Role of Vanadium Carbide in Hydrogen Embrittlement of Press-Hardened Steels: Strategy From 1500 to 2000 MPa
Source abstract
Abstract
This work investigated hydrogen trapping and hydrogen embrittlement (HE) in two press-hardened steels, 22MnB5 for 1,500 MPa grade and 34MnB5V for 2000 MPa grade, respectively. Superior to the 22MnB5 steel, the newly developed 34MnB5V steel has an ultimate tensile strength of over 2000 MPa without sacrificing ductility due to the formation of vanadium carbides (VCs). Simulated press hardening was applied to two steels, and hydrogen was induced by cathodic charging. Susceptibility to HE was validated by slow strain-rate tensile test. When hydrogen content was high, the 34MnB5V steel fractured in elastic regime. However, when hydrogen content was 0.8–1.0 ppmw, the 34MnB5V steel bore much higher stress than the 22MnB5 steel before fracture. The behavior of hydrogen trapping was investigated by thermal desorption analyses. Although the two steels trapped similar amounts of hydrogen after cathodic charging, their trapping mechanisms and effective trapping sites were different. In summary, a finer prior austenite grain size due to the pinning effect of VCs can also improve the toughness of 34MnB5V steel. Moreover, trapping hydrogen by grain boundary suppresses the occurrence of hydrogen-enhanced local plasticity. Microstructural refinement enhanced by VCs improves the resistance to HE in 34MnB5V steel. Importantly, the correlation between hydrogen trapping by VCs and improvement of HE is not significant. Hence, this work presents the challenge in designing irreversible trapping sites in future press-hardened steels.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Hydrogen trapping behavior in vanadium-added steel10.2355/isijinternational.43.527 ↗
2. Baker · 1959
3. Prevention of hydrogen embrittlement in steels10.2355/isijinternational.ISIJINT-2015-430 ↗
4. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
5. Driving force and logic of development of advanced high strength steels for automotive applications10.1002/srin.201200288 ↗
6. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
7. Warm ductility enhanced by austenite reversion in ultrafine-grained duplex steel10.1016/j.actamat.2018.01.060 ↗
8. Influence of vanadium on the hydrogen embrittlement of aluminized ultra-high strength press hardening steel10.1016/j.msea.2018.08.027 ↗
9. Hydrogen absorption and embrittlement of ultra-high strength aluminized press hardening steel10.1016/j.msea.2018.08.003 ↗
10. Hydrogen trapping phenomena in carbon steel10.1007/BF00540409 ↗
11. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
12. Hydrogen embrittlement of low carbon structural steel10.1016/j.mspro.2014.06.190 ↗
13. Hydrogen solubility, diffusivity and trapping in a tempered Fe–C–Cr martensitic steel under various mechanical stress states10.1016/j.msea.2011.11.084 ↗
14. Absorption/desorption of diffusible hydrogen in aluminized boron steel10.2355/isijinternational.53.1295 ↗
15. Effect of dislocation trapping on hydrogen and deuterium diffusion in iron10.2320/matertrans1960.28.368 ↗
16. Hydrogen-induced embrittlement of nickel-chromium-molybdenum containing HSLA steels10.1080/02533839.2019.1676659 ↗
17. New protocol for orientation reconstruction from martensite to austenite in steels10.1016/j.mtla.2019.100554 ↗
18. Press hardening steel (PHS): a new coating and process tech nology
19. Results of further X-ray structural investigations of the iron–carbon and iron–nitrogen systems and of related interstitial alloys10.1107/S0365110X50001075 ↗
20. Development of niobium alloyed press hardening steel with improved properties for crash performance10.4028/www.scientific.net/AMR.1063.7 ↗
21. Effects of Al-Si coating and Zn coating on the hydrogen uptake and embrittlement of ultra-high strength press-hardened steel10.1016/j.surfcoat.2019.06.047 ↗
22. II. On some remarkable changes produced in iron and steel by the action of hydrogen and acids10.1098/rspl.1874.0024 ↗
