journal article·2025-04-03Open access

Enhancing steel slag cement mortar performance under low-temperature curing through alkali activation: mechanisms and implications

Wei Ye, Tengteng Feng, Wangwen Sun, Lauren Y. Gómez-Zamorano

Abstract

The effective utilization of steel slag waste offers a sustainable approach to advancing construction materials, particularly in cold regions. This study investigates the influence of alkaline activators and low-temperature curing (10°C) on the performance of steel slag cement mortar. The setting time of mixed slurry with varying steel slag powder content was analyzed, along with the effects of different activators and water glass modulus on compressive strength. Advanced characterization techniques, including thermogravimetric analysis (TGA), X-ray diffraction (XRD), and scanning electron microscopy (SEM), were employed to examine the hydration products and microstructural evolution of optimally activated samples. The results indicate that a Na2O content of 4% significantly enhances the compressive strength of steel slag cement mortar. The composite activator (containing water glass and NaOH) exhibited superior performance compared to neat NaOH, increasing the strength. Activated samples demonstrated increased early hydration products, as evidenced by intensified Ca(OH)2 diffraction peaks. The activators facilitated calcium ion dissolution, reduced the activation energy of cementitious materials, and accelerated hydration kinetics, leading to the enhanced formation of hydration products. Microstructural analysis revealed that the activators disrupted the vitreous network structure of the steel slag powder, promoting more complete hydration and the formation of dense C-S-H gels and Ca(OH)2. This densification reduced porosity and significantly improved the mechanical properties of the cement matrix. These findings highlight the potential of alkaline-activated steel slag cement mortar as a sustainable and high-performance material for construction applications in cold climates.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Concrete Properties and Behavior · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (85)

