Effect of microstructure on the mechanical properties and corrosion resistance of a welded joint of 620-grade marine steel

Yifan Dong, Denghui Liu, Hegang Du, Haoran Sun, Xiurong Zuo

Abstract

The relationship between the microstructure and the mechanical and corrosion properties of a welded joint of 620-grade marine steel was studied using metallographic microscopy, scanning electron microscopy, an energy dispersive spectrometer, transmission electron microscopy, and microhardness and tensile tests. The results showed that the strength and hardness of the weld center area (WMmid) were higher than those of the inner and outer welding surface region (WMin and WMout) because the volume fraction of the martensite-austenite (MA) constituents (21.6%) was higher than that in WMin and WMout (18.0% and 14.3%, respectively). There were numerous MnO-Al2O3-SiO2-TiO2-type inclusions located at the bottom of dimples in the fracture surface; however, the MA constituents took precedence over this kind of inclusion in inducing pitting corrosion. In contrast, pitting corrosion can be initiated by Al2O3-MgO-CaO-CaS inclusions in the heat-affected zone (HAZ) and base metal (BM). The corrosion resistance of the welded joint was in the order of weld metal > HAZ > BM. The WMmid with smaller dendrite spacing and a larger size of MA constituents had better corrosion resistance compared with the WMin and WMout. The corrosion resistance of the HAZ decreased in the sequence of coarse grain HAZ, fine grain HAZ, and intercritical HAZ.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Effect of normalization temperatures on ductile–brittle transition temperature of a modified 9Cr–1Mo steel10.1016/j.msea.2014.09.021 ↗
2. Comparative study of microstructure and mechanical properties of X80 SAW welds prepared using different wires and heat inputs10.1007/s11665-020-04986-5 ↗
3. Effect of plastic deformation on the electrochemical and stress corrosion cracking behavior of X70 steel in near-neutral pH environment10.1016/j.msea.2016.09.033 ↗
4. Correlation between microstructure and mechanical properties of welded joint of X70 submarine pipeline steel with heavy wall thickness10.3390/met12050716 ↗
5. Effects of Si, Mn on the corrosion behavior of ferritic–martensitic steels in supercritical water (SCW) environments10.1016/j.corsci.2020.108432 ↗
6. Pitting behavior and mechanism caused by Ca-Al-O-S composite inclusions in low-alloy steels10.1108/ACMM-05-2016-1675 ↗
7. Effects of solution pH and Cl-on electrochemical behaviour of an Aermet100 ultra-high strength steel in acidic environments10.1016/j.corsci.2011.08.024 ↗
8. Influence of martensite-austenite (MA) on impact toughness of X80 line pipe steels10.1016/j.msea.2016.03.095 ↗
9. Microstructure refinement and mechanical properties improvement by developing IAF on inclusions in Ti–Al complex deoxidized HSLA steel10.1016/j.matchar.2015.08.018 ↗
10. Effectiveness of an intercritical heat-treatment on localized corrosion resistance at the microstructural boundaries of medium-carbon steels10.1016/j.corsci.2019.04.019 ↗
11. Fuzzy logic analysis of parameters of dimples of ductile tearing on the digital image of fracture surface10.1016/j.proeng.2017.04.369 ↗
12. Operando electrochemical TEM, eEx-situ SEM and atomistic modeling studies of MnS dissolution and its role in triggering pitting corrosion in 304L stainless steel10.1016/j.corsci.2022.110184 ↗
13. Influence of the dissolution of MnS inclusions under free corrosion and potentiostatic conditions on the composition of passive films and the electrochemical behaviour of stainless steels10.1016/j.electacta.2005.09.015 ↗
14. Microstructure-based approach to the evaluation of welded joints of bainitic rails designed for high-speed railways10.1016/j.jcsr.2020.106372 ↗
15. Effect of welding heat input and post-weld thermal aging on the sensitization and pitting corrosion behavior of AISI 304L stainless steel butt welds10.1007/s11665-021-05454-4 ↗
16. Influence of peak temperature during in-service welding of API X70 pipeline steels on microstructure and fracture energy of the reheated coarse grain heat-affected zones10.1007/s10853-011-5592-7 ↗