23. Effects of prior austenite grain size on hydrogen delayed fracture of hot-stamped boron martensitic steel10.1007/s11661-019-05523-3 ↗
24. Effects of titanium content on hydrogen embrittlement susceptibility of hot-stamped boron steels10.1016/j.jallcom.2017.12.004 ↗
25. Martensite in steel: strength and structure10.1016/S0921-5093(99)00288-9 ↗
26. Deep trapping states for hydrogen in deformed iron10.1016/0001-6160(80)90038-3 ↗
27. Über den Mechanismus der Stahlhӓrtung10.1007/BF01397346 ↗
28. Hydrogen trapping by TiC particles in iron10.1016/0001-6160(84)90210-4 ↗
29. Effects of vanadium carbides on hydrogen embrittlement of tempered martensitic steel10.1007/s12540-016-5631-7 ↗
30. Effect of niobium precipitation behavior on microstructure and hydrogen induced cracking of press hardening steel 22MnB510.1016/j.msea.2018.02.021 ↗
31. Response of hydrogen desorption and hydrogen embrittlement to precipitation of nanometer-sized copper in tempered martensitic low-carbon steel10.1007/s11837-019-03330-0 ↗
32. Hydrogen trapping and desorption of dual precipitates in tempered low-carbon martensitic steel10.1016/j.actamat.2020.06.046 ↗
33. New approaches in understanding the effects of hydrogen trapping and the fishscaling resistance of enameled steels10.1016/j.surfcoat.2020.126135 ↗
34. Alloy optimization for reducing delayed fracture sensitivity of 2000 MPa press hardening steel10.3390/met10070853 ↗
35. Hydrogen detrapping from grain boundaries and dislocations in high purity iron10.1016/0956-7151(92)90436-I ↗
36. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
37. A quantitative analysis of hydrogen trapping10.1007/BF02661939 ↗
38. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
39. Influence of traps on the deuterium behaviour in the low activation martensitic steels F82H and Batman10.1016/S0022-3115(97)00021-4 ↗
40. Fracture surface topography analysis of the hydrogen-related fracture propagation process in martensitic steel10.1007/s10704-017-0182-6 ↗
41. Grains, phases, and interfaces:An introduction of microstructure10.1007/s11661-010-0215-5 ↗
42. Theory for hydrogen desorption in ferritic steel10.1016/j.commatsci.2013.06.008 ↗
43. Mechanisms of hydrogen-enhanced localized plasticity: an atomistic study using α-Fe as a model system10.1016/j.actamat.2014.01.008 ↗
44. The first direct observation of hydrogen trapping sites in TiC precipitation-hardening steel through atom probe tomography10.1016/j.scriptamat.2010.03.012 ↗
45. Direct observation of hydrogen-trapping sites in vanadium carbide precipitation steel by atom probe tomography10.1016/j.scriptamat.2012.04.022 ↗
46. Correlation between vanadium carbide size and hydrogen trapping in ferritic steel10.1016/j.scriptamat.2018.04.013 ↗
47. The effect of dislocation contrast on x‐ray line broadening: a new approach to line profile analysis10.1063/1.117951 ↗
48. Molybdenum alloying in high-performance flat-rolled steel grades10.1007/s40436-019-00285-y ↗
49. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
50. Nano-preciptates design with hydrogen trapping character in high strength steel10.1007/978-3-642-17665-4_11 ↗
51. Precise determination of the activation energy for desorption of hydrogen in two Ti-added steels by a single thermal-desorption spectrum10.1007/s11663-004-0057-x ↗
52. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
53. The dislocation density of acicular ferrite in steel welds
54. Interphase precipitation of nanometer-sized carbides in a titanium-molybdenum-bearing low-carbon steel10.1016/j.actamat.2011.06.037 ↗
55. Interactions between deformation-induced defects and carbides in a vanadium-containing TWIP steel10.1016/j.scriptamat.2012.02.002 ↗
56. Yi · 2018
57. Effects of niobium and vanadium on hydrogen-induced delayed fracture in high strength spring steel10.1016/S1006-706X(11)60077-0 ↗
58. Effect of Nb on hydrogen-induced delayed fracture in high strength hot stamping steels10.1016/j.msea.2014.12.051 ↗
59. Effect of Nb–Ti multi-microalloying on the hydrogen trapping efficiency and hydrogen embrittlement susceptibility of hot-stamped boron steel10.1016/j.msea.2019.138788 ↗