Show source-provided references
1. Enduring performance of alkali-activated mortars with metakaolin as granulated blast furnace slag replacement10.1016/j.cscm.2021.e00845 ↗
2. Influence of activator on the strength and drying shrinkage of alkali-activated slag mortar10.1016/j.conbuildmat.2007.10.011 ↗
3. Engineering and durability properties of concretes based on alkali-activated granulated blast furnace slag/metakaolin blends10.1016/j.conbuildmat.2012.01.017 ↗
4. Evolution of binder structure in sodium silicate-activated slag-metakaolin blends10.1016/j.cemconcomp.2010.09.004 ↗
5. Comparison of thermogravimetry response of alkali-activated slag and Portland cement pastes after stopping their hydration using solvent exchange method10.1007/s10973-024-12934-5 ↗
6. Alkali activation of mortars containing different replacement levels of ground granulated blast furnace slag10.1016/j.conbuildmat.2011.10.018 ↗
7. Influence of steel slag on properties of cement-based materials: a review10.3390/buildings14092985 ↗
8. Solution calorimetry to assess effects of water-cement ratio and low temperature on hydration heat of cement10.1016/j.conbuildmat.2020.121222 ↗
9. Investigating the hydration, mechanical properties, and pozzolanic activity of cement paste containing co-combustion fly ash10.3390/buildings14051305 ↗
10. Nonevaporable water from neat OPC and replacement materials in composite cements hydrated at different temperatures10.1016/s0008-8846(03)00208-4 ↗
11. Experimental study of alkali-excited steel slag–granulated blast furnace slag–cement-based grouting material based on response surface methodology10.3390/buildings14123841 ↗
12. Workability and mechanical properties of alkali-activated fly ash-slag concrete cured at ambient temperature10.1016/j.conbuildmat.2018.04.008 ↗
13. Utilization of gasification coarse slag powder as cement partial replacement: hydration kinetics characteristics, microstructure and hardening properties10.3390/ma16051922 ↗
14. Reaction kinetics, gel character and strength of ambient temperature cured alkali activated slag–fly ash blends10.1016/j.conbuildmat.2015.01.065 ↗
15. Compatibility studies between NASH and CASH gels. Study in the ternary diagram Na2O–CaO–Al2O3–SiO2–H2O10.1016/j.cemconres.2011.05.006 ↗
16. Thermal reactivation of hydrated cement paste: properties and impact on cement hydration10.3390/ma17112659 ↗
17. Characterisation of alkali-activated stainless steel slag and blast-furnace slag cements10.1016/j.cemconcomp.2023.105230 ↗
18. Experimental study on the effect of compound activator on the mechanical properties of steel slag cement mortar10.3390/cryst11060658 ↗
19. Steel slag in China: treatment, recycling, and management10.1016/j.wasman.2018.04.045 ↗
20. Effects of steel slag as fine aggregate on static and impact behaviours of concrete10.1016/j.conbuildmat.2018.10.129 ↗
21. Unveiling the dielectric property change of concrete during hardening process by ground penetrating radar with the antenna frequency of 1.6 GHz and 2.6 GHz10.1016/j.cemconcomp.2023.105279 ↗
22. Unraveling microstructural evolution in air-entrained mortar and paste: insights from MIP and micro-CT tomography amid cyclic freezing-thawing damage10.1016/j.jobe.2024.109922 ↗
23. Field study of the dielectric constant of concrete: a parameter less sensitive to environmental variations than electrical resistivity10.1016/j.jobe.2023.106938 ↗
24. Temperature dependence of structural build-up and its relation with hydration kinetics of cement paste10.1016/j.conbuildmat.2018.12.226 ↗
25. Study on impact resistance of alkali-activated slag cementitious material with steel fiber10.3390/buildings14113442 ↗
26. Properties, microstructure development and life cycle assessment of alkali-activated materials containing steel slag under different alkali equivalents10.3390/ma17010048 ↗
27. Hydration and microstructure of steel slag as cementitious material and fine aggregate in mortar10.3390/molecules25194456 ↗
28. Hydration of hybrid cements at low temperatures: a study on portland cement-blast furnace slag—Na2SO410.3390/ma15051914 ↗
29. Integrated policies to promote sustainable use of steel slag for construction—a consequential life cycle embodied energy and greenhouse gas emission perspective10.1016/j.enbuild.2015.04.036 ↗
30. The early age hydration products and mechanical properties of cement paste with steel slag powder as additive under steam curing conditions10.3390/buildings13092192 ↗
31. Structural characteristics and hydration kinetics of modified steel slag10.1016/j.cemconres.2010.11.018 ↗
32. Evaluating the effect of high fly ash content and low curing temperature on early hydration heat of blended cement based on isothermal calorimetric method10.1016/j.conbuildmat.2024.136110 ↗
33. Hydration of the silica fume-Portland cement binary system at lower temperature10.1016/j.conbuildmat.2015.05.056 ↗
34. Analysis of hydration mechanism of steel slag-based cementitious materials under saline–alkaline-coupled excitation10.3390/buildings14030597 ↗
35. Study on impact resistance of alkali-activated slag cementitious material with steel fiber10.3390/buildings14113442 ↗
36. Effect of CO2 treatment on the microstructure and properties of steel slag supplementary cementitous materials10.1016/j.conbuildmat.2021.125171 ↗
37. Effects of steel-slag components on interfacial-reaction characteristics of permeable steel-slag–bitumen mixture10.3390/ma13173885 ↗
38. Microstructure and phase evolution of alkali-activated steel slag during early age10.1016/j.conbuildmat.2019.01.213 ↗
