Grain refinement of Mg-14Li alloy by Sn addition and large strain rolling
Source abstract
Abstract
Mg-Li alloy is the lowest density structural metal, which has great potential for various industrial applications. Although Mg-Li alloy has excellent plasticity, it has low strength and requires further strengthening. In this study, the grain size of Mg-14 wt% Li alloy was refined to 15.7 μm by the addition of 6 wt% Sn, the initial grain size of as-cast Mg-14Li alloy was 180 μm. Furthermore, the grain size of Mg-14Li-6Sn was further refined to 400 nm by the subsequent large strain rolling (LSR). The yield strength of the ultra-fine grained Mg-14Li-6Sn reached 160 MPa, and the elongation was not sacrificed but increased to 30% compared with the as-cast alloy (14%). The microstructural evolution was characterized by optical microscopy (OM), scanning electron microscope (SEM) and transmission electron microscopy (TEM). The high ductility of the ultra-fine grained Mg-14Li-6Sn is attributed primarily to the dynamic recovery, and the increase in strength is mainly due to the grain refinement.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Density of magnesium and magnesium-lithium alloys in solid and liquid states10.1016/s1003-6326(19)64959-9 ↗
2. Application of texture simulation to understanding mechanical behavior of Mg and solid solution alloys containing Li or Y10.1016/s1359-6454(01)00297-x ↗
3. Comparative study of the deformation behavior of hexagonal magnesium–lithium alloys and a conventional magnesium AZ31 alloy10.1016/j.actamat.2009.01.031 ↗
4. Influence of texture and grain size on work hardening and ductility in magnesium-based alloys processed by ECAP and rolling10.1016/j.actamat.2006.05.018 ↗
5. Comparison of the microstructure and thermal stability of an AZ31 alloy processed by ECAP and large strain hot rolling10.1016/j.msea.2005.08.081 ↗
6. Independent slip systems in crystals10.1080/14786436308213843 ↗
7. Effect of strain rate on the ductility of a nanostructured aluminum alloy10.1016/j.scriptamat.2005.11.035 ↗
8. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
9. Microstructure characterization and mechanical properties of the as-cast and as-extruded Mg-xLi-5Zn-0.5 Er (x= 8, 10 and 12 wt%) alloys10.1016/j.matchar.2019.110008 ↗
10. High specific strength Mg-Li-Zn-Er alloy processed by multi deformation processes10.1016/j.matchar.2020.110135 ↗
11. Combination effects of Yb addition and cryogenic-rolling on microstructure and mechanical properties of LA141 alloy10.1016/j.msea.2020.139611 ↗
12. Deformation of an Al–7Mg alloy with extensive structural micro-segregations during dynamic plastic deformation10.1016/j.msea.2015.01.057 ↗
13. Effect of carbonate additive on the microstructure and corrosion resistance of plasma electrolytic oxidation coating on Mg-9Li-3Al alloy10.1007/s12613-021-2377-0 ↗
14. A flash of magnesium10.1038/nchem.459 ↗
15. The importance of twinning for the ductility of CPH polycrystals
16. Microstructure and mechanical behavior of friction stir processed ultrafine grained Al–Mg–Sc alloy10.1016/j.msea.2011.03.109 ↗
17. Effects of Nd on microstructure and mechanical properties of as-cast LA141 alloys10.1016/j.msea.2007.10.073 ↗
18. Large plasticity in magnesium mediated by pyramidal dislocations10.1126/science.aaw2843 ↗
19. Corrosion behavior of Mg−Li alloys: A review10.1016/s1003-6326(21)65728-x ↗
20. Bimodally grained microstructure development during hot extrusion of Mg–2.4 Zn–0.1 Ag–0.1 Ca–0.16 Zr (at.%) alloys10.1016/j.actamat.2009.07.057 ↗
21. Development of low-alloyed and rare-earth-free magnesium alloys having ultra-high strength10.1016/j.actamat.2018.03.002 ↗
22. Achieving high strength in commercial Mg cast alloys through large strain rolling10.1016/j.matlet.2005.04.061 ↗
23. Weight loss with magnesium alloys10.1126/science.1182848 ↗
24. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
25. Basal and non-basal dislocation slip in Mg–Y10.1016/j.msea.2013.03.006 ↗
26. Bulk nanocrystalline high-strength magnesium alloys prepared via rotary swaging10.1016/j.actamat.2020.09.024 ↗
27. Synergistically improved damping, elastic modulus and mechanical properties of rolled Mg-8Li-4Y-2Er-2Zn-0.6Zr alloy with twins and long-period stacking ordered phase10.1016/j.jallcom.2021.160663 ↗
28. The transformation of LPSO type in Mg-4Y-2Er-2Zn-0.6 Zr and its response to the mechanical properties and damping capacities10.1016/j.jma.2019.10.003 ↗
29. Enhanced electromagnetic interference shielding in a duplex-phase Mg–9Li–3Al–1Zn alloy processed by accumulative roll bonding10.1007/s40195-020-01017-z ↗
30. Tensile flow and strain-hardening behaviors of dual-phase Mg–Li–Zn alloy thin sheets10.1016/j.msea.2010.08.019 ↗
31. The origins of high hardening and low ductility in magnesium10.1038/nature15364 ↗
32. Overview of advancement and development trend on magnesium alloy10.1016/j.jma.2019.08.001 ↗
33. Nanostructured high‐entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
34. Improving the corrosion resistance of MgZn1.2Gd Zr0.18 (x = 0, 0.8, 1.4, 2.0) alloys via Gd additions10.1016/j.corsci.2020.108962 ↗
35. Slip, twinning, and fracture in hexagonal close-packed metals10.1007/bf02648537 ↗
36. Tailoring the mechanical properties of Mg–Zn magnesium alloy by calcium addition and hot extrusion process10.1016/j.msea.2020.138929 ↗
37. Coherent interface strengthening of ultrahigh pressure heat-treated Mg-Li-Y alloys10.1016/j.jmst.2020.02.039 ↗
38. Effect of Sn alloying and cold rolling on microstructure and mechanical properties of Mg14Li alloy10.1016/j.matchar.2021.111491 ↗