Vickers Indentation Cracking of Ion-Exchanged Glasses: Quasi-Static vs. Dynamic Contact
Source abstract
Abstract
The indentation deformation and cracking responses of ion-exchanged glasses were measured using quasi-static and dynamic loading cycles. Two glass types were compared, a normal glass that deforms to a large extent by a shearing mechanism and a damage resistant glass that comparatively deforms with less shear and more densification. The quasi-static indentation cracking threshold for median/radial cracks for the ion-exchanged normal glass was determined to be 7 kilograms force (kgf), while the ion-exchanged damage resistant glass required loads exceeding 30 kgf. The increased cracking threshold of the damage resistant glass composition is attributed to the deformation mechanism, i.e. deformation with greater densification/less shear results in less subsurface damage and less residual stress. Both glass types were also subjected to dynamic indentation where the contact event time was more than 10,000 times shorter than the quasi-static condition. Under dynamic loading conditions, the cracking thresholds of the ion-exchanged normal and damage resistant glasses increased to greater than 50 kgf and greater than 150 kgf, respectively. The stress induced optical retardation was compared for quasi-static and dynamic indents made at sub-cracking threshold loads for both glasses. For indents made at the same sub-cracking threshold load in the normal glass, optical retardation mapping indicates less residual stress surrounding dynamic indents when compared to quasi-static indents. This suggests a rate dependence on the deformation mechanism in normal glasses with higher rates promoting densification in favor of shear. However, for damage resistant glass, the stress induced optical retardation is the same for indents made at both quasi-static and dynamic indentation rates.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Glass properties and applications · Advanced ceramic materials synthesis · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Indentation deformation/fracture of normal and anomalous glasses10.1016/0022-3093(79)90154-6 ↗
2. Barefoot · 2013
3. Properties and structure of vitreous silica I10.1016/0022-3093(70)90190-0 ↗
4. “A review of glass strength,”
5. The capillary force in micro- and nano-indentation with different indenter shapes10.1016/j.ijsolstr.2008.01.014 ↗
6. Direct observation and analysis of indentation cracking in glasses and ceramics10.1111/j.1151-2916.1990.tb05119.x ↗
7. Dejneka · 2012
8. Dejneka · 2014
9. Pressure-induced structural changes in a borosilicate glass-forming liquid: boron coordination, non-bridging oxygens, and network ordering10.1016/j.jnoncrysol.2004.03.115 ↗
10. Role of densification in deformation of glasses under point loading10.1111/j.1151-2916.1968.tb13318.x ↗
11. Mechanical properties of glass10.1016/0022-3093(77)90096-5 ↗
12. Poisson’s ratio and modern materials10.1038/nmat3134 ↗
13. Irreversible structural changes in vitreous B2O3 under pressure10.1103/PhysRevB.54.152 ↗
14. Deformation and cracking behavior of glasses indented with diamond tips of various sharpness10.1016/j.jnoncrysol.2012.01.052 ↗
15. “Low modulus, damage resistant glass for ultra-thin applications,”10.1002/9781118946404.ch3 ↗
16. Cone cracks around Vickers indentations in fused silica glass10.1007/BF00589840 ↗
17. Shear deformation under pyramidal indentations in soda-lime glass10.1007/BF00752121 ↗
18. The origin of median and lateral cracks around plastic indents in brittle materials10.1088/0022-3727/11/15/007 ↗
19. Plastic processes in a range of soda-lime silica glasses
20. “Sources of weakness and the ultimate strength of brittle amorphous solids,”
21. Microhardness of SiO2 glass in various environments10.1111/j.1151-2916.1987.tb05683.x ↗
22. Effect of B2O3 content on crack initiation under Vickers indentation test10.2109/jcersj2.118.792 ↗
23. Indentation behavior of soda-lime silica glass, fused silica, and single crystal quartz at liquid nitrogen temperature10.1111/j.1151-2916.1995.tb08241.x ↗
24. Kinetics of shear-activated indentation crack initiation in soda-lime glass10.1007/BF00547596 ↗
25. High pressure effects on oxide glasses: I, densification in rigid state10.1111/j.1151-2916.1963.tb13776.x ↗
26. Hardness and low-temperature deformation of silica glass10.1007/BF00757906 ↗
27. Densification and flow phenomena of glass in indentation experiments10.1016/0022-3093(70)90188-2 ↗
28. The strength and weakness of brittle materials
29. 69.3: A mechanics framework for ion-exchanged cover glass with a deep compression layer10.1889/1.3256467 ↗
30. Driving force of indentation cracking in glass: composition, pressure and temperature dependence10.1098/rsta.2014.0140 ↗
31. Stress corrosion and static fatigue of glass10.1111/j.1151-2916.1970.tb15962.x ↗
32. Structural response of a highly viscous aluminoborosilicate melt to isotropic and anisotropic compressions10.1063/1.3223282 ↗
33. Acoustic and elastic properties of glass in the Na2O-Al2O3-SiO2 system
34. Elastic stress fields caused by indenting brittle materials10.1080/01418618208236917 ↗
35. Quantitative evaluation of indentation-induced densification in glass10.1557/JMR.2005.0418 ↗