39. Effect of triisopropanolamine on compressive strength and hydration of cement-fly ash paste10.1016/j.conbuildmat.2018.05.117 ↗
40. Responses of concrete using steel slag as coarse aggregate replacement under splitting and flexure10.3390/su12124913 ↗
41. Reaction mechanisms of alkali-activated materials10.1590/s1983-41952021000300009 ↗
42. Enhancement of mechanical properties and porosity of concrete using steel slag coarse aggregate10.3390/ma13122865 ↗
43. Producing Portland cement from iron and steel slags and limestone10.1016/s0008-8846(99)00028-9 ↗
44. Revisiting the effect of slag in reducing heat of hydration in concrete in comparison to other supplementary cementitious materials10.3390/ma11101847 ↗
45. Generalized structural description of calcium–sodium aluminosilicate hydrate gels: the cross-linked substituted to bermorite model10.1021/la4000473 ↗
46. Concrete properties comparison when substituting a 25% cement with slag from different provenances10.3390/ma11061029 ↗
47. Alkali activated materials
48. Geopolymers and related alkali-activated materials10.1146/annurev-matsci-070813-113515 ↗
49. Advances in understanding alkali-activated materials10.1016/j.cemconres.2015.04.013 ↗
50. Use of low CaO unprocessed steel slag in concrete as fine aggregate10.1016/j.conbuildmat.2008.06.003 ↗
51. Mechanical properties and constitutive model of geopolymer lightweight aggregate concrete10.3390/buildings15010098 ↗
52. The calcium silicate hydrates10.1016/j.cemconres.2007.11.005 ↗
53. A cost-effective slag-based mix activated with soda ash and hydrated lime: a pilot study10.1061/ppscfx.sceng-1426 ↗
54. Ecological carbonated steel slag pervious concrete prepared as a key material of sponge city10.1016/j.jclepro.2020.120244 ↗
55. Effects of steel slag powder as a cementitious material on compressive strength of cement-based composite10.3390/min13070869 ↗
56. Stabilization/solidification of hazardous and radioactive wastes with alkali-activated cements10.1016/j.jhazmat.2006.05.008 ↗
57. New cements for the 21st century: the pursuit of an alternative to Portland cement10.1016/j.cemconres.2011.03.016 ↗
59. Development of newer composite cement through mechano-chemical activation of steel slag10.1016/j.conbuildmat.2020.121147 ↗
60. The properties of magnesium silicate hydrate prepared from the magnesium silicate minerals in the Earth’s crust10.3390/buildings14051188 ↗
61. 2005
62. 2007
63. 2011
64. Gradual transformation of Ca(OH)2 into CaCO3 on cement hydration: XRD study10.1007/s10973-006-7840-7 ↗
65. Hydration properties and microstructure characteristics of alkali-activated steel slag10.1016/j.conbuildmat.2020.118141 ↗
66. Calorimetric studies of alkali-activated blast-furnace slag cements at early hydration processes in the temperature range of 20–80° C10.3390/ma14195872 ↗
67. Effect of different environments’ conditioning on the debonding phenomenon in fiber-reinforced cementitious matrix-concrete joints10.3390/ma14247566 ↗
68. Effect of diethanol-isopropanolamine and typical supplementary cementitious materials on the hydration mechanism of BOF slag cement pastes10.3390/buildings14051268 ↗
69. Mechanical performance optimization and microstructural mechanism study of alkali-activated steel slag–slag cementitious materials10.3390/buildings14051204 ↗
70. Recycle of steel slag as cementitious material and fine aggregate in concrete: mechanical, durability property and environmental impact10.1007/s11356-024-34746-0 ↗
71. Axial performance of seawater sea-sand concrete columns reinforced with basalt fibre-reinforced polymer bars under concentric compressive load10.1016/j.jobe.2021.103828 ↗
72. Experimental investigation of basic oxygen furnace slag used as aggregate in asphalt mixture10.1016/j.jhazmat.2006.02.073 ↗
73. The preparation of ground blast furnace slag-steel slag pavement concrete using different activators and its performance investigation10.3390/buildings13071590 ↗
74. An overview of utilization of steel slag10.1016/j.proenv.2012.10.108 ↗
75. The influence of steel slag and ferronickel slag on the properties of alkali-activated slag mortar10.1016/j.conbuildmat.2019.07.340 ↗
76. Nano-silica and silica fume modified cement mortar used as surface protection material to enhance the impermeability10.1016/j.cemconcomp.2018.05.012 ↗
77. Effects of lime powder on the properties of Portland cement–sulphoaluminate cement composite system at low temperature10.3390/ma17153658 ↗
78. Influence of different activators on microstructure and strength of alkali-activated nickel slag cementitious materials10.1016/j.conbuildmat.2019.117449 ↗
79. Hydration and mechanical properties of cement-steel slag system incorporating different activators10.1016/j.conbuildmat.2022.129981 ↗
80. Comparative research on the effect of various mineral admixtures on the early hydration process of cement10.1016/j.conbuildmat.2021.124372 ↗
81. Mechanical properties and microscopic mechanism of a multi-cementitious system comprising cement, fly ash, and steel slag powder10.3390/ma16227195 ↗
82. Hydration mechanisms of composite binders containing phosphorus slag at different temperatures10.1016/j.conbuildmat.2017.04.202 ↗
83. Mechanical properties and durability of alkali-activated steel slag–blastfurnace slag cement10.1007/s42243-023-01003-6 ↗
84. Study on the mechanical properties and hydration behavior of steel slag–red mud–electrolytic manganese residue based composite mortar10.3390/app13105913 ↗
85. Inhibition mechanisms of steel slag on the early-age hydration of cement10.1016/j.cemconres.2020.106283 ↗