Coarsening Evolution of γ′ Phase and Failure Mechanism of Co-Ni-Al-Ti-Based Superalloys During Isothermal Aging
Source abstract
Abstract
Novel Co-based superalloys, as potentially ideal aero-engine hot section materials, have a higher temperature bearing capacity and better oxidation resistance than Ni-based superalloys. Coarsening evolution of γ′ phase and failure mechanism of Co-Ni-Al-Ti-based superalloys during the isothermal aging process at 1073 K were investigated using multiple characterizations and testing methods. The results show that γ′ phase is uniformly distributed on the γ phase matrix, and coarsening with the increase in isothermal aging time, which results in a decrease in maximum tensile strength. Furthermore, Mo element is preferred to distribute in γ′ phase and provides stronger solution strengthening effect than Cr element, which determines more excellent mechanical properties of 2Mo superalloy than that of 2Cr superalloy. The coarsening rate of γ′ phase in the 2Cr superalloy is significantly higher than that in the 2Mo superalloy. Grain boundary failure is dominant in isothermal aging, and the cracks nucleate and expand along the vertical direction of loading stress on the grain boundary. The current work suggests that the coarsening of the γ′ phase, reduction in the volume fraction of γ′ phase, and formation of ′-precipitate depleted zone (PDZ) near the grain boundary during aging controls the deterioration of mechanical properties in Co-Ni-Al-Ti-based superalloys.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Advanced Materials Characterization Techniques · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Kinetics Pathway of Precipitation in Model Co-Al-W Superalloy10.1016/j.actamat.2017.12.032 ↗
2. Phase-Field Simulation of γʹ Coarsening Behavior in Cobalt-Based Superalloy10.1016/j.commatsci.2021.110358 ↗
3. Development of Low-Density γ/γ′ Co-Al-Ta-Based Superalloys with High Solvus Temperature10.1016/j.actamat.2020.02.049 ↗
4. Effect of Cr on the Microstructure and Oxidation Properties of Co-Al-W Superalloys Studied by In Situ Environmental TEM10.1016/j.corsci.2019.108179 ↗
5. On the Possibility of Simultaneously Achieving Sufficient Oxidation Resistance and Creep Property at High Temperatures Exceeding 1000 °C in Co-Based Superalloys10.1016/j.jallcom.2020.157724 ↗
6. Effects of Cr on the Properties of Multicomponent Cobalt-Based Superalloys with Ultra High γ' Volume Fraction10.1016/j.jallcom.2020.154790 ↗
7. Cyclic Oxidation Behavior of Al-Si Coating on New γ′-Strengthened Cobalt-Based Superalloy: Experimental Study and First-Principles Calculation10.1016/j.corsci.2021.109422 ↗
8. Co-Strengthening of Dislocations and Precipitates in Alumina-Forming Austenitic Steel with Cold Rolling Followed by Aging10.1016/j.msea.2021.142181 ↗
9. Effects of Alloying Elements on Microstructure and Mechanical Properties of Co-Ni-Al-Ti Superalloy10.1016/j.msea.2020.139139 ↗
10. High-Temperature Oxidation Behavior of Modified 4Al Alumina-Forming Austenitic Steel: Effect of Cold Rolling10.1016/j.jmst.2020.08.013 ↗
11. Effect of Cu Addition on Microstructure and Properties of Fe-20Ni-14Cr Alumina-Forming Austenitic Steel10.1016/j.intermet.2021.107312 ↗
12. Isothermal Oxidation Behavior of W‐Free Co-Ni-Al‐Based Superalloy at High Temperature10.1002/maco.202112789 ↗
13. Environmental Embrittlement and Other Causes of Brittle Grain Boundary Fracture in Ni3Al10.1016/0921-5093(94)03236-x ↗
14. Effect of Microstructure on Temperature Dependence of Deformation Behavior in Polycrystalline CoNi-Based Superalloy10.1007/s10853-021-06582-x ↗
15. Investigation on γ′ Stability in CoNi-Based Superalloys during Long-Term Aging at 900 °C10.1016/j.jallcom.2020.155891 ↗
16. Precipitation and Coarsening Behavior of γ′ Phase in CoNi-Base Superalloy under Different Aging Treatments10.1016/j.vacuum.2020.109247 ↗
17. The Effect of Isothermal Aging on Creep Behavior of Modified 2.5Al Alumina-Forming Austenitic Steel10.1016/j.msea.2020.140219 ↗
18. The Effect of Isothermal Aging on Microstructure and Mechanical Behavior of Modified 2.5Al Alumina-Forming Austenitic Steel10.1016/j.msea.2019.01.087 ↗