17. In-situ EBSD study of deformation behaviour of 600 MPa grade dual phase steel during uniaxial tensile tests10.1016/j.msea.2019.05.083 ↗
18. Uniformity of passive films formed on ferrite and martensite by different inorganic inhibitors10.1016/S0010-938X(01)00178-0 ↗
19. Ex situ characterization of metallurgical inclusions in X100 pipeline steel before and after immersion in a neutral pH bicarbonate solution10.1016/j.jallcom.2016.02.224 ↗
20. Evaluation of mechanical properties and microstructure of X70 pipeline steel with strain-based design10.3390/met12101616 ↗
21. Pitting corrosion of steel induced by Al2O3 inclusions10.3390/met7090347 ↗
22. Creep behavior and microstructure evaluation of welded joint in dissimilar modified 9Cr–1Mo steels10.1016/j.msea.2015.07.068 ↗
23. Investigation of corrosion behavior of welded joint of X70 pipeline steel for deep sea10.11900/0412.1961.2017.00149 ↗
24. Stress corrosion cracking of E690 steel as a welded joint in a simulated marine atmosphere containing sulphur dioxide10.1016/j.corsci.2015.08.039 ↗
25. Comparative study on corrosion fatigue behaviour of high strength low alloy steel and simulated HAZ microstructures in a simulated marine atmosphere10.1016/j.ijfatigue.2020.105666 ↗
26. Study on effect of double austenitization treatment on fracture morphology tensile tested nuclear grade P92 steel10.1016/j.engfailanal.2018.09.036 ↗
27. Effect of creep phenomena on room-temperature tensile properties of cast & forged P91 steel10.1016/j.engfailanal.2017.05.025 ↗
28. Fatigue and failure of steel of offshore gas pipeline after the laying operation10.1016/j.acme.2016.03.003 ↗
29. Effect of pearlitic morphology with varying fineness on the cavitation erosion behavior of eutectoid rail steel10.1016/j.ultsonch.2020.105399 ↗
30. The influence of Ni content on the weldability, mechanical, and pitting corrosion properties of a high-nickel-bearing supermartensitic stainless steel10.1007/s11665-021-05600-y ↗
31. The effect of microstructure and non-metallic inclusions on corrosion behavior of low carbon steel in chloride containing solutions10.1016/j.corsci.2013.11.038 ↗
32. Influence of heat input on the pitting corrosion and tensile behavior of GTA welded martensitic stainless steel (AISI410 SS) joints10.1016/j.matpr.2020.12.187 ↗
33. Pitting corrosion inhibition of 304 stainless steel in NaCl solution by three newly synthesized carboxylic Schiff bases10.1016/j.corsci.2019.108130 ↗
34. Thermodynamics of chemical and electrochemical stability of corrosion active nonmetal inclusions10.1134/S0033173207010043 ↗
35. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
36. Role of inclusions in the pitting initiation of pipeline steel and the effect of electron irradiation in SEM10.1016/j.corsci.2017.10.029 ↗
37. Correlation between active/inactive (Ca, Mg, Al)-Ox-Sy inclusions and localised marine corrosion of EH36 steels10.1016/j.jmrt.2021.06.030 ↗
38. Corrosion resistance of the welded joint of submarine pipeline steel with ferrite plus bainite dual-phase microstructure10.1002/srin.201400309 ↗
39. Pitting and sulphide inclusions in steel10.1016/S0010-938X(74)80047-8 ↗
40. Enhanced interface strength in steel-nickel bimetallic component fabricated using wire arc additive manufacturing with interweaving deposition strategy10.1016/j.jmst.2020.04.019 ↗
41. Influence of QLT treatment on microstructure and mechanical properties of a high nickel steel10.1016/j.jmatprotec.2012.08.005 ↗
42. Challenge of mechanical properties of an acicular ferrite pipeline steel10.1016/j.msea.2006.05.029 ↗
43. Characteristics of inclusions in low carbon Al-killed steel during ladle furnace refining and calcium treatment10.2355/isijinternational.53.1401 ↗
44. Fracture toughness of the materials in welded joint of X80 pipeline steel10.1016/j.engfracmech.2015.07.061 ↗
45. Mechanism of (Mg, Al, Ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
46. Research of strain aging in pipeline steel with a ferrite/martensite dual–phase microstructure10.1002/srin.201300465 ↗