journal article·2019-05-07Open access

Silica Fume as Precursor in the Development of Sustainable and High-Performance MK-Based Alkali-Activated Materials Reinforced With Short PVA Fibers

Raquel P. Batista, Ana Carolina C. Trindade, Paulo H. R. Borges, Flávio de A. Silva

Abstract

Alkali-activated materials (AAM) are currently the subject of increasing interest and research, mainly due to the possibility to reduce the carbon dioxide (CO2) emissions in their production when compared to Portland cement (PC) and still achieve superior performance in many aspects when compared to traditional PC-based products. However, the use of sodium silicate (SS) as an alkaline activator in AAM is controversial when the aim is to reduce the environmental impact, as the production of the first also releases significant amount of CO2 per ton of activator produced. Therefore, a demand has emerged for alternative silica-rich materials that could effectively reduce the demand for SS without compromising the mechanical behaviour of the matrices and consequently the performance of fibre reinforced AAM. This paper investigates the gradual replacement (0% to 18% wt.) of metakaolin (MK) with silica fume (SF) in PVA-reinforced AAM, allowing the reduction of SS in the activator, also containing NaOH. Matrices with different composition were studied, i.e. with [SiO2]/[Al2O3] molar ratios of 3.0 and 3.8. All formulations were reinforced with 2% vol. of PVA fibres. The mechanical properties investigated were compressive strength, modulus of elasticity, flexural strength and toughness. Apparent dry density, water absorption and porosity of the composites were also assessed to give an indication of their durability. Single fibre pullout, fracture toughness and direct tensile tests were also carried out in order to understand the deformation capability of the composites. Results indicated that the employment of SF may effectively reduce the demand for SS in the alkaline activators, in order to produce alkali-activated composites with lower environmental impact (reduced CO2 emissions). Adjustments in the formulations may improve toughness in flexion in 170% with 30 wt.% reduction of SS in the activator, as well as improvements in deformation capability in tension. The development of strain-hardening MK-based AAM, however, has some challenging aspects that are also discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. ASTM C293 - 02 · 2002
2. NBR 7215 - Cimento Portland - Determinação da Resistência à Compressão · 1996 · 1
3. NBR 13276 - Argamassa Para Assentamento e Revestimento de Paredes e Tetos - Determinação do Índice de Consistência · 2016
4. NBR 8522 - Concreto - Determinação dos Módulos Estáticos de Elasticidade e de Deformação à Compressão · 2017
5. Silica fume-sodium hydroxide binding systems10.1016/S0008-8846(97)00192-0 ↗
6. Resistance of alkali-activated slag concrete to acid attack10.1016/S0008-8846(03)00125-X ↗
7. Resistance of alkali-activated slag concrete to alkali–aggregate reaction10.1016/S0008-8846(00)00483-X ↗
8. Resistance of alkali-activated slag concrete to carbonation10.1016/S0008-8846(01)00574-9 ↗
9. Sulfate attack on alkali-activated slag concrete10.1016/S0008-8846(01)00659-7 ↗
10. Bentur · 2007
11. Other potential applications for alkali-activated materials10.1007/978-94-007-7672-2_12 ↗
12. Activation of metakaolin/slag blends using alkaline solutions based on chemically modified silica fume and rice husk ash10.1007/s12649-011-9093-3 ↗
13. Mechanical properties Mk-based geopolymer composites reinforced with
14. Engineering properties of alkali activated natural pozzolan concrete
15. Effect of SiO2/Al2O3 molar ratio on mechanical behavior and capillary sorption of MK-based alkali-activated composites reinforced with PVA fibers10.1617/s11527-017-1021-y ↗
16. Estudo comparativo da análise de ciclo de vida de concretos geopoliméricos e de concretos à base de cimento Portland composto (CP II)10.1590/S1678-86212014000200011 ↗
17. Properties of geopolymer cements
18. Geopolymer technology: the current state of the art10.1007/s10853-006-0637-z ↗
19. Effect of alkali cations on aluminum incorporation in geopolymeric gels10.1021/ie0494216 ↗
20. Crucial insights on the mix design of alkali-activated cement-based binders10.1533/9781782422884.1.49 ↗
21. Advances in alternative cementitious binders10.1016/j.cemconres.2010.11.012 ↗
22. Substitution of sodium silicate with rice husk ash-NaOH solution in metakaolin based geopolymer cement concerning reduction in global warming10.1016/j.jclepro.2016.10.164 ↗
23. Practical design criteria for saturated pseudo strain hardening behavior in ECC10.3151/jact.4.59 ↗
24. Mechanical strength and Young's modulus of alkali-activated cement-based binders10.1533/9781782422884.2.171 ↗
