Deterioration laws of concrete durability under the coupling action of salt erosion and drying–wetting cycles

Shaojie Chen, Jianxi Ren, Xiang Ren, Yugen Li

Abstract

To investigate the deterioration laws of concrete durability under the coupling action of salt erosion and drying–wetting cycles, this study evaluated the macro–performance evolution of concrete under different environments (NaCl, Na2SO4, and MgSO4). Several measuring methods including nuclear magnetic resonance, computerized tomography tests, and microscopic morphology analysis are employed to investigate the damage mechanism of concrete. Experimental results show that with the action of salt erosion and drying–wetting cycles, the mass loss rate of concrete decreased first and then increased, and the relative dynamic modulus of elasticity and the compressive strength increased first and then decreased. The porosity and the pore quantity fluctuation increased. During the whole erosion process, needle-like attack products were formed in the pores, the crystals gradually filled the pores, and generated expansion pressure on the pore wall. As a result, concrete damage gradually occurred. Consequently, the damage degree was greater. The degrees of concrete damage under drying–wetting cycles induced were arranged as MgSO4>Na2SO4>NaCl.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Durabilidad del hormigón armado expuesto a condiciones agresivas10.3989/mc.2013.00313 ↗
2. Service life prediction and performance testing — current developments and practical applications10.1016/j.cemconres.2015.05.013 ↗
3. Potential accelerated test methods for physical sulfate attack on concrete10.1016/j.conbuildmat.2019.116920 ↗
4. Lab and field study of physical sulfate attack on concrete mixtures with supplementary cementitious materials10.1061/(ASCE)MT.1943-5533.0003500 ↗
5. Impact of chloride on the mineralogy of hydrated Portland cement systems10.1016/j.cemconres.2010.03.002 ↗
6. Performance-based approaches for concrete durability: State of the art and future research needs10.1016/j.cemconres.2019.01.003 ↗
7. Life prediction of reinforced concrete in saline soil based on wiener stochastic process [J]10.15961/j.jsuese.202000275 ↗
8. Experiment study on the failure mechanism of dry-mix shotcrete under the combined actions of sulfate attack and drying–wetting cycles10.1016/j.conbuildmat.2015.02.007 ↗
9. Concrete deformation and interior humidity during dry-wet cycles [J]10.16511/j.cnki.qhdxxb.2012.02.009 ↗
10. Volume absorption rate of non air-entrained concrete in different salt solution during freeze-thaw process [J]10.3969/j.issn.1001-6864.2011.01.002 ↗
11. Effect of dry–wet ratio on properties of concrete under sulfate attack10.3390/ma12172755 ↗
12. Ultrasonic testing and microscopic analysis on concrete under sulfate attack and cyclic environment10.1007/s11771-014-2482-6 ↗
13. Mechanism of concrete destruction under sodium sulfate and magnesium sulfate solution [J]10.3321/j.issn:0454-5648.2007.04.022 ↗
14. Grey model research based on the pore structure fractal and strength of NMR aeolian sand lightweight aggregate concrete10.1007/s11837-019-03887-w ↗
15. An accelerated sulfate resistance test for concrete10.1617/s11527-015-0731-2 ↗
16. Invading track of chloride ions in cemented-based materials10.1007/s11771-010-0040-4 ↗
17. Study on concrete structure’s durability considering the interaction of multi-factors10.1016/j.conbuildmat.2016.05.032 ↗
18. Experimental study on pore characteristics of different coarse aggregate concrete based on NMR technique [J]10.3969/j.issn.1001-9731.2017.10.011 ↗
19. Damage to recycled concrete with different aggregate substitution rates from the coupled action of freeze-thaw cycles and sulfate attack10.1016/j.conbuildmat.2019.06.060 ↗
20. The damage mechanism and failure prediction of concrete under wetting–drying cycles with sodium sulfate solution10.1016/j.conbuildmat.2020.120525 ↗
21. Physical salt attack on concrete: Mechanisms, influential factors, and protection [J]10.14359/51727015 ↗
22. Investigation on meso-debonding process of the sandstone–concrete interface induced by freeze–thaw cycles using NMR technology10.1016/j.conbuildmat.2020.118962 ↗
23. Assessment of the long-term performance of SCC incorporating different mineral admixtures in a magnesium sulphate environment10.1016/j.conbuildmat.2015.01.067 ↗
24. Sulfate durability and leaching behaviour of dry- and wet-mix shotcrete mixes10.1016/j.cemconres.2020.106180 ↗
25. Evaluation of damage in concrete suffered freeze-thaw cycles by CT technique10.3151/jact.14.679 ↗
26. Fly ash slag geopolymer concrete: Resistance to sodium and magnesium sulfate attack10.1061/(ASCE)MT.1943-5533.0001618 ↗
27. Effects of deicing salts on the scaling resistance of concrete10.1061/(ASCE)MT.1943-5533.0001106 ↗
28. An approach to the recent trends of concrete science and technology [J]10.14062/j.issn.0454-5648.1979.03.010 ↗
29. Effect of mineral admixtures on durability of concrete in wetting-drying cyclic sulfate environment [J]10.3321/j.issn:0454-5648.2009.10.031 ↗
30. Interior humidity of concrete under dry-wet cycles10.1061/(ASCE)MT.1943-5533.0000382 ↗
31. The influence of admixture on chloride time-varying diffusivity and microstructure of concrete by low-field NMR10.1016/j.oceaneng.2017.06.065 ↗
32. Damage of concrete in sulfate and chloride solution [J]10.3321/j.issn:0454-5648.2006.05.025 ↗