.3389/fmats.2016.00038 ↗
43. Using fly ash to partially substitute metakaolin in geopolymer synthesis10.1016/j.clay.2013.12.025 ↗
44. Potential application of geopolymers as protection coatings for marine concrete III. Field experiment10.1016/j.clay.2012.05.008 ↗