19. Coarsening Kinetics of Cuboidal Gamma Prime Precipitates in Single Crystal Nickel Base Superalloy CMSX-4
20. Microstructural Stability and Mechanical Behavior of a Co–20Ni–7Al–7W–4Ti at.% Superalloy10.1016/j.jallcom.2020.156378 ↗
21. Effects of Cr and Al/W Ratio on the Microstructural Stability, Oxidation Property and γ′ Phase Nano-Hardness of Multi-Component Co-Ni-Base Superalloys10.1016/j.jallcom.2020.154182 ↗
22. Rafting of γ′ Precipitates in a Co-9Al-9W Superalloy during Compressive Creep10.1016/j.msea.2018.02.017 ↗
23. Effects of Mo on the Evolution of Microstructures and Mechanical Properties in Co-Al-W Base Superalloys10.1016/j.msea.2018.11.087 ↗
24. Segregation-Assisted Phase Transformation and Anti-Phase Boundary Formation during Creep of a γ′-strengthened Co-Based Superalloy at High Temperatures10.1016/j.actamat.2021.117099 ↗
25. A New Tungsten-Free γ-γ' Co-al-Mo-Nb-Based Superalloy10.1016/j.scriptamat.2014.11.009 ↗
26. A New Class of High Strength High Temperature Cobalt Based γ-γ′ Co-Mo-Al Alloys Stabilized with Ta Addition10.1016/j.actamat.2015.06.034 ↗
27. Lattice Misfit Measurement in Inconel 706 Containing Coherent γ′ and γ″ Precipitates10.1016/S1359-6462(02)00456-6 ↗
28. Diffusion of Solutes in Fcc Cobalt Investigated by Diffusion Couples and First Principles Kinetic Monte Carlo10.1016/j.actamat.2016.01.028 ↗
29. Effect of Cr Additions on a γ-γ' Microstructure and Creep Behavior of a Co-Based Superalloy with Low W Content10.1016/j.msea.2020.139108 ↗
30. Shape Memory and Magnetic Properties of Co-Al Ferromagnetic Shape Memory Alloys10.1016/j.msea.2005.12.068 ↗
31. On the Effect of Ti Addition on Microstructural Evolution, Precipitate Coarsening Kinetics and Mechanical Properties in a Co-30Ni-10Al-5Mo-2Nb Alloy10.1016/j.mtla.2021.101072 ↗
32. Cobalt-Base High-Temperature Alloys10.1126/science.1121738 ↗
33. γ'-(L12) Precipitate Evolution during Isothermal Aging of a Co Al W Ni Superalloy10.1016/j.actamat.2018.11.014 ↗
34. Microstructural Evolution and High-Temperature Strength of a γ(f.c.c.)/γ'(L12) Co-Al-W-Ti-B Superalloy10.1016/j.actamat.2019.05.058 ↗
35. Thermophysical and Magnetic Properties of Co-Ni-Mo-Al-Ta Class of Tungsten Free Co-Based Superalloys10.1016/j.jallcom.2021.160379 ↗
36. Temperature Dependence of Thermodynamic Stability and Mechanical Property of Alloying Co3Ta Compounds10.1016/j.jallcom.2019.06.170 ↗
37. Effects of Al Content on Microstructures and High-Temperature Tensile Properties of Two Newly Designed CoNi-Base Superalloys10.1016/j.jallcom.2020.155337 ↗
38. Accelerating the Discovery of Novel γ/γ' Co-Based Superalloys by Probing Temperature and Alloying Effects on the γ' Precipitates10.1016/j.mtla.2021.101171 ↗
39. Plasticity-Induced Stacking Fault Behaviors of γ' Precipitates in Novel CoNi-Based Superalloys10.1016/j.jmst.2021.02.031 ↗
40. On the Microstructural Evolution and Partitioning Behavior of L12-Structured γ′-Based Co-Ti-W Alloys upon Cr and Al Alloying10.1016/j.intermet.2018.10.027 ↗
41. Diffusion Multiple Study of the Co-Fe-Ni System at 800 °C10.1016/j.calphad.2018.12.005 ↗
42. Mechanical Properties and Lattice Misfit of γ/γ′ Strengthened Co-base Superalloys in the Co-W-Al-Ti Quaternary System10.1016/j.intermet.2014.07.006 ↗
43. A Novel Type of Co-Ti-Cr-base γ/γ′ Superalloys with Low Mass Density10.1016/j.actamat.2017.06.024 ↗
44. Microstructure Evolution of Multicomponent γ′-Strengthened Co-Based Superalloy at 750 °C and 1000 °C with Different Al and Ti Contents10.1007/s11661-020-05652-0 ↗
45. Effects of Aluminum and Molybdenum Content on the Microstructure and Properties of Multi-Component γ′-Strengthened Cobalt-Base Superalloys10.1016/j.msea.2018.09.058 ↗
46. Effect of Mo on Microstructural Characteristics and Coarsening Kinetics of γ' Precipitates in Co-Al-W-Ta-Ti Alloys10.1016/j.jmst.2017.04.012 ↗
47. Abnormal Precipitation of the μ Phase during Solution Treatment of γ′-strengthened Co-Ni-Al-W-Based Superalloys10.1016/j.scriptamat.2020.02.010 ↗
48. Microstructures and Properties of a Novel γ′-strengthened Multi-Component CoNi-Based Wrought Superalloy Designed by CALPHAD Method10.1016/j.msea.2020.139219 ↗