25. Potential of geopolymer technology towards green buildings and sustainable cities10.1016/j.proeng.2011.11.2108 ↗
26. Damage behavior of geopolymer composites exposed to elevated temperatures10.1016/j.cemconcomp.2008.08.001 ↗
27. Comparative performance of geopolymers made with metakaolin and fly ash after exposure to elevated temperatures10.1016/j.cemconres.2007.08.021 ↗
28. Strain hardening fiber reinforced alkali-activated mortar – A feasibility study10.1016/j.conbuildmat.2012.06.007 ↗
29. Steady-state and multiple cracking of short random fiber composites10.1061/(ASCE)0733-9399(1992)118:11(2246) ↗
30. Tensile strain-hardening behavior of polyvinyl alcohol engineered cementitious composite (PVA-ECC)10.14359/10851 ↗
31. Interface tailoring for strain-hardening Polyvinyl Alcohol-engineered cementitious composite (PVA-ECC)10.14359/12325 ↗
32. Short fiber reinforced geopolymer composites manufactured by extrusion10.1061/(ASCE)0899-1561(2005)17:6(624) ↗
33. Geopolymer concrete: a review of development and opportunities
34. Behaviour of strain-hardening cement-based composites under high strain rates10.3151/jact.9.51 ↗
35. Micromechanics constitutive modelling and optimization of strain hardening geopolymer composite10.1016/j.ceramint.2017.01.138 ↗
36. Comparative deflection hardening behavior of short fiber reinforced geopolymer composites10.1016/j.conbuildmat.2014.07.085 ↗
37. Tensile strain hardening behavior of PVA fiber-reinforced engineered geopolymer composite10.1061/(ASCE)MT.1943-5533.0001242 ↗
38. Nanoindentation characteristics of alkali-activated aluminosilicate materials10.1016/j.cemconcomp.2010.10.005 ↗
39. Advancing the use of secondary inputs in geopolymer binders for sustainable cementitious composites: a review10.3390/su3020410 ↗
40. A feasibility study of strain hardening fiber reinforced fly ash-based geopolymer composites10.1016/j.conbuildmat.2014.02.005 ↗
41. OliveiraA. M. Fluência a Altas Temperaturas, Aderência Fibra-Matriz E Comportamento Mecânico Sob Ações Higrotérmicas De Compósitos Cimentí2015
42. Utilization of mining wastes to produce geopolymer binders10.1533/9781845696382.2.267 ↗
43. Durability and testing-physical processes10.1007/978-94-007-7672-2_10 ↗
44. The role of mathematical modelling and gel chemistry in advancing geopolymer technology10.1205/cherd.04329 ↗
45. Nanostructure/microstructure of metakaolin geopolymers10.1533/9781845696382.1.72 ↗
46. Mechanical and durable behaviour of alkaline cement mortars reinforced with polypropylene fibres10.1016/S0008-8846(03)00222-9 ↗
47. Use of glass waste as an activator in the preparation of alkali-activated slag. Mechanical strength and paste characterisation10.1016/j.cemconres.2013.12.005 ↗
48. Measuring and modifying interface properties of PVA fibers in ECC matrix10.1061/(asce)0899-1561(2001)13:6(399) ↗
49. CPC 11.3. Absorption d'eau par immersion sous vide [Absorption of water by immersion under vacuum]10.1007/BF02478713 ↗
50. RILEM Draft Recommendation TC 89-FMT (Fracture Mechanics of Concrete - Test Methods): determination of fracture parameters of plain concrete using three-point bend tests10.1007/B.F.02472029 ↗
51. Effect of nanosilica-based activators on the performance of an alkali-activated fly ash binder10.1016/j.cemconcomp.2012.08.025 ↗
52. Silica fume-basic blast furnace slag systems activated by an alkali silica fume activator10.1016/S0008-8846(97)00191-9 ↗
53. Reinforced geopolymer composites for enhanced material greenness and durability10.1016/j.scs.2011.07.009 ↗
54. Deflection hardening behaviour of short fibre reinforced fly ash based geopolymer composites10.1016/j.matdes.2013.03.063 ↗
55. StavrinidesG. LondonUniversity College LondonAlternative Cements in Concrete Construction: Assessment, Prospects and Commercialisation Strategies2010
56. Geopolymer binders from metakaolin using sodium waterglass from waste glass and rice husk ash as alternative activators: a comparative study10.1016/j.conbuildmat.2016.03.184 ↗
57. Waste glass in the geopolymer preparation. Mechanical and microstructural characterisation10.1016/j.jclepro.2014.11.074 ↗
58. High strength geopolymer binder based on waste-glass powder10.1016/j.apt.2016.09.034 ↗
59. Chemical research and climate change as drivers in the commercial adoption of alkali activated materials10.1007/s12649-010-9015-9 ↗
60. Engineered cementitious composites with high-volume fly ash10.14359/18668 ↗
61. Understanding the drying shrinkage performance of alkali-activated slag mortars10.1016/j.cemconcomp.2016.11.010 ↗
62. Possibilities of a novel use of silica fume in mineral binding systems10.1016/S0950-0618(99)00028-8 ↗
63. High effective silica fume alkali activator10.1007/BF02708502 ↗
64. Effectiveness of new silica fume alkali activator10.1016/j.cemconcomp.2005.07.004 ↗